Abstract AITranslate
The flow stress behavior of TA15 titanium alloy during hot compression was studied by-thermal/ mechanical model experiments. The results show that controlled by both strain rate and deforming temperature, the flow stress of the alloy decreases with deforming temperature increasing but increases with strain rate increasing. Based on experimental data,the constant in-the constitutive function of alloy hot plasticity was calculated. And the flow stress behavior is represented by a Zener-Hollomon parameter in a hyperbolic sine relationship.
KeyWords AITranslate
1朱维,韩志强,贾湛湛,赵海东,柳百成.挤压铸造铝合金弹粘塑性本构模型[J].金属学报,2008,44(4):440-444. 被引量:6
2李梁,孙健科,孟祥军.钛合金的应用现状及发展前景[J].钛工业进展,2004,21(5):19-24. 被引量:208
3徐文臣,单德彬,李春峰,吕炎.TA15钛合金的动态热压缩行为及其机理研究[J].航空材料学报,2005,25(4):10-15. 被引量:71
4J. Shen,S. S. Xie and J. H. tang (General Research Institute for Non - ferrous Metals,Beijing 100088, China).DYNAMIC RECOVERY AND DYNAMIC RECRYSTALLIZATION OF 7005 ALUMINIUM ALLOY DURING HOT COMPRESSION[J].金属学报:英文版,2000,0(1):379-386. 被引量:33
5李兴无,沙爱学,张旺峰,储俊鹏,马济民.TA15合金及其在飞机结构中的应用前景[J].钛工业进展,2003,20(4):90-94. 被引量:103
6洪权,张振祺,赵永庆,曲恒磊,魏寿庸.Ti-6Al-2Zr-1Mo-1V合金的热压变形特性及塑性流动方程[J].广东有色金属学报,2001,11(2):129-133. 被引量:14
7彭艳萍,曾凡昌,王俊杰,章怡宁,夏绍玉.国外航空钛合金的发展应用及其特点分析[J].材料工程,1997(10):3-6. 被引量:97
1李成铭,李萍,赵蒙,薛克敏.TA15钛合金高温压缩变形行为与组织研究[J].航空材料学报,2013,33(3):25-29. 被引量:14
2申发兰,陈明和,冯建超.TA15合金高温应力松弛和流变应力行为[J].宇航材料工艺,2013,43(3):114-119. 被引量:7
3王琪,文智,王斌,易丹青,钱锋.粉末冶金TA15钛合金的高温塑性变形行为[J].粉末冶金材料科学与工程,2013,18(5):647-654. 被引量:3
4赵慧俊,王宝雨,刘钢,杨雷.基于球化机理的TA15钛合金热变形统一本构模型[J].北京科技大学学报,2014,36(7):925-930. 被引量:2
5丁群燕.发动机用Ti600高温钛合金组织及力学性能研究[J].稀有金属与硬质合金,2017,45(3):41-44. 被引量:2
6丁群燕.轧制对Ti600钛合金组织及性能的影响[J].特种铸造及有色合金,2017,37(7):789-791.
7刘意,蔡雨升,姜沐池,任德春,吉海宾,雷家峰,肖旋.激光选区熔化成形高温钛合金组织与力学性能研究[J].稀有金属与硬质合金,2023,51(2):78-84.
1姚彭彭,李萍,李成铭,薛传妹,甘国强,薛克敏.TA15钛合金在相变点附近的热变形机制及组织演化[J].稀有金属与硬质合金,2015,43(1):46-52. 被引量:1
2李成铭,李萍,赵蒙,甘国强,薛克敏.TA15钛合金的热变形微观组织与织构[J].中国有色金属学报,2014,24(1):91-96. 被引量:14
3温涛,张绪虎,文秀青,阴中炜,赵磊.2219铝合金热变形行为对精密旋压成形的影响[J].宇航材料工艺,2018,48(6):45-48. 被引量:2
4龚宗辉,谢兰生,陈明和,叶建华.新型TA32钛合金板的高温拉伸变形行为[J].机械工程材料,2019,43(1):69-74. 被引量:5
5闻瑶,薛克敏,李萍,甘国强.TA15钛合金在热压缩过程中的织构演化研究[J].稀有金属与硬质合金,2014,42(5):55-59. 被引量:2
6姚彭彭,李萍,李成铭,薛传妹,薛克敏.基于摩擦修正的TA15钛合金热变形行为及加工图[J].精密成形工程,2014,6(4):46-51. 被引量:3
7闻瑶,薛克敏,李萍,甘国强,惠文.TA15钛合金高温变形多晶体塑性有限元模拟[J].塑性工程学报,2014,21(6):86-90. 被引量:3
8谭丽琴,王高潮,甘雯晴,熊城.基于应变速率循环法的TA15钛合金超塑性本构方程[J].航空材料学报,2014,34(6):21-27. 被引量:3
9王春艳,陈国亮.TA1钛合金应力松弛试验研究[J].热加工工艺,2015,44(18):78-80. 被引量:5
10姚彭彭,李萍,李成铭,薛克敏,甘国强.TA15钛合金β热变形行为及显微组织[J].稀有金属,2015,39(11):967-974. 被引量:17
1杨雷,王宝雨,刘钢,赵慧俊.基于内变量的TA15板材室温拉伸力学性能预测模型[J].中国有色金属学报,2015,25(3):652-661. 被引量:1
2瑞钢奥隆推出一款用于优化耐磨钢板选材的新型软件[J].中国矿业,2008,17(11):107-107.
3王延辉,龚冰,李冰,宋宝韫.H62黄铜合金热变形行为[J].有色金属,2010,62(2):7-10. 被引量:14
4杨瑛.WearCalcTM——用于优化耐磨钢板选材的新型软件[J].工程机械,2008,39(11):96-96.
5靳力,吴建军,朱彤.薄铝板淬火换热系数求解[J].锻压装备与制造技术,2012,47(3):93-95. 被引量:1
6鲁福魁.异种钢焊缝熔合区边界氢致裂纹敏感性研究[J].现代焊接,2007(6):26-30.
7薛勇,张治民,杨勇彪.Mg-11.21Gd-2.26Y-0.44Zr稀土镁合金热变形行为[J].塑性工程学报,2011,18(6):58-63. 被引量:7
8傅晓,于九明,陈海耿.包铜钢线热浸镀过程的简化模型[J].金属学报,2000,36(8):828-832. 被引量:3
9曾祥国,盛鹰,韩悌信,陈军,陈华燕.考虑热粘塑性钛合金动态本构关系及其实验验证[J].四川大学学报:工程科学版,2014,46(6):152-157. 被引量:12
10魏智,王惠森,孙东昌.形状记忆合金紧缩滞回型伪弹性的数学模型及振动分析[J].河北工业大学学报,2001,30(5):1-5.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]
Citation Information:
The flow stress behavior of TA15 titanium alloy during hot compression was studied by-thermal/ mechanical model experiments. The results show that controlled by both strain rate and deforming temperature, the flow stress of the alloy decreases with deforming temperature increasing but increases with strain rate increasing. Based on experimental data,the constant in-the constitutive function of alloy hot plasticity was calculated. And the flow stress behavior is represented by a Zener-Hollomon parameter in a hyperbolic sine relationship.
quote
| GB/T 7714-2015 | [1] JI Ren-feng, MIN Xin-hua, HU Hong-jian, et al. Study on Flow Stress Behavior of TA15 Titanium Alloy during High Temperature Plastic Deformation[J]. Rare Metals and Cemented Carbides, 2009(2): 12-16. |
| MLA | [1] JI Ren-feng, et al., "Study on Flow Stress Behavior of TA15 Titanium Alloy during High Temperature Plastic Deformation." Rare Metals and Cemented Carbides, no. 2, 2009, pp. 12-16. |
| APA | [1] JI Ren-feng, MIN Xin-hua, HU Hong-jian, & LIAO Hong-jun. (2009). Study on Flow Stress Behavior of TA15 Titanium Alloy during High Temperature Plastic Deformation. Rare Metals and Cemented Carbides(2), 12-16. |
| IEEE | [1] JI Ren-feng, MIN Xin-hua, HU Hong-jian, and LIAO Hong-jun, "Study on Flow Stress Behavior of TA15 Titanium Alloy during High Temperature Plastic Deformation," Rare Metals and Cemented Carbides, no. 2, pp. 12-16, 2009. keywords: {TA15 titanium alloy;high temperature plastic deformation;Zener-Hollomon parameter;flow stress} |