Effect of SnO2 Particle Size on Properties of AgSnO2 Contact Material AITranslate

State Key Laboratory of Reliability and Intelligence of Electrical Equipment,Hebei University of Technology;State Key Laboratory of Reliability and Intelligence of Electrical Equipment,Hebei University of Technology;State Key Laboratory of Reliability and Intelligence of Electrical Equipment,Hebei University of Technology;State Key Laboratory of Reliability and Intelligence of Electrical Equipment,Hebei University of Technology;State Key Laboratory of Reliability and Intelligence of Electrical Equipment,Hebei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Undoped AgSnO2 and AgSnO2/La2O3 contact materials with six kinds of SnO2 particle sizes were prepared by powder metallurgy,and the influence was studied of SnO2 particle size on physical properties and electrical contact properties of the two kinds of AgSnO2 contact materials.The results show that when SnO2 particle sizes are 1 000 nm and 500 nm,respectively,both the undoped AgSnO2 and AgSnO2/La2O3 materials have moderate hardness,high conductivity,small and stable contact resistance and arc energy.The properties of AgSnO2 contact materials can be improved by selecting appropriate SnO2 particle size.

KeyWords AITranslate

AgSnO2 contact material SnO2 particle size rare earth La doping physical property electrical contact property

1王俊勃,刘英,付翀,杨敏鸽,丁秉钧.热压烧结制备La混杂纳米复合AgSnO_2电接触合金[J].稀有金属材料与工程,2009,38(11):2023-2026. 被引量:17

2王志法,张迎九,姜国圣,吕维洁,许贞.粒度对Cu/FeNi复合材料性能的影响[J].中南工业大学学报,1997,28(3):246-249. 被引量:1

3朱艳彩,王景芹,王海涛.Bi掺杂纳米AgSnO_2的耐电弧侵蚀性能研究[J].稀有金属材料与工程,2013,42(1):149-152. 被引量:20

4郑冀,李松林,高后秀,李群英.纳米氧化锡银基电触头材料的研究[J].稀有金属材料与工程,2003,32(10):829-831. 被引量:32

5王海涛,王景芹,杜江,孟凡青.稀土对AgSnO_2触头材料润湿性影响(英文)[J].稀有金属材料与工程,2014,43(8):1846-1849. 被引量:21

6王俊勃,李英民,王亚平,丁秉钧.纳米复合银基电触头材料的研究[J].稀有金属材料与工程,2004,33(11):1213-1217. 被引量:34

7朱艳彩,王海涛,赵军.低压电器中纳米AgSnO_2电接触材料的制备方法及研究进展[J].低压电器,2012(4):1-5. 被引量:5

8刘海英,王亚平,丁秉钧.纳米AgSnO_2触头材料的制备与组织分析[J].稀有金属材料与工程,2002,31(2):122-124. 被引量:39

9王永根,曹小青,倪玉萍,魏永亮.电触头材料在低压电器中的应用[J].低压电器,2011(10):58-61. 被引量:10

1王塞北,王松,孙勇,谢明,陈永泰,李爱坤,侯攀,刘满门.新型银基电接触材料的研究进展[J].贵金属,2019,40(4):72-77. 被引量:6

2吴新合,沈涛,杨辉,祁更新,穆成法,陈晓.环保型氧化物增强银基电接触功能复合材料研究进展[J].贵金属,2021,42(1):79-87. 被引量:3

3李朕,王召斌,陈康宁,李维燕,尚尚.银氧化锡触头制备工艺对比及其电弧侵蚀特性综述[J].电工材料,2021(4):3-9. 被引量:2

4周光华,庞杰林,冯朋飞,黎联杰,卢菲.Ag粉的粒度及形貌对粉末冶金法AgSnO_(2)材料性能的影响[J].电工材料,2022(3):39-42.

1魏明霞,赵君,王剑平,高勤琴,杨有才,陈永泰,段云昭,谢明.AgSnO2/Cu材料焊接钎着率及界面的组织研究[J].贵金属,2020,41(S01):22-26.

2陈鸿武,汪聪,郑东辉,陈洁,苏传明,杨铭瑞.电接触材料对导电滑环寿命和可靠性的影响[J].信息记录材料,2021,22(8):18-21.

3王金龙,付翀,宁静,李旭,李清馨,路杨.Ag-SnO_(2)电接触材料的研究进展及发展趋势[J].贵金属,2021,42(3):85-92. 被引量:1

4黄秋玲,李肖瑶,张晓,肖红新.铅试金-重量法测定银钨合金中的银[J].材料研究与应用,2022,16(2):311-315. 被引量:1

5杨芳儿,秦海波,张继,穆成法,沈涛,郑晓华.制备工艺对Ag/Co_(3)O_(4)电接触材料物理性能的影响[J].贵金属,2022,43(1):27-33. 被引量:1

6胡钟元,王开旭,周馨,高林辉,李跃.Bi_(2)Sn_(2)O_(7)含量对改性Ag/SnO_(2)电接触复合材料微观结构及性能的影响[J].稀有金属材料与工程,2022,51(10):3808-3818.

7陈鑫,周铭,王明月,尤胜利,莫有堂.银-石墨烯电接触材料的制备方法对比分析[J].装备制造技术,2022(10):143-147.

8滕汶宋,周晓龙,胡晨,于杰,刘满门,王立惠.ZnO含量对AgCuOIn_(2)O_(3)SnO_(2)ZnO材料电接触性能的影响[J].功能材料,2023,54(2):2159-2166.

9郑晓华,张红生,沈涛,杨芳儿,陈琍.Ni掺杂改善Ag/Bi_(2)Sn_(2)O_(7)电接触材料的力学性能[J].浙江工业大学学报,2023,51(2):193-198.

10尹智勇,李雨,李亮.轨道交通车辆直流继电器自主化设计[J].电器与能效管理技术,2023(4):40-46.

1杨珍,莫立焕,李军,徐峻.La掺杂改性纳米TiO_2的制备及其在O_3协同下的光催化活性[J].造纸科学与技术,2018,37(1):61-64. 被引量:2

2李勰,朱晓东,王婷婷,王会.La掺杂纳米ZnO/硅藻土复合材料的制备及其对甲醛气体的降解性能[J].材料研究学报,2018,32(9):685-690. 被引量:6

3程振,王巍,杨丽梅,徐政,纪仲光,黄松涛.La掺杂TiO2的制备及光催化处理石化二级出水的研究[J].稀有金属,2018,42(9):950-958. 被引量:7

4罗林山,刘雯雯,文小强,张帆,周新华,郭春平,周有池,普建.稀土La掺杂对层状富锂锰基氧化物正极材料结构及电化学性能的影响[J].有色金属科学与工程,2019,10(3):104-110. 被引量:3

5施辰阳,沙旭明,白炜炜,陈柏峰,陈李庆,杨华云,李伟东.一种新型La掺杂PbO_2电极用于X-GRL降解的研究[J].杭州师范大学学报:自然科学版,2018,17(5):499-505.

6张晓辉,田保红,刘勇,张毅,宋克兴,李全安.真空热压烧结-内氧化法制备Al2O3-Cu/(W,Cr)触头材料的电接触性能[J].中国有色金属学报,2019,29(6):1242-1249. 被引量:4

7陈阳雯,刘蕊,姚洁,袁兴程.La掺杂钛基氧化物电极降解水中2,4-二氯酚的研究[J].环境科学与技术,2018,41(1):94-98. 被引量:5

8徐静,何波.La掺杂Ba_(0.67)Sr_(0.33)TiO_3陶瓷高介电常数机制探讨[J].电子显微学报,2019,38(1):27-33. 被引量:1

9赵鹤然,田爱民,苏琳,马艳艳,刘洪涛,刘庆川.长方形封口器件储能焊的PIND控制[J].电子与封装,2019,19(9):1-4. 被引量:1

10王怀伟,王艳阳.La2O3强化等离子喷焊镍包铝涂层的组织及高温耐磨性能[J].材料保护,2019,0(6):52-57.

Basic Information:

DOI:

Chinese Library Classification Number:TG146[金属学及工艺—金属材料]

Citation Information:

Undoped AgSnO2 and AgSnO2/La2O3 contact materials with six kinds of SnO2 particle sizes were prepared by powder metallurgy,and the influence was studied of SnO2 particle size on physical properties and electrical contact properties of the two kinds of AgSnO2 contact materials.The results show that when SnO2 particle sizes are 1 000 nm and 500 nm,respectively,both the undoped AgSnO2 and AgSnO2/La2O3 materials have moderate hardness,high conductivity,small and stable contact resistance and arc energy.The properties of AgSnO2 contact materials can be improved by selecting appropriate SnO2 particle size.

quote

GB/T 7714-2015 [1] WANG Hai-tao, ZHANG Mei, YANG Meng-lin, et al. Effect of SnO2 Particle Size on Properties of AgSnO2 Contact Material[J]. Rare Metals and Cemented Carbides, 2019(4): 58-64.
MLA [1] WANG Hai-tao, et al., "Effect of SnO2 Particle Size on Properties of AgSnO2 Contact Material." Rare Metals and Cemented Carbides, no. 4, 2019, pp. 58-64.
APA [1] WANG Hai-tao, ZHANG Mei, YANG Meng-lin, WANG Jing-qin, & Zhu Yan-cai. (2019). Effect of SnO2 Particle Size on Properties of AgSnO2 Contact Material. Rare Metals and Cemented Carbides(4), 58-64.
IEEE [1] WANG Hai-tao, ZHANG Mei, YANG Meng-lin, WANG Jing-qin, and Zhu Yan-cai, "Effect of SnO2 Particle Size on Properties of AgSnO2 Contact Material," Rare Metals and Cemented Carbides, no. 4, pp. 58-64, 2019. keywords: {AgSnO2 contact material;SnO2 particle size;rare earth La doping;physical property;electrical contact property}