daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Use of Quadruple Hydrogen Bonding as the Switching Phase in Thermo- and Light-Responsive Shape Memory Hydrogel AITranslate

Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Université de Sherbrooke
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

2-Ureido-4[1H]-pyrimidinone (UPy) is widely deployed in bulk materials for switching phase or physical cross-linking because of exceptional quadruple H-bond strength and thermal reversibility. However, utilization of UPy dimers as the switching phase to prepare shape memory hydrogels has been rarely explored due to the competition with water molecules. Herein, hydrogels with high UPy contents are synthesized and exhibit excellent shape memory ability, even at high water contents. By introduction of tetraphenylporphyrin into hydrogels, the shape memory behavior can further be controlled by light through a photothermal effect. This finding offers possibilities for applications of UPy in developing shape memory hydrogels.

KeyWords AITranslate

UPy switching phase thermal reversible hydrogel shape memory
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00230

Chinese Library Classification Number:

Citation Information:

2-Ureido-4[1H]-pyrimidinone (UPy) is widely deployed in bulk materials for switching phase or physical cross-linking because of exceptional quadruple H-bond strength and thermal reversibility. However, utilization of UPy dimers as the switching phase to prepare shape memory hydrogels has been rarely explored due to the competition with water molecules. Herein, hydrogels with high UPy contents are synthesized and exhibit excellent shape memory ability, even at high water contents. By introduction of tetraphenylporphyrin into hydrogels, the shape memory behavior can further be controlled by light through a photothermal effect. This finding offers possibilities for applications of UPy in developing shape memory hydrogels.

quote

GB/T 7714-2015 [1] Yufang Song, Yiming Chen, Ran Chen, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00230.
MLA [1] Yufang Song, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00230.
APA [1] Yufang Song, Yiming Chen, Ran Chen, Hongji Zhang, Dongjian Shi, Yang Wang, Weifu Dong, Piming Ma, & Yue Zhao. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00230
IEEE [1] Yufang Song, Yiming Chen, Ran Chen, Hongji Zhang, Dongjian Shi, Yang Wang, Weifu Dong, Piming Ma, and Yue Zhao, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00230. keywords: {UPy;switching phase;thermal reversible;hydrogel;shape memory}