Fused Heterocyclic Polymers with Aggregation-Induced Emission: Synthesis and Applications AITranslate
Abstract AITranslate
Fused heterocyclic polymers with aggregation-induced emission (AIE) have attracted much attention due to their unique photoelectric properties, efficient aggregate-state fluorescence, high thermal stability, and superamplification effect as fluorescence sensors as well as multiple functionalities. Among various synthetic methodologies toward fused heterocyclic AIE polymers, polymerization based on triple bond-containing monomers such as alkynes and (iso)cyanides is a powerful synthesis tool that can in situ generate fused heterocyclic units in polymer backbones in high efficiency. In this Review, we summarize the recent progress in the synthesis of nitrogen-, oxygen-, and multiple heteroatom-containing fused cyclic polymers with AIE features based on polymerizations of triple bond-containing monomers. Furthermore, the high-tech applications of the corresponding fused heterocyclic AIE polymers in the visualization of morphological structures, fluorescence chemo-sensors, stimuli-responsive materials, and photodynamic therapy are illustrated. Finally, perspectives on the challenges and future development directions of this field are discussed.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01476
Chinese Library Classification Number:
Citation Information:
Fused heterocyclic polymers with aggregation-induced emission (AIE) have attracted much attention due to their unique photoelectric properties, efficient aggregate-state fluorescence, high thermal stability, and superamplification effect as fluorescence sensors as well as multiple functionalities. Among various synthetic methodologies toward fused heterocyclic AIE polymers, polymerization based on triple bond-containing monomers such as alkynes and (iso)cyanides is a powerful synthesis tool that can in situ generate fused heterocyclic units in polymer backbones in high efficiency. In this Review, we summarize the recent progress in the synthesis of nitrogen-, oxygen-, and multiple heteroatom-containing fused cyclic polymers with AIE features based on polymerizations of triple bond-containing monomers. Furthermore, the high-tech applications of the corresponding fused heterocyclic AIE polymers in the visualization of morphological structures, fluorescence chemo-sensors, stimuli-responsive materials, and photodynamic therapy are illustrated. Finally, perspectives on the challenges and future development directions of this field are discussed.
quote
| GB/T 7714-2015 | [1] Dongyang Fan, Dong Wang, Ting Han, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01476. |
| MLA | [1] Dongyang Fan, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01476. |
| APA | [1] Dongyang Fan, Dong Wang, Ting Han, & Ben Zhong Tang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01476 |
| IEEE | [1] Dongyang Fan, Dong Wang, Ting Han, and Ben Zhong Tang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01476. keywords: {fused heterocyclic polymers;aggregationinduced emission;C−H activation;multicomponent polymerization;polymer synthesis} |