Catalytic Amine Functionalization and Polymerization of Cyclic Alkenes Creates Adhesive and Self-Healing Materials AITranslate
Abstract AITranslate
The chemical functionalization of polyolefins to access responsive materials is a long-standing challenge in materials science. Current protocols do not typically tolerate polar functional groups, and postpolymerization modification often leads to material defects. Here the catalytic synthesis of amine-functionalized polyolefins has been achieved using a two-step catalytic combination of hydroaminoalkylation and ring-opening metathesis polymerization (ROMP). Furthermore, reduction was used to obtain an aminated polyethylene analogue. This preparation transforms simple starting materials into polar-functionalized polymers with complete atom economy. Utilizing dynamic associative interactions, including hydrogen bonding, these materials demonstrate tunable rheological properties, autonomous self-healing, and unexpected adhesion to polytetrafluoroethylene (PTFE).
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00158
Chinese Library Classification Number:
Citation Information:
The chemical functionalization of polyolefins to access responsive materials is a long-standing challenge in materials science. Current protocols do not typically tolerate polar functional groups, and postpolymerization modification often leads to material defects. Here the catalytic synthesis of amine-functionalized polyolefins has been achieved using a two-step catalytic combination of hydroaminoalkylation and ring-opening metathesis polymerization (ROMP). Furthermore, reduction was used to obtain an aminated polyethylene analogue. This preparation transforms simple starting materials into polar-functionalized polymers with complete atom economy. Utilizing dynamic associative interactions, including hydrogen bonding, these materials demonstrate tunable rheological properties, autonomous self-healing, and unexpected adhesion to polytetrafluoroethylene (PTFE).
quote
| GB/T 7714-2015 | [1] Damon J. Gilmour, Tanja Tomkovic, Nirmalendu Kuanr, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00158. |
| MLA | [1] Damon J. Gilmour, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00158. |
| APA | [1] Damon J. Gilmour, Tanja Tomkovic, Nirmalendu Kuanr, Mitchell R. Perry, Hans Gildenast, Savvas G. Hatzikiriakos, & Laurel L. Schafer. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00158 |
| IEEE | [1] Damon J. Gilmour, Tanja Tomkovic, Nirmalendu Kuanr, Mitchell R. Perry, Hans Gildenast, Savvas G. Hatzikiriakos, and Laurel L. Schafer, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00158. keywords: {amines;polyolefins;aminecontaining polymer;hydroaminoalkylation;ROMP;hydrogen bonding;selfhealing;adhesion} |