Among the many extraordinary qualities of graphene, its thermoelectric properties have attracted significant interest, for example, in active cooling applications. Here, we report on the thermoelectric transport properties of centimeter-sized monolayer CVD graphene, electrostatically controlled by a high-capacity ionic gel. The power factor reaches 7 and 5.4 mW m–1 K–2 for hole and electron conduction, respectively, similar to earlier reports obtained for microdevices despite our devices being over 2 orders of magnitude larger. On the basis of these results, we propose nonvolatile ferroelectric polarization as a scalable technology for graphene-based thermoelectric applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.1c00995
Chinese Library Classification Number:
Citation Information:
Among the many extraordinary qualities of graphene, its thermoelectric properties have attracted significant interest, for example, in active cooling applications. Here, we report on the thermoelectric transport properties of centimeter-sized monolayer CVD graphene, electrostatically controlled by a high-capacity ionic gel. The power factor reaches 7 and 5.4 mW m–1 K–2 for hole and electron conduction, respectively, similar to earlier reports obtained for microdevices despite our devices being over 2 orders of magnitude larger. On the basis of these results, we propose nonvolatile ferroelectric polarization as a scalable technology for graphene-based thermoelectric applications.
quote
| GB/T 7714-2015 | [1] Matthias Schrade, Wen Xing, Knut Thorshaug, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c00995. |
| MLA | [1] Matthias Schrade, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c00995. |
| APA | [1] Matthias Schrade, Wen Xing, Knut Thorshaug, & Branson D. Belle. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c00995 |
| IEEE | [1] Matthias Schrade, Wen Xing, Knut Thorshaug, and Branson D. Belle, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c00995. keywords: {graphene electrostatic doping thermoelectric ionic gel ferroelectric} |