Investigation of Electrode Cycling Performance and Electrochemical Corrosion Behaviour of RE-Mg-Ni Alloy AITranslate

School of Quality and Technical Supervision of Hebei University;School of Quality and Technical Supervision of Hebei University;School of Quality and Technical Supervision of Hebei University;School of Quality and Technical Supervision of Hebei University;School of Quality and Technical Supervision of Hebei University;School of Quality and Technical Supervision of Hebei University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cast or heat treated La0.80Mg0.20(Ni0.94Co0.06)3.7 alloys were prepared to investigate effects of heat treatment on electrode cycling performance, phase composition and electrochemical corrosion behaviour of the alloys. The results from SEM and EDS analysis show that heat treatment will result in less Mg and Ni concentration difference between phases in the alloys. Compared with cast alloy, heat treated alloy has a more positive interphase corrosion mixed potential. The maximum interphase corrosion current density of cast alloy and heat treated alloy is 106.1 mA/g and 82.4 mA/g,respectively. After heat treatment, the al loy has better electrode cycling performance due to lower interphase electrochemical corrosion.

KeyWords AITranslate

RE- Mg- Ni alloy hydrogen storage alloy electrode heat treatment cycling performance phasecomposition electrochemical corrosion

1胡 静,张 云,林栋梁.Ni_3Al中B和Mg的非平衡晶界共偏聚[J].金属学报,2002,38(8):829-834. 被引量:8

2董小平,吕反修,张羊换,杨丽颖,王新林.Effect of annealing temperature on microstructure and electrochemical performance of La_(0.75)Mg_(0.25)Ni_(3.5)Co_(0.2) hydrogen storage electrode alloy[J].稀土学报:英文版,2008,26(1):99-104. 被引量:8

3董小平,杨丽颖,李小亭,马力辉,林玉芳,赵栋梁.退火方式对La_(0.75)Mg_(0.25)Ni_(3.44)Co_(0.2)Al_(0.03)Ti_(0.03)合金的电化学性能影响[J].材料热处理学报,2010,31(1):80-85. 被引量:5

1方智赫,连建峰,张琳,吴荫顺.用微电极研究20钢和16Mn钢微区相电化学行为[J].腐蚀科学与防护技术,1996,8(3):195-200. 被引量:6

2钱海帆,张宇光,王炜,张建平.Fe-C-Mn-Al系TRIP钢两相区奥氏体转变模拟[J].钢铁,2012,47(9):57-62. 被引量:2

3曹楚南.混合电位下的法拉第导纳[J].中国腐蚀与防护学报,1993,13(2):91-100. 被引量:19

4周琦,贾建刚,南雪丽,臧树俊,赵红顺,程新兰.CO2环境介质下16Mn钢的高温高压腐蚀性能[J].兰州理工大学学报,2008,34(1):14-18. 被引量:6

5徐敏杰,张华民.断电法测得的极化电位的研究[J].油田地面工程,1991,10(6):28-31.

6曹楚南.混合电位下的电极过程研究[J].腐蚀科学与防护技术,1998,10(1):1-5. 被引量:17

7刘宇,石勇,李宁,张海宽.5083铝合金与2205不锈钢在天然海水中的电偶腐蚀行为[J].腐蚀与防护,2012,33(6):532-534. 被引量:10

8张宇光,赵爱民,赵征志,张明明,唐荻,李本海.冷轧TRIP钢两相区奥氏体化中合金元素的扩散[J].沈阳工业大学学报,2011,33(1):62-67. 被引量:6

9杨玉国,许韵华,周曦.化学镀镍过程中金属基体的引发催化特性研究[J].北方交通大学学报,2002,26(3):74-76. 被引量:1

10梁平,张云霞,闫永贵,张海兵,苏策.氯化镧对2024铝合金缝隙腐蚀的缓蚀作用[J].北京科技大学学报,2010,32(1):50-54. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG139.7[一般工业技术—材料科学与工程]

Citation Information:

Cast or heat treated La0.80Mg0.20(Ni0.94Co0.06)3.7 alloys were prepared to investigate effects of heat treatment on electrode cycling performance, phase composition and electrochemical corrosion behaviour of the alloys. The results from SEM and EDS analysis show that heat treatment will result in less Mg and Ni concentration difference between phases in the alloys. Compared with cast alloy, heat treated alloy has a more positive interphase corrosion mixed potential. The maximum interphase corrosion current density of cast alloy and heat treated alloy is 106.1 mA/g and 82.4 mA/g,respectively. After heat treatment, the al loy has better electrode cycling performance due to lower interphase electrochemical corrosion.

quote

GB/T 7714-2015 [1] DONG Xiao-ping, YANG Li-ying, WANG Qing, et al. Investigation of Electrode Cycling Performance and Electrochemical Corrosion Behaviour of RE-Mg-Ni Alloy[J]. Rare Metals and Cemented Carbides, 2012(5): 28-32.
MLA [1] DONG Xiao-ping, et al., "Investigation of Electrode Cycling Performance and Electrochemical Corrosion Behaviour of RE-Mg-Ni Alloy." Rare Metals and Cemented Carbides, no. 5, 2012, pp. 28-32.
APA [1] DONG Xiao-ping, YANG Li-ying, WANG Qing, ZHU Kai-ning, XU Ya-wei, & WANG Cui-biao. (2012). Investigation of Electrode Cycling Performance and Electrochemical Corrosion Behaviour of RE-Mg-Ni Alloy. Rare Metals and Cemented Carbides(5), 28-32.
IEEE [1] DONG Xiao-ping, YANG Li-ying, WANG Qing, ZHU Kai-ning, XU Ya-wei, and WANG Cui-biao, "Investigation of Electrode Cycling Performance and Electrochemical Corrosion Behaviour of RE-Mg-Ni Alloy," Rare Metals and Cemented Carbides, no. 5, pp. 28-32, 2012. keywords: {RE- Mg- Ni alloy;hydrogen storage alloy electrode;heat treatment;cycling performance;phasecomposition;electrochemical corrosion}