Study on Performance Improvement of WC-Co Cemented Carbide by TiC/TaC Additive AITranslate
Abstract AITranslate
In order to improve the status quo that the commonly used cutter pick in coal mining engineering is easy to failure due to the damage of the carbide bit,the effects of TiC and TaC additives on the performance of WC-Co cemented carbide bit were studied.The results show that the structural hardness (HRA)of the treated bit can reach 87 ,which is much higher than the national standard of cutter pick of 65.Compared with the interior,the surface fracture toughness of the cutter pick is lower due to the formation of a large number of carbides on the surface,the average fracture toughness is about 15.50 MPa ·m^1/2.The internal fracture toughness is improved due to the presence of a large number of non-carbides,and its average value is 16.31 MPa ·m^1/2.
KeyWords AITranslate
1李建楠,李惠琪,王淑峰,迟静.国内矿用镐形截齿的研究现状及趋势[J].煤矿机械,2013,34(1):7-10. 被引量:13
2迟静,李惠琪,王淑峰,李敏.矿用WC硬质合金的研究进展与趋势[J].矿山机械,2010,38(8):23-28. 被引量:7
3申胜利.采煤机和掘进机截齿的失效分析及对策[J].煤矿机械,2005,26(7):53-55. 被引量:43
4史留勇,张守全,黄继华.WC-Co功能梯度硬质合金研究进展[J].粉末冶金技术,2010,28(4):305-312. 被引量:15
5羊建高,王海兵,刘咏,黄伯云,张武装.WC晶粒度不同的双层硬质合金中的梯度结构[J].中南大学学报:自然科学版,2005,36(3):349-353. 被引量:9
6何宪峰,石建华.优质粗晶WC碳化工艺研究[J].稀有金属快报,2005,24(10):28-35. 被引量:23
1倪莹驰,江佳阳,董凯林,时凯华.不同添加剂对(W,Mo)C-6%Ni合金性能的影响[J].硬质合金,2022,39(2):118-126.
1刘雪梅,范金莲,冯浩,宋晓艳.WC-Co硬质合金的高温氧化过程研究[J].中国体视学与图像分析,2018,23(4):343-350. 被引量:1
2刘晓伟.SH波在圆形孔洞上的散射[J].山海经,2018(11):0148-0148.
3孔德方,刘斌,张卫兵,邓涛.硬质合金表面覆钴机理及其影响因素[J].硬质合金,2018,35(6):457-466. 被引量:2
4赵克全,朱巧,汪定国.基于假设B的非凸分离定理及其在向量优化中的应用(英文)[J].重庆师范大学学报:自然科学版,2018,35(3):1-8. 被引量:1
5吴石新,陈登福,汪勤政,靳星,刘涛,龙木军,段华美.钛微合金钢连铸中TiN与TiC析出热力学研究[J].连铸,2019,44(1):28-34. 被引量:10
6蓓亦,韩波,胡慧文,龙伟,王丽,蔡正茂,王慧艳,虞斌.新生育政策下孕妇年龄的变化及对母婴并发症的影响[J].中华围产医学杂志,2019,22(3):157-163. 被引量:29
7李鹏飞,范景莲,章曼,冯康杰,韩勇,田家敏.烧结温度对W-40vol%ZrC性能与组织的影响[J].稀有金属材料与工程,2019,48(1):335-340.
8张力简介[J].技术与创新管理,2019,40(2).
9王宜豹,黄楠,刘鲁生,袁子尧,李鹏,张文雪,姜辛.加工7075航空铝合金用金刚石涂层刀具的制备及其切削性能[J].材料研究学报,2019,33(1):15-26. 被引量:12
10信德.亚丁湾安全了么?[J].珠江水运,2019,0(6):51-51.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
In order to improve the status quo that the commonly used cutter pick in coal mining engineering is easy to failure due to the damage of the carbide bit,the effects of TiC and TaC additives on the performance of WC-Co cemented carbide bit were studied.The results show that the structural hardness (HRA)of the treated bit can reach 87 ,which is much higher than the national standard of cutter pick of 65.Compared with the interior,the surface fracture toughness of the cutter pick is lower due to the formation of a large number of carbides on the surface,the average fracture toughness is about 15.50 MPa ·m^1/2.The internal fracture toughness is improved due to the presence of a large number of non-carbides,and its average value is 16.31 MPa ·m^1/2.
quote
| GB/T 7714-2015 | [1] WANG Ze-yu, WANG Hong-fu, ZHAO Wen, et al. Study on Performance Improvement of WC-Co Cemented Carbide by TiC/TaC Additive[J]. Rare Metals and Cemented Carbides, 2019(1): 70-73. |
| MLA | [1] WANG Ze-yu, et al., "Study on Performance Improvement of WC-Co Cemented Carbide by TiC/TaC Additive." Rare Metals and Cemented Carbides, no. 1, 2019, pp. 70-73. |
| APA | [1] WANG Ze-yu, WANG Hong-fu, ZHAO Wen, WANG Guang, & WANG Hai-peng. (2019). Study on Performance Improvement of WC-Co Cemented Carbide by TiC/TaC Additive. Rare Metals and Cemented Carbides(1), 70-73. |
| IEEE | [1] WANG Ze-yu, WANG Hong-fu, ZHAO Wen, WANG Guang, and WANG Hai-peng, "Study on Performance Improvement of WC-Co Cemented Carbide by TiC/TaC Additive," Rare Metals and Cemented Carbides, no. 1, pp. 70-73, 2019. keywords: {TiC;TaC;WC-Co cemented carbide;cutter pick structure;wear resistance;fracture toughness} |