daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A note on “Barrel Compression Test”: A method for evaluation of friction AITranslate

Sharif University of Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Friction plays an important role in metal forming operations. Therefore, many techniques are developed for evaluation of friction in large deformation processes. Among them the “Barrel Compression Test” (BCT) is a very simple method that quantitatively evaluates the constant friction factor, m, simply by compressing a cylindrical specimen. BCT was analyzed by Avitzur [B. Avitzur, Metal Forming Processes and Analysis, McGraw-Hill, 1968] using the upper bound theory. Ebrahimi et al. [R. Ebrahimi, A. Najafizadeh, J. Mater. Process. Technol. 152 (2004) 136–143] suggested a method in order to make Avitzur’s mathematical results applicable. However, they made an assumption in their work which results in some miscalculations. In this note their mathematical analysis is corrected and also the method is modified.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.04.047

Chinese Library Classification Number:

Citation Information:

Friction plays an important role in metal forming operations. Therefore, many techniques are developed for evaluation of friction in large deformation processes. Among them the “Barrel Compression Test” (BCT) is a very simple method that quantitatively evaluates the constant friction factor, m, simply by compressing a cylindrical specimen. BCT was analyzed by Avitzur [B. Avitzur, Metal Forming Processes and Analysis, McGraw-Hill, 1968] using the upper bound theory. Ebrahimi et al. [R. Ebrahimi, A. Najafizadeh, J. Mater. Process. Technol. 152 (2004) 136–143] suggested a method in order to make Avitzur’s mathematical results applicable. However, they made an assumption in their work which results in some miscalculations. In this note their mathematical analysis is corrected and also the method is modified.

quote

GB/T 7714-2015 [1] Soheil Solhjoo. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.04.047.
MLA [1] Soheil Solhjoo. Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.04.047.
APA [1] Soheil Solhjoo. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.04.047
IEEE [1] Soheil Solhjoo, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.04.047.