daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Amphiphilic Copolymer-Based Multichannel Toolbox with Multistage Adjustable and Visualized Catalytic Properties AITranslate

Xiamen University; Xiamen University; Xiamen University; Xiamen University; Xiamen University; Xiamen University; Xiamen University; Xiamen University; Xiamen University; Xiamen University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Multiple responsive polymers have attracted increasing attention for a wide range of applications including nanocarriers and nanocomposite catalysts. Herein, an amphiphilic block copolymer P(NIPAAm-r-CA)-b-PMMA was synthesized by reversible addition–fragmentation chain-transfer polymerization with coumarin units embedded in the side chain. Followed by a reduction of the terminal group to hydrosulfonyl, relatively stable polymer microspheres can be prepared after self-assembling, and those microspheres could be further employed as carriers of gold nanoparticles (Au NPs) due to the strong interrelationship between −SH and Au. The polymer microspheres with Au NPs decorated onto the surface were endowed with reversible catalytic properties by adjusting temperature and UV irradiation owing to the introduction of photo-responsive coumarin units and thermo-responsive poly(N-isopropyl acrylamide) segments. Moreover, the catalytic performance could be retained even after several cycles of photo- or thermo-responsive regulation. Importantly, the fluorescence of the smart polymer under different pH values was studied to clarify the mechanism of emission, laying a necessary foundation for further visualization of the catalytic process.

KeyWords AITranslate

amphiphilic copolymer coumarin multiresponse multistage adjustment controllable catalysis
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00930

Chinese Library Classification Number:

Citation Information:

Multiple responsive polymers have attracted increasing attention for a wide range of applications including nanocarriers and nanocomposite catalysts. Herein, an amphiphilic block copolymer P(NIPAAm-r-CA)-b-PMMA was synthesized by reversible addition–fragmentation chain-transfer polymerization with coumarin units embedded in the side chain. Followed by a reduction of the terminal group to hydrosulfonyl, relatively stable polymer microspheres can be prepared after self-assembling, and those microspheres could be further employed as carriers of gold nanoparticles (Au NPs) due to the strong interrelationship between −SH and Au. The polymer microspheres with Au NPs decorated onto the surface were endowed with reversible catalytic properties by adjusting temperature and UV irradiation owing to the introduction of photo-responsive coumarin units and thermo-responsive poly(N-isopropyl acrylamide) segments. Moreover, the catalytic performance could be retained even after several cycles of photo- or thermo-responsive regulation. Importantly, the fluorescence of the smart polymer under different pH values was studied to clarify the mechanism of emission, laying a necessary foundation for further visualization of the catalytic process.

quote

GB/T 7714-2015 [1] Tong Shen, Chuanluan Guo, Ying Cao, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00930.
MLA [1] Tong Shen, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00930.
APA [1] Tong Shen, Chuanluan Guo, Ying Cao, Yan Lv, Jiatian Zhang, Conghui Yuan, Birong Zeng, Guorong Chen, Yiting Xu, & Lizong Dai. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00930
IEEE [1] Tong Shen, Chuanluan Guo, Ying Cao, Yan Lv, Jiatian Zhang, Conghui Yuan, Birong Zeng, Guorong Chen, Yiting Xu, and Lizong Dai, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00930. keywords: {amphiphilic copolymer;coumarin;multiresponse;multistage adjustment;controllable catalysis}