Abstract AITranslate

Electron microscopy has played an important role in polymer characterization. Traditionally, electron diffraction is used to study crystalline polymers while transmission electron microscopy is used to study microphase separation in stained block copolymers and other multiphase systems. We describe developments that eliminate the barrier between these two approaches—it is now possible to image polymer crystals with atomic resolution. The focus of this Review is on high-resolution imaging (30 Å and smaller) of unstained polymers. Recent advances in hardware allow for capturing numerous (as many as 105) low-dose images from an unperturbed specimen; beam damage is a significant barrier to high-resolution electron microscopy of polymers. Machine-learning-based software is then used to sort and average the images to retrieve pristine structural information from a collection of noisy images. Acknowledging the heterogeneity in polymer samples prior to averaging is essential. Molecular conformations in a wide range of amphiphilic block copolymers, polymerized ionic liquids, and conjugated polymers can be gleaned from two-dimensional projections (2D), three-dimensional (3D) tomograms, and four-dimensional (4D) scanning transmission electron microscopy (STEM) data sets where 2D diffraction patterns are taken as a function of position. Some methods such as phase contrast STEM have been used to image closely related materials such as metal–organic frameworks but not polymers. With improvements in hardware and software, such methods may soon be applied to polymers. Our goal is to provide a comprehensive understanding of the strategies toward the high-resolution imaging of radiation sensitive polymer materials at different length scales.

KeyWords AITranslate

transmission electron microscopy fourdimensional scanning transmission electron microscopy cryogenic lowdose imaging Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00217

Chinese Library Classification Number:

Citation Information:

Electron microscopy has played an important role in polymer characterization. Traditionally, electron diffraction is used to study crystalline polymers while transmission electron microscopy is used to study microphase separation in stained block copolymers and other multiphase systems. We describe developments that eliminate the barrier between these two approaches—it is now possible to image polymer crystals with atomic resolution. The focus of this Review is on high-resolution imaging (30 Å and smaller) of unstained polymers. Recent advances in hardware allow for capturing numerous (as many as 105) low-dose images from an unperturbed specimen; beam damage is a significant barrier to high-resolution electron microscopy of polymers. Machine-learning-based software is then used to sort and average the images to retrieve pristine structural information from a collection of noisy images. Acknowledging the heterogeneity in polymer samples prior to averaging is essential. Molecular conformations in a wide range of amphiphilic block copolymers, polymerized ionic liquids, and conjugated polymers can be gleaned from two-dimensional projections (2D), three-dimensional (3D) tomograms, and four-dimensional (4D) scanning transmission electron microscopy (STEM) data sets where 2D diffraction patterns are taken as a function of position. Some methods such as phase contrast STEM have been used to image closely related materials such as metal–organic frameworks but not polymers. With improvements in hardware and software, such methods may soon be applied to polymers. Our goal is to provide a comprehensive understanding of the strategies toward the high-resolution imaging of radiation sensitive polymer materials at different length scales.

quote

GB/T 7714-2015 [1] Xi Jiang, Nitash P. Balsara. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00217.
MLA [1] Xi Jiang, and Nitash P. Balsara. ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00217.
APA [1] Xi Jiang, & Nitash P. Balsara. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00217
IEEE [1] Xi Jiang and Nitash P. Balsara, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00217. keywords: {transmission electron microscopy;fourdimensional scanning transmission electron microscopy;cryogenic;lowdose imaging;Show More}