Three-Dimensional Printing of Liquid Crystal Elastomers and Their Applications AITranslate

Beihang University; Beijing Institute of Technology; University of California; Beihang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Liquid crystal elastomers (LCEs), which are composed of liquid crystal mesogens and polymer networks, exhibit excellent actuation performance and tailorable energy dissipation behavior. They have shown great potential in practical applications in artificial muscles, soft robotics, and wearable devices. However, it is challenging to fabricate LCE samples in arbitrary three-dimensional (3D) shapes and desired alignment patterns with traditional manufacturing methods. Recently, 3D printing techniques have been introduced in combination with alignment methods of LCEs to meet this challenge. In this Review, we highlight recent advances in the 3D printing techniques of LCEs. Two kinds of printing techniques, materials extrusion and vat photopolymerization, are discussed in detail. We compare the differences and key parameters in the printing techniques, such as director fields, resolutions, and printing speeds. The applications of the printed LCE structures in soft robots, reconfigurable surfaces, and haptic devices are also introduced.

KeyWords AITranslate

liquid crystal elastomers 3D printing soft actuators shape morphing soft robotics
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01598

Chinese Library Classification Number:

Citation Information:

Liquid crystal elastomers (LCEs), which are composed of liquid crystal mesogens and polymer networks, exhibit excellent actuation performance and tailorable energy dissipation behavior. They have shown great potential in practical applications in artificial muscles, soft robotics, and wearable devices. However, it is challenging to fabricate LCE samples in arbitrary three-dimensional (3D) shapes and desired alignment patterns with traditional manufacturing methods. Recently, 3D printing techniques have been introduced in combination with alignment methods of LCEs to meet this challenge. In this Review, we highlight recent advances in the 3D printing techniques of LCEs. Two kinds of printing techniques, materials extrusion and vat photopolymerization, are discussed in detail. We compare the differences and key parameters in the printing techniques, such as director fields, resolutions, and printing speeds. The applications of the printed LCE structures in soft robots, reconfigurable surfaces, and haptic devices are also introduced.

quote

GB/T 7714-2015 [1] Zhijian Wang, Yubing Guo, Shengqiang Cai, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01598.
MLA [1] Zhijian Wang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01598.
APA [1] Zhijian Wang, Yubing Guo, Shengqiang Cai, & Jiping Yang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01598
IEEE [1] Zhijian Wang, Yubing Guo, Shengqiang Cai, and Jiping Yang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01598. keywords: {liquid crystal elastomers;3D printing;soft actuators;shape morphing;soft robotics}