Thermoelectric and Charge Transport Properties of Solution-Processable and Chemically Doped Dioxythienothiophene Copolymers AITranslate
Abstract AITranslate
This study reports the electronic properties of a family of 3,6-dioxythienothiophene copolymer thin films (referred to as DOTTs) as a function of F4TCNQ doping level. We find that DOTTs have unusually low Seebeck coefficients and that the dependence on carrier concentration could not be accurately explained with present transport models. Furthermore, electrical conductivities were measured as a function of temperature, and some polymer/dopant systems demonstrated unusually low activation energies. The Mott polaron model transport parameters were further evaluated to quantify the effects of carrier concentration. Overall, this work discusses the electronic properties of DOTTs and provides guidance for designing polymer chemistries.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00093
Chinese Library Classification Number:
Citation Information:
This study reports the electronic properties of a family of 3,6-dioxythienothiophene copolymer thin films (referred to as DOTTs) as a function of F4TCNQ doping level. We find that DOTTs have unusually low Seebeck coefficients and that the dependence on carrier concentration could not be accurately explained with present transport models. Furthermore, electrical conductivities were measured as a function of temperature, and some polymer/dopant systems demonstrated unusually low activation energies. The Mott polaron model transport parameters were further evaluated to quantify the effects of carrier concentration. Overall, this work discusses the electronic properties of DOTTs and provides guidance for designing polymer chemistries.
quote
| GB/T 7714-2015 | [1] Shawn A. Gregory, James F. Ponder, Jr., Sandra L. Pittelli, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00093. |
| MLA | [1] Shawn A. Gregory, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00093. |
| APA | [1] Shawn A. Gregory, James F. Ponder, Jr., Sandra L. Pittelli, Mark D. Losego, John R. Reynolds, & Shannon K. Yee. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00093 |
| IEEE | [1] Shawn A. Gregory, James F. Ponder, Jr., Sandra L. Pittelli, Mark D. Losego, John R. Reynolds, and Shannon K. Yee, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00093. keywords: {semiconducting polymers;redox doping;charge transport;polymer thermoelectrics;organic electronics} |