First principles study on electronic structures and properties of Sn-doped rutile TiO2 AITranslate

Jiangsu University; Jiangsu University; Jiangsu University; Fudan University; Fudan University; Jiangsu University;Suzhou Institute of Nano-tech and Nano-bionics
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Density functional theory calculations have been carried out to determine the effects of Sn doping on the geometrical and electronic properties of rutile TiO2. According to calculations, the effect of Sn on energy band structure depends on its substitutional sites in the rutile lattice. The substitution sites of Sn in rutile TiO2 induces effective reduction of the energy gap, with the energy gap being continuously increased when decreasing Sn doping level. On the other hand, when Sn is in the interstitial site of rutile TiO2, and then this interstitial doping is not energetically preferred, the excitation energy increases slightly compared with the undoped case due to the a significant local structure distortion. The results provide explanations not only for the red-shift of the optical absorption edge in different experiments, but also for the electronic properties of Sn-doped rutile TiO2, with a certain potential use in many fields.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.05.034

Chinese Library Classification Number:

Citation Information:

Density functional theory calculations have been carried out to determine the effects of Sn doping on the geometrical and electronic properties of rutile TiO2. According to calculations, the effect of Sn on energy band structure depends on its substitutional sites in the rutile lattice. The substitution sites of Sn in rutile TiO2 induces effective reduction of the energy gap, with the energy gap being continuously increased when decreasing Sn doping level. On the other hand, when Sn is in the interstitial site of rutile TiO2, and then this interstitial doping is not energetically preferred, the excitation energy increases slightly compared with the undoped case due to the a significant local structure distortion. The results provide explanations not only for the red-shift of the optical absorption edge in different experiments, but also for the electronic properties of Sn-doped rutile TiO2, with a certain potential use in many fields.

quote

GB/T 7714-2015 [1] Xiaohui Yu, Changsheng Li, Hua Tang, et al. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.05.034.
MLA [1] Xiaohui Yu, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.05.034.