Additive Manufacturing of Conducting Polymers: Recent Advances, Challenges, and Opportunities AITranslate
Abstract AITranslate
Conducting polymers (CPs) have been attracting great attention in the development of (bio)electronic devices. Most of the current devices are rigid two-dimensional systems and possess uncontrollable geometries and architectures that lead to poor mechanical properties presenting ion/electronic diffusion limitations. The goal of the article is to provide an overview about the additive manufacturing (AM) of conducting polymers, which is of paramount importance for the design of future wearable three-dimensional (3D) (bio)electronic devices. Among different 3D printing AM techniques, inkjet, extrusion, electrohydrodynamic, and light-based printing have been mainly used. This review article collects examples of 3D printing of conducting polymers such as poly(3,4-ethylene-dioxythiophene), polypyrrole, and polyaniline. It also shows examples of AM of these polymers combined with other polymers and/or conducting fillers such as carbon nanotubes, graphene, and silver nanowires. Afterward, the foremost applications of CPs processed by 3D printing techniques in the biomedical and energy fields, that is, wearable electronics, sensors, soft robotics for human motion, or health monitoring devices, among others, will be discussed.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00252
Chinese Library Classification Number:
Citation Information:
Conducting polymers (CPs) have been attracting great attention in the development of (bio)electronic devices. Most of the current devices are rigid two-dimensional systems and possess uncontrollable geometries and architectures that lead to poor mechanical properties presenting ion/electronic diffusion limitations. The goal of the article is to provide an overview about the additive manufacturing (AM) of conducting polymers, which is of paramount importance for the design of future wearable three-dimensional (3D) (bio)electronic devices. Among different 3D printing AM techniques, inkjet, extrusion, electrohydrodynamic, and light-based printing have been mainly used. This review article collects examples of 3D printing of conducting polymers such as poly(3,4-ethylene-dioxythiophene), polypyrrole, and polyaniline. It also shows examples of AM of these polymers combined with other polymers and/or conducting fillers such as carbon nanotubes, graphene, and silver nanowires. Afterward, the foremost applications of CPs processed by 3D printing techniques in the biomedical and energy fields, that is, wearable electronics, sensors, soft robotics for human motion, or health monitoring devices, among others, will be discussed.
quote
| GB/T 7714-2015 | [1] Miryam CriadoGonzalez, Antonio DominguezAlfaro, Naroa LopezLarrea, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00252. |
| MLA | [1] Miryam CriadoGonzalez, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00252. |
| APA | [1] Miryam CriadoGonzalez, Antonio DominguezAlfaro, Naroa LopezLarrea, Nuria Alegret, & David Mecerreyes. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00252 |
| IEEE | [1] Miryam CriadoGonzalez, Antonio DominguezAlfaro, Naroa LopezLarrea, Nuria Alegret, and David Mecerreyes, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00252. keywords: {conducting polymers;additive manufacturing;3D printing;PEDOT;electronic applications;inks;bioelectronics} |