Insulating Silicones Based on Dynamic Hindered Urea Bonds with High Dielectric Healability and Recyclability AITranslate
Abstract AITranslate
Silicone-containing dynamically hindered urea bonds are developed as a smart insulating material for power equipment and electronic devices. In this work, silicones are constructed by isocyanate–piperazine-based dynamic bonds with cross-linking degree adjusted by glycerol. Healing and recycling based on dielectric and insulating properties are mainly emphasized in this study. We find that dynamic bonds not only heal the cut-damaged feature of the silicone but also enable dielectric property recovery. A healing efficiency above 95% and a recycling efficiency above 90% based on insulation performance are achieved. After recycling, cross-linked silicone exhibits only a slight variation in permittivity and tan δ, while linear silicone shows an apparent increase. Insulation performance of materials with different cross-linking agent concentrations is also investigated. A higher cross-linking degree was found to further improve insulation properties but reduces the recycling efficiency. Importantly, the developed silicones exhibit high intrinsic insulation properties, comparable to commercial silicone materials, which are very attractive for electrical applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00948
Chinese Library Classification Number:
Citation Information:
Silicone-containing dynamically hindered urea bonds are developed as a smart insulating material for power equipment and electronic devices. In this work, silicones are constructed by isocyanate–piperazine-based dynamic bonds with cross-linking degree adjusted by glycerol. Healing and recycling based on dielectric and insulating properties are mainly emphasized in this study. We find that dynamic bonds not only heal the cut-damaged feature of the silicone but also enable dielectric property recovery. A healing efficiency above 95% and a recycling efficiency above 90% based on insulation performance are achieved. After recycling, cross-linked silicone exhibits only a slight variation in permittivity and tan δ, while linear silicone shows an apparent increase. Insulation performance of materials with different cross-linking agent concentrations is also investigated. A higher cross-linking degree was found to further improve insulation properties but reduces the recycling efficiency. Importantly, the developed silicones exhibit high intrinsic insulation properties, comparable to commercial silicone materials, which are very attractive for electrical applications.
quote
| GB/T 7714-2015 | [1] Wenjie Sun, Jiaming Luo, Lei Zhang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00948. |
| MLA | [1] Wenjie Sun, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00948. |
| APA | [1] Wenjie Sun, Jiaming Luo, Lei Zhang, Yue Chen, Pengxin Li, Yiting Zheng, & Yonghong Cheng. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00948 |
| IEEE | [1] Wenjie Sun, Jiaming Luo, Lei Zhang, Yue Chen, Pengxin Li, Yiting Zheng, and Yonghong Cheng, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00948. keywords: {Silicone;dynamic chemical bonds;dielectric performance;healability;recyclability} |