Thermal properties of Cu–Pd alloy under high pressure AITranslate

Zanjan University; Zanjan University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this investigation, we focus on the melting of elements Cu, Pd as well as Cux–Pd1−x random alloys. The thermodynamic properties such as melting temperature, isobaric heat capacity and lattice thermal expansion coefficient were calculated as a function of pressure in the range of 0–100 GPa. Moreover, the temperature dependence of energy, order parameter, volume, and density were calculated in various pressures. These calculations were performed by molecular dynamics simulation technique in NPT ensemble. The results showed melting temperature increase upon increasing pressure. Furthermore, isobaric heat capacity and lattice thermal expansion decreased with increasing pressure. These variations were found to be nonlinear approximating a constant value at higher pressures. Our results are in reasonable agreement with the experimental data where they are available.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.03.052

Chinese Library Classification Number:

Citation Information:

In this investigation, we focus on the melting of elements Cu, Pd as well as Cux–Pd1−x random alloys. The thermodynamic properties such as melting temperature, isobaric heat capacity and lattice thermal expansion coefficient were calculated as a function of pressure in the range of 0–100 GPa. Moreover, the temperature dependence of energy, order parameter, volume, and density were calculated in various pressures. These calculations were performed by molecular dynamics simulation technique in NPT ensemble. The results showed melting temperature increase upon increasing pressure. Furthermore, isobaric heat capacity and lattice thermal expansion decreased with increasing pressure. These variations were found to be nonlinear approximating a constant value at higher pressures. Our results are in reasonable agreement with the experimental data where they are available.

quote

GB/T 7714-2015 [1] J. Davoodi, M. Ahmadi. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.03.052.
MLA [1] J. Davoodi, and M. Ahmadi. Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.03.052.
APA [1] J. Davoodi, & M. Ahmadi. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.03.052
IEEE [1] J. Davoodi and M. Ahmadi, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.03.052.