Investigation on Wear Properties of (V2O5+WO3+C)/Ni60 Coatings Prepared by Laser Cladding AITranslate
Abstract AITranslate
In order to improve the wear properties of 45#steel,(V2O5+WO3+C)/Ni60 coatings were prepared by laser cladding on steel 45#steel surface.The microstructure and phase of the cladding layer were analyzed by metallographic microscope,scanning electron microscope and X-ray diffractometer,the microhardness of the cladding layer was measured by microhardness tester,and the friction test was carried out by high-speed ring wear tester.The results show that the coating is composed of solid solutionγ(NiFe)and in-situ synthesized reinforcing phases including W2C,WC,VC and Cr3C2.The hardness and wear resistance of the(V2O5+WO3+C)/Ni60 coating are greatly improved.The average HV0.3 hardness of the cladding layer is as high as 1 400,which is one fifth of the wear weight loss of Ni60 coating.
KeyWords AITranslate
1李昊真,杨勇,于丹丹,王玉玲,杨涛涛.20CrMnTi基体高功率熔覆Co基合金熔覆层性能[J].激光杂志,2017,38(3):28-32. 被引量:6
2达则晓丽,朱彦彦,李铸国.激光功率对激光熔覆Fe-Co-B-Si-Nb涂层组织和性能的影响[J].中国表面工程,2012,25(3):52-56. 被引量:20
3李美艳,韩彬,王勇,宋立新.激光熔覆Ni-WC/Cr_3C_2涂层组织及性能[J].焊接学报,2016,37(3):17-21. 被引量:12
4陈美容,曾宪光,孙德恩,黄佳木.Zr掺杂类金刚石薄膜摩擦性能及耐腐蚀性能的影响[J].表面技术,2017,46(6):138-142. 被引量:10
5李荐,李淳伟,夏亨,刘凡,李艳芬,杨亮,杨俊.添加ZrO_2对Si_3N_4复合陶瓷材料力学性能的影响[J].稀有金属与硬质合金,2012,40(1):38-40. 被引量:7
6严凯,陈长军,张敏,秦兰兰,任博,王晓南,邹涛.增材制造H13钢表面熔覆Ni/WC涂层组织及性能研究[J].应用激光,2017,37(2):175-180. 被引量:11
7于香苑,徐培全,曹晓莲,姚德军,周东冉,李颖.YG20硬质合金/45~#钢激光焊缝的显微组织与腐蚀行为研究[J].稀有金属与硬质合金,2015,43(6):73-78. 被引量:3
8高正源,潘复生,汤爱涛,程毅.AZ31镁合金表面纳米Al_2O_3涂层的耐蚀耐磨性能研究[J].功能材料,2013,44(8):1069-1072. 被引量:15
9李明玉,晁明举,梁二军,张俊吉,李德川.Cu材料激光表面强化研究[J].中国激光,2011,38(8):65-69. 被引量:8
10WANG Jiansheng,MENG Huimin,YU Hongying,FAN Zishuan,and SUN Dongbai School of Materials Science and Engineering,University of Science and Technology Beijing,Beijing 100083,China.Surface hardening of Fe-based alloy powders by Nd:YAG laser cladding followed by electrospark deposition with WC-Co cemented carbide[J].稀有金属:英文版,2010,0(4):380-384. 被引量:19
1于天彪,韩继标,乔若真,陈辽原,黎柏春,陈亚东.工艺参数对铁基和镍基粉末涂层性能的影响[J].激光与红外,2019,49(7):801-807. 被引量:4
2薛丽军.基于激光熔覆技术的单体液压支柱试验研究[J].机械管理开发,2019,0(7):112-114.
3花超.简述工艺参数对激光熔覆的影响[J].科技风,2019,0(24):150-150. 被引量:1
4吴雄喜.锻压温度对新型汽车模具钢性能的影响[J].机械制造与自动化,2019,48(4):62-64.
5吴杰,王忠华,吕健.HVOF喷涂超细结构WC-12Co涂层磨粒磨损性能[J].稀有金属与硬质合金,2019,47(4):24-29.
6花超.浅述激光熔覆技术的应用[J].科技风,2019,0(21):146-146. 被引量:3
7傅耀坤,王成磊,郑英,梁朝杰,谢映光,黄磊,程刚,黄锡腾.铝合金表面激光熔覆Re+Ni60电化学腐蚀性能研究[J].桂林电子科技大学学报,2019,39(3):236-241. 被引量:3
8钟豪,金青林.藕状多孔铜基自润滑材料的载流磨损性能[J].热加工工艺,2019,48(14):80-83.
9侯晓云,庄怀风,柏明磊,王浩.CeO2对Ti811表面钛基激光熔覆层微观组织及性能的影响[J].热加工工艺,2019,48(14):84-87.
10崔虹云,胡明,孙建波,王天浩,张漫,马佳.金属基碳纳米管复合材料的研究及展望[J].热加工工艺,2019,48(14):16-18. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TG156.99[金属学及工艺—热处理]
Citation Information:
In order to improve the wear properties of 45#steel,(V2O5+WO3+C)/Ni60 coatings were prepared by laser cladding on steel 45#steel surface.The microstructure and phase of the cladding layer were analyzed by metallographic microscope,scanning electron microscope and X-ray diffractometer,the microhardness of the cladding layer was measured by microhardness tester,and the friction test was carried out by high-speed ring wear tester.The results show that the coating is composed of solid solutionγ(NiFe)and in-situ synthesized reinforcing phases including W2C,WC,VC and Cr3C2.The hardness and wear resistance of the(V2O5+WO3+C)/Ni60 coating are greatly improved.The average HV0.3 hardness of the cladding layer is as high as 1 400,which is one fifth of the wear weight loss of Ni60 coating.
quote
| GB/T 7714-2015 | [1] YANG Ning, LI Li-kai. Investigation on Wear Properties of (V2O5+WO3+C)/Ni60 Coatings Prepared by Laser Cladding[J]. Rare Metals and Cemented Carbides, 2019(4): 54-57. |
| MLA | [1] YANG Ning, and LI Li-kai. "Investigation on Wear Properties of (V2O5+WO3+C)/Ni60 Coatings Prepared by Laser Cladding." Rare Metals and Cemented Carbides, no. 4, 2019, pp. 54-57. |
| APA | [1] YANG Ning, & LI Li-kai. (2019). Investigation on Wear Properties of (V2O5+WO3+C)/Ni60 Coatings Prepared by Laser Cladding. Rare Metals and Cemented Carbides(4), 54-57. |
| IEEE | [1] YANG Ning and LI Li-kai, "Investigation on Wear Properties of (V2O5+WO3+C)/Ni60 Coatings Prepared by Laser Cladding," Rare Metals and Cemented Carbides, no. 4, pp. 54-57, 2019. keywords: {laser cladding;(V2O5+WO3+C)/Ni60 coating;microhardness;wear property} |