Low-Dielectric Polymers Derived From Biomass AITranslate
Abstract AITranslate
Biomass-derived high-performance polymers have recently received much attention because they are easily available and renewable. More recently, researchers have been interested in low-dielectric polymers derived from biomass feedstock. These polymers display good dielectric properties and high thermostability, as well as good mechanical properties, implying that they have potential application in microelectronic industry, especially in fifth-generation communication (5G). This review summarizes recent progress in low dielectric polymers based on the biomass, including the synthesis and properties of different types of biomass resins such as epoxy resins, benzoxazine resins, benzocyclobutene resins, perfluorocyclobutane resins, cyanate eaters, polyester resins, phthalonitrile resins, and a functional maleimide.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00043
Chinese Library Classification Number:
Citation Information:
Biomass-derived high-performance polymers have recently received much attention because they are easily available and renewable. More recently, researchers have been interested in low-dielectric polymers derived from biomass feedstock. These polymers display good dielectric properties and high thermostability, as well as good mechanical properties, implying that they have potential application in microelectronic industry, especially in fifth-generation communication (5G). This review summarizes recent progress in low dielectric polymers based on the biomass, including the synthesis and properties of different types of biomass resins such as epoxy resins, benzoxazine resins, benzocyclobutene resins, perfluorocyclobutane resins, cyanate eaters, polyester resins, phthalonitrile resins, and a functional maleimide.
quote
| GB/T 7714-2015 | [1] Jiaren Hou, Linxuan Fang, Gang Huang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00043. |
| MLA | [1] Jiaren Hou, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00043. |
| APA | [1] Jiaren Hou, Linxuan Fang, Gang Huang, Menglu Dai, Fengping Liu, Caiyun Wang, Minghui Li, Heng Zhang, Jing Sun, & Qiang Fang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00043 |
| IEEE | [1] Jiaren Hou, Linxuan Fang, Gang Huang, Menglu Dai, Fengping Liu, Caiyun Wang, Minghui Li, Heng Zhang, Jing Sun, and Qiang Fang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00043. keywords: {biomass;renewable resource;dielectric constant;lowdielectric polymers;highperformance materials} |