daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Highly Cationized and Porous Hyper-cross-linked Polymer Nanospheres for Composite Anion Exchange Membranes AITranslate

Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hyper-cross-linked polymer (HCP), a category of porous organic materials (POMs), is exploited as an anion conducting membrane via a highly cationized and porous quaternized ammonium triptycene-based HCP in the form of <100 nm nanospheres (QTP-HCP-NS) for the first time. The material possesses a high ion density of 3.65 mmol g–1 as well as a high Brunauer–Emmett–Teller (BET) surface area of 706 m2 g–1. Anion exchange membranes (AEMs) are prepared by mixing different loadings of QTP-HCP-NS with quaternized poly(phenylene oxide) (QPPO) and compared with a compressed QTP-HCP pellet. Owing to the high ion density and high water sorption, which results in abundant ion conduction channels in QTP-HCP, the ion conductivity of the composite AEMs is enhanced by 79.5% compared with the unfilled QPPO membrane and by 677% compared with a compressed QTP-HCP pellet. In addition, lower dimensional swelling and higher tensile strength are achieved for the composite AEMs. Aggregation and the resulting interfacial defects of QTP-HCP-NS are found in the composite AEM at a high loading and in the comparative compressed pellet, causing a significant reduction in ion conduction and mechanical properties.

KeyWords AITranslate

hypercrosslinked polymer triptycene porosity anion exchange membrane fuel cell
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00934

Chinese Library Classification Number:

Citation Information:

Hyper-cross-linked polymer (HCP), a category of porous organic materials (POMs), is exploited as an anion conducting membrane via a highly cationized and porous quaternized ammonium triptycene-based HCP in the form of <100 nm nanospheres (QTP-HCP-NS) for the first time. The material possesses a high ion density of 3.65 mmol g–1 as well as a high Brunauer–Emmett–Teller (BET) surface area of 706 m2 g–1. Anion exchange membranes (AEMs) are prepared by mixing different loadings of QTP-HCP-NS with quaternized poly(phenylene oxide) (QPPO) and compared with a compressed QTP-HCP pellet. Owing to the high ion density and high water sorption, which results in abundant ion conduction channels in QTP-HCP, the ion conductivity of the composite AEMs is enhanced by 79.5% compared with the unfilled QPPO membrane and by 677% compared with a compressed QTP-HCP pellet. In addition, lower dimensional swelling and higher tensile strength are achieved for the composite AEMs. Aggregation and the resulting interfacial defects of QTP-HCP-NS are found in the composite AEM at a high loading and in the comparative compressed pellet, causing a significant reduction in ion conduction and mechanical properties.

quote

GB/T 7714-2015 [1] Tong Huang, Junfeng Zhang, Xin Liu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00934.
MLA [1] Tong Huang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00934.
APA [1] Tong Huang, Junfeng Zhang, Xin Liu, Jiandang Xue, Haifei Jiang, Yanxiong Ren, Xiaoyu Qiu, Yan Yin, Zhongyi Jiang, & Michael D. Guiver. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00934
IEEE [1] Tong Huang, Junfeng Zhang, Xin Liu, Jiandang Xue, Haifei Jiang, Yanxiong Ren, Xiaoyu Qiu, Yan Yin, Zhongyi Jiang, and Michael D. Guiver, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00934. keywords: {hypercrosslinked polymer;triptycene;porosity;anion exchange membrane;fuel cell}