Study on the Influence of VC and TiC on Friction and Wear Properties of Binderless WC-based Cemented Carbide AITranslate
Abstract AITranslate
The friction and wear properties of binderless WC-based cemented carbide with different VC and TiC concentration were investigated.The experimental results show that the average friction coefficient and wear rate of cemented carbide decrease with the increase of VC and TiC content.The minimum wear rate of 4.6× 10^-5 mm^3/Nm is obtained when the mola concentration of VC and TiC are 5%,which is reduced by about 98% compares with that of cemented carbide without VC or TIC'.The wear resistance of cemented carbide is positively correlated with its hardness.The hardness of cemented carbide without or with low content of VC and TiC is lower,and its wear mechanism is mainly adhesive wear and abrasive wear,and the wear rate is higher.The hardness of cemented carbide with high VC and TiC content is higher,and its wear mechanism is mainly grain pullout and surface cracking,and the wear rate is lower.
KeyWords AITranslate
1张辉,邓建新,李桂玉.晶粒尺寸对WC硬质合金刀具材料摩擦磨损性能的影响[J].工具技术,2010,44(6):9-12. 被引量:15
2刘超.无粘结相硬质合金的发展及展望[J].中国材料进展,2016,35(8):622-628. 被引量:7
3李海艳,刘宁.VC对WC-6.5%Co硬质合金组织和性能的影响[J].硬质合金,2009,26(4):206-211. 被引量:14
4张端锋,江垚,吝楠,吴冲浒,杜勇,贺跃辉.WC-TiC-Ni硬质合金的制备与性能[J].粉末冶金材料科学与工程,2011,16(2):303-308. 被引量:11
5李大梅,尤显卿,许育东,刘宁,石敏.氧化铝基陶瓷材料断裂韧性的测量与评价[J].硬质合金,2004,21(4):231-236. 被引量:7
1陈振磊,喻琛,邵鸣宇.不同粘结相硬质合金的研究进展[J].机械研究与应用,2021,34(5):204-209. 被引量:2
2范益,李伟,王锟艺,王晓斌,邹家生,刘坤,严铿.12MnNiVR钢板大热输入焊接接头组织与性能[J].压力容器,2023,40(3):21-27.
3邹芹,李壮,李艳国,贺文全,罗永安.中熵碳化物陶瓷TiC_(0.4)/VC/NbC结合的WC基硬质合金合成与性能[J].中国有色金属学报,2023,33(6):1914-1923.
1张云龙,牛楚涵,牛广津,张宇民,李启荣,高志杨,张唯一.La_(2)O_(3)掺杂量对WC-12Co硬质合金微观结构和硬度的影响[J].中国钨业,2022,37(2):53-59.
2胡启明,廖宇.贫碳WC-12%(Co+Ni)硬质合金微观组织与性能[J].硬质合金,2023,40(1):66-72.
1胡涛,胡忠举,郭世柏,郭涛.无粘结相WC基硬质合金刀具材料的研究现状与前景[J].工具技术,2019,53(2):7-11. 被引量:8
2张静,单磊,苏晓磊,李金龙,董敏鹏.基体材料对Cr/CrN多层涂层在海水环境中磨蚀性能的影响[J].表面技术,2018,47(12):198-204. 被引量:2
3王宝伟.浅谈高边坡加固中预应力锚索的控制要点及措施[J].河南建材,2019(2):306-308. 被引量:3
4颜新宇,王守仁,王勇.碳化钨基硬质合金的制备与力学性能研究[J].山东科学,2018,31(3):28-33. 被引量:1
5张超,花银群,帅文文,李志宝.激光冲击对WC-Co硬质合金微观结构和残余应力的影响[J].表面技术,2018,47(4):230-235. 被引量:6
6廖江雄,徐纯芳,聂婭.WC-Co合金中晶粒形貌的演变机制及其对合金性能的影响[J].硬质合金,2018,35(1):63-68. 被引量:4
7胡辉,周燕,文世峰,魏青松.激光选区熔化成形TiB_2增强S136模具钢[J].中国激光,2018,45(12):125-134. 被引量:6
8刘明,张伟,王海斗,王海军,刘天寅,王晶晨.涂层在冲击式压入条件下的失效机理及声发射信号特征[J].材料保护,2018,51(12):125-131.
9肖桥平,张立,罗国凯,崔焱茗,吴厚平,黄龙.无金属粘结相TiCN基金属陶瓷在NaOH溶液中的电化学腐蚀行为[J].粉末冶金材料科学与工程,2019,24(2):120-128. 被引量:7
10宋巍,郑才涛,孙晓峰,黄元林,从众帅.热浸镀铝/微弧氧化处理20钢工艺方法及性能研究[J].装甲兵工程学院学报,2018,32(6):107-111. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The friction and wear properties of binderless WC-based cemented carbide with different VC and TiC concentration were investigated.The experimental results show that the average friction coefficient and wear rate of cemented carbide decrease with the increase of VC and TiC content.The minimum wear rate of 4.6× 10^-5 mm^3/Nm is obtained when the mola concentration of VC and TiC are 5%,which is reduced by about 98% compares with that of cemented carbide without VC or TIC'.The wear resistance of cemented carbide is positively correlated with its hardness.The hardness of cemented carbide without or with low content of VC and TiC is lower,and its wear mechanism is mainly adhesive wear and abrasive wear,and the wear rate is higher.The hardness of cemented carbide with high VC and TiC content is higher,and its wear mechanism is mainly grain pullout and surface cracking,and the wear rate is lower.
quote
| GB/T 7714-2015 | [1] CHEN Lin-bo, LI Chang-sheng, ZHANG Shuai, et al. Study on the Influence of VC and TiC on Friction and Wear Properties of Binderless WC-based Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2019(1): 74-79. |
| MLA | [1] CHEN Lin-bo, et al., "Study on the Influence of VC and TiC on Friction and Wear Properties of Binderless WC-based Cemented Carbide." Rare Metals and Cemented Carbides, no. 1, 2019, pp. 74-79. |
| APA | [1] CHEN Lin-bo, LI Chang-sheng, ZHANG Shuai, & LI Jian-feng. (2019). Study on the Influence of VC and TiC on Friction and Wear Properties of Binderless WC-based Cemented Carbide. Rare Metals and Cemented Carbides(1), 74-79. |
| IEEE | [1] CHEN Lin-bo, LI Chang-sheng, ZHANG Shuai, and LI Jian-feng, "Study on the Influence of VC and TiC on Friction and Wear Properties of Binderless WC-based Cemented Carbide," Rare Metals and Cemented Carbides, no. 1, pp. 74-79, 2019. keywords: {tungsten carbide;vanadium carbide;titanum carbide;binderless cemented carbide;friction and wear propertiess} |