daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Local Atomic Configuration Control of Superconductivity in the Undoped Pnictide Parent Compound BaFe2As2 Local Atomic Configuration Control of Superconductivity in the Undoped Pnictide Parent Compound BaFe2As2 AITranslate

University of Wisconsin-Madison; Dublin City University; Argonne National Laboratory; University of Wisconsin-Madison; University of Wisconsin-Madison; University of Wisconsin-Madison; University of Wisconsin-Madison; University of Wisconsin-Madison; Iowa State University; Iowa State University; Florida State University; Florida State University; Iowa State University; University of Wisconsin-Madison; University of Wisconsin-Madison; University of Wisconsin-Madison
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Emergent superconductivity is strongly correlated with the symmetry of local atomic configuration in the parent compounds of iron-based superconductors. While chemical doping or hydrostatic pressure can change the local geometry, conventional approaches do not provide a clear pathway in predictably tuning the detailed atomic arrangement due to the parent compound’s complicated structural deformation in the presence of the tetragonal-to-orthorhombic phase transition. Here, we demonstrate a systematic approach to manipulate local structural configurations in BaFe2As2 epitaxial thin films by controlling two independent structural factors, orthorhombicity (in-plane anisotropy) and tetragonality (out-of-plane/in-plane balance), from lattice parameters. We tune superconductivity without doping utilizing both structural factors separately and controlling local tetrahedral coordination in the designed thin film heterostructures with substrate clamping and biaxial strain. We further show this allows quantitative control of the structural phase transition, the associated magnetism, and superconductivity in parent material BaFe2As2. This approach will advance the development of tunable thin film superconductors in a reduced dimension.

KeyWords AITranslate

superconductivity thin films atomic configuration phase transition parent materials
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00291

Chinese Library Classification Number:

Citation Information:

Emergent superconductivity is strongly correlated with the symmetry of local atomic configuration in the parent compounds of iron-based superconductors. While chemical doping or hydrostatic pressure can change the local geometry, conventional approaches do not provide a clear pathway in predictably tuning the detailed atomic arrangement due to the parent compound’s complicated structural deformation in the presence of the tetragonal-to-orthorhombic phase transition. Here, we demonstrate a systematic approach to manipulate local structural configurations in BaFe2As2 epitaxial thin films by controlling two independent structural factors, orthorhombicity (in-plane anisotropy) and tetragonality (out-of-plane/in-plane balance), from lattice parameters. We tune superconductivity without doping utilizing both structural factors separately and controlling local tetrahedral coordination in the designed thin film heterostructures with substrate clamping and biaxial strain. We further show this allows quantitative control of the structural phase transition, the associated magnetism, and superconductivity in parent material BaFe2As2. This approach will advance the development of tunable thin film superconductors in a reduced dimension.

quote

GB/T 7714-2015 [1] JongHoon Kang, Philip J. Ryan, JongWoo Kim, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00291.
MLA [1] JongHoon Kang, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00291.
APA [1] JongHoon Kang, Philip J. Ryan, JongWoo Kim, Jonathon Schad, Jacob P. Podkaminer, Neil Campbell, Joseph Suttle, Tae Heon Kim, Liang Luo, Di Cheng, Yesusa G. Collantes, Eric E. Hellstrom, Jigang Wang, Robert McDermott, Mark S. Rzchowski, & ChangBeom Eom. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00291
IEEE [1] JongHoon Kang, Philip J. Ryan, JongWoo Kim, Jonathon Schad, Jacob P. Podkaminer, Neil Campbell, Joseph Suttle, Tae Heon Kim, Liang Luo, Di Cheng, Yesusa G. Collantes, Eric E. Hellstrom, Jigang Wang, Robert McDermott, Mark S. Rzchowski, and ChangBeom Eom, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00291. keywords: {superconductivity thin films atomic configuration phase transition parent materials}