Constructing S-scheme charge separation in cobalt phthalocyanine/oxygen-doped g-C3N4 heterojunction with enhanced photothermal-assisted photocatalytic H2 evolution AITranslate

School of Material Science and Engineering;School of Material Science and Engineering;School of Material Science and Engineering;School of Material Science and Engineering;School of Material Science and Engineering;School of Material Science and Engineering;School of Material Science and Engineering;School of Material Science and Engineering;School of Material Science and Engineering
AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hydrogen acquisition from solar energy is an effective way to address energy crisis,which makes the development of efficient photocatalysts become the main direction of scientific research.Herein,cobalt phthalocyanine/oxygen-doped g-C3N4(CoPc/OCN) S-scheme heterojunction photocatalyst was designed by coupling multi-step calcination with solvothermal method for enhanced photothermal-assisted photocatalytic H2 evolution.The multistep calcined g-C3N4 is easier for O-doping formation,and the ethanol solvothermal strategy is utilized to enhance the dispersion of CoPc on OCN nano sheet surface and forms sufficient S-scheme heterojunction through H-bonds.In addition,the active sites and excellent photothermal properties of CoPc itself further improve the integrated photocatalytic activity of CoPc/OCN S-scheme heterojunction.The optimal photocatalytic hydrogen evolution rate of CoPc/OCN S-scheme heterojunction photocatalyst reached 9.56 mmol·g-1·h-1,which is 2.69 and 1.23 times higher than that of CN and OCN,respectively.This work provides a valuable design idea and scheme for enhancing the multi-factor co-assisted photocatalytic H2 evolution performance.

KeyWords AITranslate

PHOTOTHERMAL Photocatalytic H2evolution Cobalt phthalocyanine Oxygen-doped g-C3N4 Sscheme heterojunction

1Xin-Long Zheng,Ying-Jie Yang,Yu-Hao Liu,Pei-Lin Deng,Jing Li,Wei-Feng Liu,Peng Rao,Chun-Man Jia,Wei Huang,Yan-Lian Du,Yi-Jun Shen,Xin-Long Tian.Fundamentals and photocatalytic hydrogen evolution applications of quaternary chalcogenide semiconductor:Cu_(2)ZnSnS_(4)[J].Rare Metals,2022,41(7):2153-2168. 被引量:3

2Syed Zulfiqar,Song Liu,Nasir Rahman,Hua Tang,Sufaid Shah,Xiao-Hui Yu,Qin-Qin Liu.Construction of S-scheme MnO_(2)@CdS heterojunction with core–shell structure as H_(2)-production photocatalyst[J].Rare Metals,2021,40(9):2381-2391. 被引量:10

3Li-Juan Sun,Hai-Wei Su,Di-Fa Xu,Le-Le Wang,Hua Tang,Qin-Qin Liu.Carbon hollow spheres as cocatalyst of Cu-doped TiO_(2)nanoparticles for improved photocatalytic H_(2)generation[J].Rare Metals,2022,41(6):2063-2073. 被引量:6

4Yang Ding,Soumyajit Maitra,Chunhua Wang,Runtian Zheng,Meiyu Zhang,Tarek Barakat,Subhasis Roy,Jing Liu,Yu Li,Tawfique Hasan,Bao-Lian Su.Hydrophilic bi-functional B-doped g-C_(3)N_(4) hierarchical architecture for excellent photocatalytic H_(2)O_(2) production and photoelectrochemical water splitting[J].Journal of Energy Chemistry,2022,31(7):236-247. 被引量:5

5白浚贤,沈荣晨,姜志民,张鹏,李佑稷,李鑫.集成二维层状CdS/WO_(3)S型异质结及金属化Ti_(3)C_(2)MXene基欧姆结高效光催化产氢[J].Chinese Journal of Catalysis,2022,43(2):359-369. 被引量:14

6吴健豪,赵婉,陈默,刘纯希,陈金超,陈智.无铅卤化物钙钛矿可见光催化研究进展[J].稀有金属,2022,46(1):96-108. 被引量:7

7Weijie Zhang,Xizhong Zhou,Jinzhao Huang,Shouwei Zhang,Xijin Xu.Noble metal-free core-shell CdS/iron phthalocyanine Z-scheme photocatalyst for enhancing photocatalytic hydrogen evolution[J].Journal of Materials Science & Technology,2022(20):199-207. 被引量:1

8Yang Li,Qinling Zhou,Jiating Wu,Junhua Xu,Weilong Shi,Chao Su,Daifen Chen,Zongping Shao.Controllably grown single-crystal films as flexoelectric nanogenerators for continuous direct current output[J].npj Flexible Electronics,2022,6(1):885-891. 被引量:2

9Feng Guo,Chunli Shi,Wei Sun,Yanan Liu,Xue Lin,Weilong Shi.Pomelo biochar as an electron acceptor to modify graphitic carbon nitride for boosting visible-light-driven photocatalytic degradation of tetracycline[J].Chinese Journal of Chemical Engineering,2022,35(8):1-11. 被引量:2

10Feng Guo,Zhihao Chen,Xiliu Huang,Longwen Cao,Xiaofang Cheng,Weilong Shi,Lizhuang Chen.Ternary Ni_(2)P/Bi_(2)MoO_(6)/g-C_(3)N_(4)composite with Z-scheme electron transfer path for enhanced removal broad-spectrum antibiotics by the synergistic effect of adsorption and photocatalysis[J].Chinese Journal of Chemical Engineering,2022,35(4):157-168. 被引量:2

1吴新鹤,谭丽红,陈郭强,康佳乐,王国宏.g-C_(3)N_(4)基S型异质结光催化剂[J].Science China Materials,2024,67(2):444-472. 被引量:1

1Jiaguo Yu,Xin Li,Junwei Fu,Kai Dai.Editorial:special topic on heterojunction in photocatalysts[J].Science China Materials,2024,67(2):379-381.

1Jianlin Jiang,Zhen Liu,Shuaijun Pan,Xinnian Xia,Bing Qin,Yang Hu,Xuxu Wang,Jiamin Lan,Yu Gu,Encai Ou,Weijian Xu,Joseph J.Richardson,Rui Guo.Tuning electronic properties of cobalt phthalocyanines for oxygen reduction and evolution reactions[J].Science China Chemistry,2024,67(1):398-407.

2Ye Yuan,Junan Pan,Weinan Yin,Haoxuan Yu,Fengshun Wang,Weifeng Hu,Longlu Wang,Dafeng Yan.Effective strategies to promote Z(S)-scheme photocatalytic water splitting[J].Chinese Chemical Letters,2024,35(3):27-39.

3Wang Nengquan.Review of the Global Energy Market in 2023[J].China Oil & Gas,2024,31(1):22-26.

4Muwang Wu,Hao Liang,Mingjie Zhang,Dianqiang Sun,Peng Zhong.Productivity Testing Design Method of Multi-Factor Control for Unconsolidated Sandstone Gas Reservoir[J].Engineering(科研),2016,8(11):815-822.

5Yuntian Liao,Rongtao Zhu,Wenjun Zhang,Haiyang Zhu,Yang Sun,Jiale Chen,Zhenhua Dong,Ronghuan Lv.Transient synthesis of carbon-supported high-entropy alloy sulfide nanoparticles via flash Joule heating for efficient electrocatalytic hydrogen evolution[J].Nano Research,2024,17(4):3379-3389. 被引量:1

6Junjun Zhang,Huiying Lu,Tianhao Yao,Xin Ji,Qingmiao Zhang,Lingjie Meng,Jianmin Feng,Hongkang Wang.Copper-induced formation of heterostructured Co_(3)O_(4)/CuO hollow nanospheres towards greatly enhanced lithium storage performance[J].Chinese Chemical Letters,2024,35(2):594-598.

7TANG Yang-yang,CUI Ying-ying,JIANG Yan-yan,SHAO Ming-zhu,ZANG Xin-xin,DANG Guang-hui,LIU Si-guo.Characteristics of Mycobacterium tuberculosis serine protease Rv1043c in enzymology and pathogenicity in mice[J].Journal of Integrative Agriculture,2023,22(12):3755-3768.

8Yao Wang,Qing Ye,Jinlong Li,Qingqing Rui,Azhi Yu.Economic and entropy production evaluation of extractive distillation and solvent-assisted pressure-swing distillation by multi-objective optimization[J].Chinese Journal of Chemical Engineering,2023,63(11):246-259.

9Dongchen Han,Nanxing Gao,Yuyi Chu,Zhaoping Shi,Ying Wang,Junjie Ge,Meiling Xiao,Changpeng Liu,Wei Xing.Key role of electron accessibility at the noble metal-free catalytic interface in hydrogen evolution reaction[J].Nano Research,2024,17(4):2538-2545.

10Wenjin Dong,Jian Liu.NAD(P)H inspired CO_(2) reduction and beyond[J].Science China Chemistry,2024,67(4):1044-1046.

Basic Information:

DOI:

Chinese Library Classification Number:O643.36[理学—物理化学];O644.1[理学—物理化学];TQ116.2[化学工程—无机化工]

Citation Information:

Hydrogen acquisition from solar energy is an effective way to address energy crisis,which makes the development of efficient photocatalysts become the main direction of scientific research.Herein,cobalt phthalocyanine/oxygen-doped g-C3N4(CoPc/OCN) S-scheme heterojunction photocatalyst was designed by coupling multi-step calcination with solvothermal method for enhanced photothermal-assisted photocatalytic H2 evolution.The multistep calcined g-C3N4 is easier for O-doping formation,and the ethanol solvothermal strategy is utilized to enhance the dispersion of CoPc on OCN nano sheet surface and forms sufficient S-scheme heterojunction through H-bonds.In addition,the active sites and excellent photothermal properties of CoPc itself further improve the integrated photocatalytic activity of CoPc/OCN S-scheme heterojunction.The optimal photocatalytic hydrogen evolution rate of CoPc/OCN S-scheme heterojunction photocatalyst reached 9.56 mmol·g-1·h-1,which is 2.69 and 1.23 times higher than that of CN and OCN,respectively.This work provides a valuable design idea and scheme for enhancing the multi-factor co-assisted photocatalytic H2 evolution performance.

quote

GB/T 7714-2015 [1] Wei-Long Shi, Zheng Xu, Yu-Xing Shi, et al. Rare Metals, 2024(1): 198-211.
MLA [1] Wei-Long Shi, et al., Rare Metals, no. 1, 2024, pp. 198-211.
APA [1] Wei-Long Shi, Zheng Xu, Yu-Xing Shi, Ling-Ling Li, Jia-Lin Lu, Xin-Hai Sun, Xin Du, Feng Guo, & Chang-Yu Lu. (2024). Rare Metals(1), 198-211.
IEEE [1] Wei-Long Shi, Zheng Xu, Yu-Xing Shi, Ling-Ling Li, Jia-Lin Lu, Xin-Hai Sun, Xin Du, Feng Guo, and Chang-Yu Lu, Rare Metals, no. 1, pp. 198-211, 2024.