Kinetic Effects of Nonisothermal Crystallization of Zr-based Bulk Amorphous Alloy AITranslate
Abstract AITranslate
The crystallization kinetics of the Zr based was investigated by differential scanning calorimetry amorphous alloys (Zr60 Al15 Ni25 and Zr65 Al10 Ni10 Cu15 ) (DSC) under nonisothermal conditions. The results show that the characteristic temperatures (Tg, Tx and Tp) of Zr60 Al15 Ni25 and Zr65 Al10 Ni10 Cu15- shift to higher ones with the increase of heating rate,and the supercooled liquid region is widened. Therefore, both the glass transition-and crystallization of Zr60Al15Ni25-and Zr65 Al10 Ni10Cu15-have kinetic effects. The activation energy of the two amorphous alloys was evaluated using Kissinger and Ozawa equations, and the resuls from the different equations are nearly equal. It can be seen from the data of activation energy,the thermal stability of the two alloys is high,and the glass transition-and initial crystallization of Zr65 Al10 Ni10Cu15-are more difficult than-those of Zr60 Al15 Ni25. However,once the crystallization starts, Zr65 Al10 Ni10Cu15-is more easier to crystallize.
KeyWords AITranslate
1卢博斯基F E.非晶态金属合金[M].北京:冶金工业出版社,1989:341.
2黄劲松,刘咏,陈仕奇,刘祖铭,黄伯云.锆基非晶合金的研究进展与应用[J].中国有色金属学报,2003,13(6):1321-1332. 被引量:39
3Qin F X,Zhang H F,Ding B Z,et al. Nanocrystallization kinetics of Ni-based bulk amorphous alloy[J]. Internatallics,2004,12(11) :1 197-1 203.
4Funakoshi N,Kanamori T,Manabe T. Crystallization kinetic of amorphous Pd-Ag-Si alloys[J]. J Appl Phys, 1979,18(10).1 885-1 889.
5Kissinger H E. Reaction kinetics in differential thermal analysis[J].Analytical Chemistry, 1957,29 ( 11 ) : 170 - 175.
6Ozawa T. Kinetic analysis of derivative curves in thermal analysis[J]. J Thermal Analysis, 1970,2 (3) : 301-324.
7Matusita K, Sakka S. Kinetic study of crystallization of glass by differential thermal-criterion on application of Kissinger plot[J]. Non-Crystalline Solids, 1980,38(39) : 741-746.
8Rohit J ,Saxena N S, Deepika B, et al. Crystallization kinetics of Cu,Ti100-x (x=43, 50 and 53) glasses[J]. Physica B,2001 ,301(4) .341-348.
9Inoue A. High strength bulk amorphous alloys with low critical cooling rates[J]. Mater Trans JIM, 1995,36 (7): 866-875.
10赵德乾,C.H.Shek,汪卫华.Zr-Ti-Cu-Ni-Be-Fe大块非晶合金晶化动力学效应[J].金属学报,2001,37(7):754-758. 被引量:21
1吉丽丽,运新兵,吕云卓.放电等离子烧结制备Zr_(50)Ti_(5)Cu_(27)Ni_(10)Al_(8)块体非晶合金[J].稀有金属,2020,44(11):1221-1226. 被引量:4
2张震,王金贺,李正坤,付华萌,杨红旺,李宏,朱正旺,张海峰.锆基非晶合金及其复合材料的非等温晶化动力学行为[J].铸造技术,2023,44(8):763-770.
1刘伟东,屈赫,屈华,杨松.Zr-Al-Ni-Cu非晶合金F-A_(2)B型晶化相析出形为[J].特种铸造及有色合金,2022,42(12):1496-1501.
2田霖,李春燕,翟建树,卢煜,寇生中.非晶合金的功能性研究进展[J].稀有金属,2021,45(8):998-1009. 被引量:6
3查越,沈学静,李明.基于纳升电喷雾-便携式离子阱质谱的苯扎氯铵快检方法[J].分析试验室,2021,40(10):1166-1170. 被引量:2
4王顺平,李春燕,王海博,李金玲,李阳,寇生中.冷-热处理对Zr基块体非晶合金结构和性能的影响[J].稀有金属材料与工程,2022,51(5):1759-1766.
1袁子洲,张香云,冯雪磊,崔立治.Cu_(60)Zr_(33)Ti_7非晶合金的非等温晶化动力学行为[J].兰州理工大学学报,2014,40(4):6-8. 被引量:1
2Zuoxiang Qin,Cuihong Li,Haifeng Zhang,Zhongguang Wang,Zhuangqi Hu,Zhiqiang Liu.Friction Stir Welding of Zr_(55)Al_(10)Ni_5Cu_(30) Bulk Metallic Glass to Crystalline Aluminum[J].材料科学技术:英文版,2009,25(6):853-856. 被引量:2
3胡勇,闫红红,宋裕,李丹,刘邦,闫志杰.不同微观结构Zr_(55)Al_(10)Ni_5Cu_(30)块体非晶合金非等温晶化动力学研究[J].铸造技术,2013,34(4):387-389. 被引量:1
4王翠霞,陈学定,魏恒斗,张静.(Ni_(0.75)Fe_(0.25))_(70)Zr_8Si_(10)B_(12)非晶合金非等温晶化行为研究[J].稀有金属,2006,30(6):828-832. 被引量:2
5何顺荣,蔡礼平,马中锋,程曙霞,陈树榆.锆基大块非晶合金及其晶化合金在0.5mol/L H_2SO_4中的腐蚀行为研究[J].材料开发与应用,2010,25(4):16-20.
6齐民,李霞,王晓东,石灿鸿.动载荷对Zr基非晶合金玻璃化转变及晶化过程影响[J].大连理工大学学报,2003,43(2):187-190.
7朱满,李俊杰,坚增运,常芳娥.Fe_(71)Nb_6B_(23)非晶薄带的非等温晶化动力学研究[J].稀有金属材料与工程,2012,41(10):1730-1734. 被引量:11
8何顺荣,吴志强,汪波,程曙霞,陈树榆.锆基大块非晶合金在NaCl溶液中的腐蚀行为[J].金属功能材料,2010,17(3):16-20. 被引量:1
9李炳,李金山,范新会,陈建.添加Y制备铜锆基大块非晶合金(英文)[J].稀有金属材料与工程,2014,43(7):1558-1561. 被引量:2
10肖超杰,刘兰俊,王知鸷,李亮,祖方遒.Zr_(65)Al_(10)Ni_(10)Cu_(15)非晶合金电阻率的研究[J].金属功能材料,2010,17(4):5-9.
Basic Information:
DOI:
Chinese Library Classification Number:TG139.8[一般工业技术—材料科学与工程]
Citation Information:
The crystallization kinetics of the Zr based was investigated by differential scanning calorimetry amorphous alloys (Zr60 Al15 Ni25 and Zr65 Al10 Ni10 Cu15 ) (DSC) under nonisothermal conditions. The results show that the characteristic temperatures (Tg, Tx and Tp) of Zr60 Al15 Ni25 and Zr65 Al10 Ni10 Cu15- shift to higher ones with the increase of heating rate,and the supercooled liquid region is widened. Therefore, both the glass transition-and crystallization of Zr60Al15Ni25-and Zr65 Al10 Ni10Cu15-have kinetic effects. The activation energy of the two amorphous alloys was evaluated using Kissinger and Ozawa equations, and the resuls from the different equations are nearly equal. It can be seen from the data of activation energy,the thermal stability of the two alloys is high,and the glass transition-and initial crystallization of Zr65 Al10 Ni10Cu15-are more difficult than-those of Zr60 Al15 Ni25. However,once the crystallization starts, Zr65 Al10 Ni10Cu15-is more easier to crystallize.
quote
| GB/T 7714-2015 | [1] WANG Bo, HE Shun-rong, WU Zhi-qiang. Kinetic Effects of Nonisothermal Crystallization of Zr-based Bulk Amorphous Alloy[J]. Rare Metals and Cemented Carbides, 2009(2): 17-21. |
| MLA | [1] WANG Bo, et al., "Kinetic Effects of Nonisothermal Crystallization of Zr-based Bulk Amorphous Alloy." Rare Metals and Cemented Carbides, no. 2, 2009, pp. 17-21. |
| APA | [1] WANG Bo, HE Shun-rong, & WU Zhi-qiang. (2009). Kinetic Effects of Nonisothermal Crystallization of Zr-based Bulk Amorphous Alloy. Rare Metals and Cemented Carbides(2), 17-21. |
| IEEE | [1] WANG Bo, HE Shun-rong, and WU Zhi-qiang, "Kinetic Effects of Nonisothermal Crystallization of Zr-based Bulk Amorphous Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 17-21, 2009. keywords: {Zr based amorphous alloy;nonisothermal crystallization;glass transition;kinetic effect;activation energy;DSC} |