Effects of Graphite Powder Doping on ZrNi Alloy Preparation by Direct Electro-deoxidation Method AITranslate
Abstract AITranslate
The sintered ZrO2-NieO3 sheets were prepared by doping graphite powders into material, and they were used as the cathode to prepare ZrNi alloy by direct eletro-deoxidation. Effects of graphite powders do- ping on morphology and composition of the sintered sheets and eletro-deoxidation reaction of the cathode were investigated. The results show that in the case of doping graphite powders, the sintered ZrO2-Ni2O3 sheets have more uniform particle size and higher porosity. Graphite powder doping can also improve ca- thodic electrolysis current and accelerate eletro-deoxidation reaction, and furthermore the content of ZrNi alloy phase in the electrolysis product is higher,with mass fraction up to 82%(from oxidation-weighing method) or 94.6% (from EDS microanalysis).
KeyWords AITranslate
1稀有金属编辑委员会.稀有金属手册(上)[M].北京:冶金工业出版社,1992.
2李自强,苏辉煌,李书年,牛求彬.还原扩散法直接制造ZrNi合金粉末的研究[J].粉末冶金技术,1996,14(4):243-248. 被引量:7
3Mohandas K S, Fray D J. FFC Cambridge process and removal of oxygen from metal-oxygen systems by mol- ten salt electrolysis., an overview[J]. Trans Indian Inst Met, 2005,57 : 579-592.
4Glowacki B A, Fray D J, Yan X Y, et al. Superconducting Nb3Sn intermetallics made by electrochemical reduction of Nb2Os-SnO2 oxides[J].Physica C, 2003,387: 242- 246.
5董云会,李德刚,王平,等.直接电脱氧法制备ZrNi合金的新工艺探讨[J].中国稀土学报,2008,26:616-619.
6郭春芳,董云会,于先进,李德刚,张丽鹏.直接电脱氧法制备金属锆[J].中国有色金属学报,2007,17(6):1019-1023. 被引量:17
7郭春芳,董云会.金属锆制备方法的研究进展[J].稀有金属与硬质合金,2008,36(2):63-67. 被引量:21
8李晴宇,杜继红,奚正平,李争显,杨升红.阴极掺杂提高熔盐电脱氧制备锆电解效率的机制[J].稀有金属材料与工程,2009,38(9):1575-1579. 被引量:7
9李颖君,王淑兰,钟和香,孙华.电化学还原TiO_2反应机理及电极电势的研究[J].有色金属,2003,55(4):68-70. 被引量:19
10Chen G Z,Fray D J. Vohammetric studies of the oxy- gen-Titanium binary system in mohen calcium chloride [J]. J Appl Electrochemical Society, 2002,149 ( 1 ) : 455- 467.
1李泽全,胡玲,卢姣,刘楠,韩梅.熔盐电脱氧法制备合金时物质间相互影响的研究进展[J].稀有金属,2016,40(11):1169-1176. 被引量:3
2贾雷,严红燕,李慧,刘畅,张帅.熔盐电脱氧法制备金属及合金的研究进展[J].矿产综合利用,2020(3):69-77. 被引量:3
1焦芸芬,王旭,廖春发,孙强超,蔡伯清,汤浩.Na3AlF6-AlF3-LiF-MgF2-Al2O3-Sm2O3熔盐体系表面张力的研究[J].稀有金属,2018,42(1):75-82. 被引量:1
2陈征,赵兴科.致密ZrO2陶瓷板表面金属层的熔盐电解法制备[J].稀有金属,2018,42(2):175-181. 被引量:3
3贾雷,严红燕,李慧,刘畅,张帅.熔盐电脱氧法制备金属及合金的研究进展[J].矿产综合利用,2020(3):69-77. 被引量:3
4张禛,张小联,杨初斌.SmF3-LiF-Sm2O3熔盐中Sm(Ⅲ)在钨与镍电极上的电化学还原[J].赣南师范大学学报,2020,41(6):48-51. 被引量:1
5康佳,闫奇操,刘玉宝,于兵,赵二雄,张全军,黄海涛.熔盐电解法制备镧合金的研究进展[J].矿产综合利用,2022(6):110-115.
6付刚华,姚洪国,陈凤,郑富强,王帅,杨凌志.熔盐氯化废渣综合利用研究进展[J].矿产综合利用,2023(3):112-118.
1王素英.YG8硬质含金渗硼工艺的探讨[J].石家庄职业技术学院学报,1999,11(2):30-31.
2陈军.联结片21工位精密级进模设计与制造[J].模具工业,1996,22(1):7-9.
3郭春芳,董云会,于先进,李德刚,张丽鹏.直接电脱氧法制备金属锆[J].中国有色金属学报,2007,17(6):1019-1023. 被引量:17
4韩华丽,范铁桢,杨彬,杨丹丹,刘书锋,杨小东,纪莲清.结合剂含量对PcBN力学性能的影响[J].铸造技术,2015,36(3):573-575. 被引量:4
5谢珊珊,李慧,梁精龙,霍东兴.金属铪的制备工艺[J].热加工工艺,2017,46(6):36-38. 被引量:5
6谢珊珊,李慧,张士宪,刘晓,霍东兴.金属锆的制备工艺[J].热加工工艺,2017,46(4):27-29. 被引量:4
7李俊,王兴庆,盛娅峥.烧结温度对电脱氧制备金属铌影响的研究[J].金属材料与冶金工程,2011,39(6):3-7.
8杨贤金,何菲,朱胜利,崔振铎,姚康德.化学修饰对NiTi形状记忆合金氧化膜的影响[J].功能材料,2002,33(2):169-171. 被引量:9
9郑辅养,马廷椿,温国谋.镀铜层阴极电解着色[J].电镀与精饰,1998,20(1):13-17.
10朱靖,曹吉林,王明涌,王岭,戴磊.熔盐电脱氧法制备ZrCr_2储氢合金的研究[J].人工晶体学报,2016,45(3):834-839. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.414[金属学及工艺—金属材料]
Citation Information:
The sintered ZrO2-NieO3 sheets were prepared by doping graphite powders into material, and they were used as the cathode to prepare ZrNi alloy by direct eletro-deoxidation. Effects of graphite powders do- ping on morphology and composition of the sintered sheets and eletro-deoxidation reaction of the cathode were investigated. The results show that in the case of doping graphite powders, the sintered ZrO2-Ni2O3 sheets have more uniform particle size and higher porosity. Graphite powder doping can also improve ca- thodic electrolysis current and accelerate eletro-deoxidation reaction, and furthermore the content of ZrNi alloy phase in the electrolysis product is higher,with mass fraction up to 82%(from oxidation-weighing method) or 94.6% (from EDS microanalysis).
quote
| GB/T 7714-2015 | [1] GUO Chun-fang, DONG Yun-hui. Effects of Graphite Powder Doping on ZrNi Alloy Preparation by Direct Electro-deoxidation Method[J]. Rare Metals and Cemented Carbides, 2012(5): 33-36. |
| MLA | [1] GUO Chun-fang, and DONG Yun-hui. "Effects of Graphite Powder Doping on ZrNi Alloy Preparation by Direct Electro-deoxidation Method." Rare Metals and Cemented Carbides, no. 5, 2012, pp. 33-36. |
| APA | [1] GUO Chun-fang, & DONG Yun-hui. (2012). Effects of Graphite Powder Doping on ZrNi Alloy Preparation by Direct Electro-deoxidation Method. Rare Metals and Cemented Carbides(5), 33-36. |
| IEEE | [1] GUO Chun-fang and DONG Yun-hui, "Effects of Graphite Powder Doping on ZrNi Alloy Preparation by Direct Electro-deoxidation Method," Rare Metals and Cemented Carbides, no. 5, pp. 33-36, 2012. keywords: {. sintered ZrO2-Ni2O3 sheet;graphite powder;cathode electrolysis;direct eletro-deoxidation;ZrNialloy} |