Light-Switchable Adhesion of Azobenzene-Containing Siloxane-Based Tough Adhesive AITranslate
Abstract AITranslate
An azobenzene-containing siloxane-based adhesive polymer was synthesized with azobenzene moieties as hard segments and siloxane moieties as soft segments. Upon UV irradiation, the adhesive energies decreased to 1.9% of the original values, and subsequent green light exposure raised adhesive energies to 98.3% of the original values. The light-switchable adhesion was applicable to various substrates. Attractively, a polymer-glued plastic ring could be reversibly opened and closed by respective exposure to UV and green light with pressure on the adhesive position. Such a strategy may be applicable for designing light-switchable tough adhesives.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00170
Chinese Library Classification Number:
Citation Information:
An azobenzene-containing siloxane-based adhesive polymer was synthesized with azobenzene moieties as hard segments and siloxane moieties as soft segments. Upon UV irradiation, the adhesive energies decreased to 1.9% of the original values, and subsequent green light exposure raised adhesive energies to 98.3% of the original values. The light-switchable adhesion was applicable to various substrates. Attractively, a polymer-glued plastic ring could be reversibly opened and closed by respective exposure to UV and green light with pressure on the adhesive position. Such a strategy may be applicable for designing light-switchable tough adhesives.
quote
| GB/T 7714-2015 | [1] Peng Zhang, Feng Cai, Wenzhong Wang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00170. |
| MLA | [1] Peng Zhang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00170. |
| APA | [1] Peng Zhang, Feng Cai, Wenzhong Wang, Guojie Wang, & Haifeng Yu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00170 |
| IEEE | [1] Peng Zhang, Feng Cai, Wenzhong Wang, Guojie Wang, and Haifeng Yu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00170. keywords: {lightswitchable;azobenzene polymer;tough;adhesive;reusability} |