Recent Advances in Applied Fluorescent Polymeric Gels AITranslate

Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Fluorescent polymeric gels (FPGs) are soft luminescent materials in which the fluorophore is the source of photoluminescence and the three-dimensional polymeric network is the fundamental matrix; thus, they have features of both fluorescent materials and gels. Furthermore, the tunable space in the gel network allows for control of the optical behaviors of the fluorophores, which are normally sensitive to the microenvironment. Therefore, FPGs can be considered a superior platform for developing functional materials and have stimulated great interest as candidate substances in multiple application areas to date. Herein, an overview of the recent development of FPGs with diverse applications is provided. Fabrication methods are illustrated from the perspective of the relationship between the fluorophore and the polymeric network. Advanced applications of FPGs in various areas including biomedical, environmentally-related, and informationally-related applications and bioinspired materials are comprehensively reviewed. In addition, the current challenges and future development tendencies are also discussed.

KeyWords AITranslate

gels fluorescent polymeric applications structure−property relationship
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01504

Chinese Library Classification Number:

Citation Information:

Fluorescent polymeric gels (FPGs) are soft luminescent materials in which the fluorophore is the source of photoluminescence and the three-dimensional polymeric network is the fundamental matrix; thus, they have features of both fluorescent materials and gels. Furthermore, the tunable space in the gel network allows for control of the optical behaviors of the fluorophores, which are normally sensitive to the microenvironment. Therefore, FPGs can be considered a superior platform for developing functional materials and have stimulated great interest as candidate substances in multiple application areas to date. Herein, an overview of the recent development of FPGs with diverse applications is provided. Fabrication methods are illustrated from the perspective of the relationship between the fluorophore and the polymeric network. Advanced applications of FPGs in various areas including biomedical, environmentally-related, and informationally-related applications and bioinspired materials are comprehensively reviewed. In addition, the current challenges and future development tendencies are also discussed.

quote

GB/T 7714-2015 [1] Gongmeiyue Su, Zhao Li, Rongji Dai. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01504.
MLA [1] Gongmeiyue Su, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01504.
APA [1] Gongmeiyue Su, Zhao Li, & Rongji Dai. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01504
IEEE [1] Gongmeiyue Su, Zhao Li, and Rongji Dai, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01504. keywords: {gels;fluorescent;polymeric;applications;structure−property relationship}