Determination of Laser Particle Size Distribution of Ultra-fine WC Powder AITranslate

Zigong Cemented Carbide Co.,Ltd;Zigong Cemented Carbide Co.,Ltd;Zigong Cemented Carbide Co.,Ltd;Zigong Cemented Carbide Co.,Ltd
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ultra-fine WC powder contains a high surface energy in the developed suriace area,which exhibits a strong adsorption capacity for gases,liquids or particles,and is easily aggregated into secondary particles spontaneously,which leads to the sample using conventional laser particle size analysis method can not be effectively dispersed.The laser particle size distribution curve is always with a "trailing".In this paper,we ground the sample for 1 hour,then added the sample after grinding into the anhydrous ethanol,and into the external ultrasound machine for 10 minutes.Finally,the sample was tested.The particle size distribution curve of this test method is normal distribution,with good precision,and the relative standard deviation of laser particle size distribution characteristic value (d (10),d (50)and d (90))is less than 5%.

KeyWords AITranslate

ultra-fine WC powder laser particle size distribution absolute ethyl alcohol ultrasonic dispersion grinding

1李启厚,黄异龄,王红军,刘志宏,杨天足.粒径≤2μm的超细粉体颗粒分散方式探讨[J].粉末冶金材料科学与工程,2007,12(5):284-289. 被引量:15

2李召好,李法强,马培华.超细粉末团聚机理及其消除方法[J].盐湖研究,2005,13(1):31-36. 被引量:38

1胡启明,张玉琪.静态图像分析法在亚微WC粉末粒度分析中的应用[J].硬质合金,2022,39(4):281-288.

1肖江涛,汤烈明.应用于钼靶材的大粒度钼粉制备技术[J].铸造技术,2017,38(9):2100-2103. 被引量:4

2沈永麟,肖正琼.测定超细硅酸盐水泥粒度分布的问题探讨[J].中国检验检测,2019,27(1):20-21.

3赵伟伟,李鹏飞,顾浩,谢孔良,侯爱芹.功能化石墨烯的制备及石墨烯/聚氨酯复合材料的性能研究[J].染整技术,2018,40(12):4-10. 被引量:2

4刘勇强,王帅,丁燕军.自组装GO/Al/Co_3O_4铝热剂的制备及性能研究[J].火工品,2019(1):30-33. 被引量:1

5刘宇宁,甘春雷,王顺成,黎小辉,郑开宏,张辉.烧结温度对石墨烯增强铜基复合材料组织和性能的影响[J].金属热处理,2019,44(2):113-118. 被引量:6

6郑兴,冯梅,应道宴,蔡暖姝.法兰接头在高温下的应力松弛分布测定[J].化工设备与管道,2018,55(6):66-69. 被引量:1

7李三妮,陈娟.运用液相色谱-质谱/质谱法检测生鲜乳中雌二醇[J].中国食品,2019,0(7):141-141.

8郭庆胜,王勇,蓝振家,周贺杰,刘纪平,纪莹莹.地图兴趣点分布式空间分析服务[J].测绘科学,2018,43(1):89-92. 被引量:1

9兰恒星,陈俊辉,伍宇明.三轴压缩试验前后含气页岩微纳尺度裂隙空间分布特征研究[J].工程地质学报,2018,26(1):24-35. 被引量:8

10陈华,周晓力.检测用基质特性对于透皮贴剂黏附力检测影响的初步研究[J].中国新药杂志,2019,28(5):581-583. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]

Citation Information:

Ultra-fine WC powder contains a high surface energy in the developed suriace area,which exhibits a strong adsorption capacity for gases,liquids or particles,and is easily aggregated into secondary particles spontaneously,which leads to the sample using conventional laser particle size analysis method can not be effectively dispersed.The laser particle size distribution curve is always with a "trailing".In this paper,we ground the sample for 1 hour,then added the sample after grinding into the anhydrous ethanol,and into the external ultrasound machine for 10 minutes.Finally,the sample was tested.The particle size distribution curve of this test method is normal distribution,with good precision,and the relative standard deviation of laser particle size distribution characteristic value (d (10),d (50)and d (90))is less than 5%.

quote

GB/T 7714-2015 [1] QIU Yong, JIAN Yu-mei, JIANG Shu-xiang, et al. Determination of Laser Particle Size Distribution of Ultra-fine WC Powder[J]. Rare Metals and Cemented Carbides, 2019(1): 65-69.
MLA [1] QIU Yong, et al., "Determination of Laser Particle Size Distribution of Ultra-fine WC Powder." Rare Metals and Cemented Carbides, no. 1, 2019, pp. 65-69.
APA [1] QIU Yong, JIAN Yu-mei, JIANG Shu-xiang, & WANG Ke. (2019). Determination of Laser Particle Size Distribution of Ultra-fine WC Powder. Rare Metals and Cemented Carbides(1), 65-69.
IEEE [1] QIU Yong, JIAN Yu-mei, JIANG Shu-xiang, and WANG Ke, "Determination of Laser Particle Size Distribution of Ultra-fine WC Powder," Rare Metals and Cemented Carbides, no. 1, pp. 65-69, 2019. keywords: {ultra-fine WC powder;laser particle size distribution;absolute ethyl alcohol;ultrasonic dispersion;grinding}