Discussion on Specific Saturated Magnetization Value of PureNi,Co and WC-Co Cemented Carbide AITranslate

Changsha Nonferrous Metallurgical Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of the literatures in respect of specific saturated magnetization value of pure Ni,Co and WC-Co cemented carbide.In more than 20 articles are indicated that the specific saturated magnetization value is about 4π times of the normal value( A·m^2/kg).The results showed that for the measured value,this is due to the author's mistake in the unit conversion of electric magnetism quantity; while for the calculated value based on related data,it is due to the fact that the measured specific saturated magnetization value is about 4π times of the normal value.Corresponding description is also made of the definition of the related physical quantity and corresponding unit conversion expression are presented for the convenience of discussion.

KeyWords AITranslate

pure Ni pure Co WC-Co cemented carbide specific saturated magnetization unit conversion expression

1聂安之.硬质合金的磁饱和[J].稀有金属与硬质合金,1991(4):17-24. 被引量:5

2庞广兴.WC-Co合金在烧结过程中自行碳的校正[J].稀有金属与硬质合金,1991(2):5-9. 被引量:10

3钟连生.低压烧结对钨钴合金碳校正的初步探讨[J].硬质合金,1990(3):5-9. 被引量:4

4图马JJ.物理计算手册[M].北京:新时代出版社,1985.182-183.

5赵凯华 等.电磁学(下)[M].北京:人民教育出版社,1978.115-119.

6近角聪信 黄锡成 译.磁性体手册(上)[M].北京:冶金工业出版社,1984..

7功能材料及其应用编写组.功能材料及其应用手册[M].北京:机械工业出版社,1991..

8特贝尔RS 译.磁性材料[M],北京冶金研究所《磁性材料》翻译组[M].北京:科学出版社,1979..

9Roebuck B, et al. Infiltration as a method for producing WC hardmetals with Co and Ni alloy binder - phases [ J ]. International Journal of Refractory Metals and Hard Materials, 1984,(3) :35.

10近角聪信 饧鹰善 译.磁性体手册(中)[M].北京:冶金工业出版社,1984..

1王喜荣.化工科技期刊插图设计与制作中存在的问题[J].化学推进剂与高分子材料,2007,5(3):61-63. 被引量:3

2王兴林.关于纯Ni、纯Co及WC-Co硬质合金比饱和磁化强度值探讨(Ⅱ)[J].硬质合金,2008,25(1):54-57. 被引量:3

3秦琴,栾道成,王正云,李亚军,左洪松,赵太源.添加TaC和Y_2O_3对超细YG6硬质合金组织及性能的影响[J].稀有金属与硬质合金,2012,40(2):48-52. 被引量:4

4张伟彬,杜勇,彭英彪,李娜,周鹏,程开明,张聪,张忠健,王社权,徐涛,陈伟民,陈利,谢文,温光华,龙坚战,张颢,刘向忠,金展鹏.研发硬质合金的集成计算材料工程[J].材料科学与工艺,2016,24(2):1-28. 被引量:11

1方华.科技论文插图形式的优化[J].编辑学报,2009,21(1):37-38. 被引量:15

2王昌栋,陈翔,幸建华.科技期刊插图质量控制机制的构建[J].编辑学报,2009,21(3):210-212. 被引量:8

3王晓灵.添加Cr及Cr_3C_2对WC-(Co,Ni)硬质合金比饱和磁化强度的影响[J].硬质合金,2011,28(6):337-344. 被引量:10

4张惠芳.科技论文插图形式处理实例分析[J].黄冈师范学院学报,2015,35(3):197-200. 被引量:1

5潘顺康,熊吉磊,成丽春,姚青荣,饶光辉.Effects of cobalt substitution on structure and microwave absorption properties of PrNi_5 alloy[J].稀土学报:英文版,2015,33(12):1324-1328.

6张伟彬,杜勇,彭英彪,李娜,周鹏,程开明,张聪,张忠健,王社权,徐涛,陈伟民,陈利,谢文,温光华,龙坚战,张颢,刘向忠,金展鹏.研发硬质合金的集成计算材料工程[J].材料科学与工艺,2016,24(2):1-28. 被引量:11

7杨小璠,李友生,李凌祥,沈志煌,刘菊东.硬质合金高温性能对碳纤维复合材料切削加工的影响研究[J].金刚石与磨料磨具工程,2017,37(5):45-49. 被引量:3

8李屏,王社权,谢文,李园园,左锐,杜勇.立方相成分对梯度合金结构的影响——理论计算及实验研究[J].硬质合金,2017,34(6):361-369.

9邝海,谭敦强,何文,王晓茹,邹志航,易志强,白杜娟.稀土元素对硬质合金影响的研究进展[J].稀有金属与硬质合金,2018,46(3):69-74. 被引量:8

10龙坚战,杜勇,陆必志,张卫兵,徐涛,张忠健,易茂中.Co-Ni-Al复合黏结相硬质合金研究进展[J].航空材料学报,2018,38(5):47-58. 被引量:2

1王兴林.关于纯Ni、纯Co及WC-Co硬质合金比饱和磁化强度值探讨(Ⅱ)[J].硬质合金,2008,25(1):54-57. 被引量:3

2刘吉萍.里氏硬度不确定度评定[J].计量技术,2004(4):50-52. 被引量:2

3张建新,高爱华,陈昊.合金元素对Al-Mg-Si系铝合金组织及性能的影响[J].铸造技术,2007,28(3):373-375. 被引量:29

4张建新,高爱华.合金元素对6063铝合金组织性能的影响[J].铸造,2007,56(6):642-644. 被引量:11

5席丽娅.浅析数控机床机械故障诊断实用方法[J].科技致富向导,2012(15):108-108.

6张春林,陈燕军,杨宴宾.钢带的带状组织对HFW焊管焊接质量的影响[J].焊管,2013,36(2):67-70. 被引量:4

7杨树林,孙文儒,王照坤,张银东,魏志刚,胡壮麒.磷和硼共同加入对GH761合金力学性能的影响[J].稀有金属材料与工程,2006,35(6):929-932. 被引量:8

8吴鹤,白明远,张文扬,虞文军.钛合金激光快速成形与热轧板材氩弧焊试验[J].航空制造技术,2009,0(21):72-73.

9曹智芬.长度的测量教学设计[J].数理化学习,2014(4):35-37. 被引量:1

10杨宾峰,张辉,杨卫国,张战斌,周义建,张超,曹海霞.电磁量测量的一体化传感器仿真分析与设计[J].空军工程大学学报:自然科学版,2015,16(1):56-61. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG113.225[金属学及工艺—物理冶金]

Citation Information:

Study is made of the literatures in respect of specific saturated magnetization value of pure Ni,Co and WC-Co cemented carbide.In more than 20 articles are indicated that the specific saturated magnetization value is about 4π times of the normal value( A·m^2/kg).The results showed that for the measured value,this is due to the author's mistake in the unit conversion of electric magnetism quantity; while for the calculated value based on related data,it is due to the fact that the measured specific saturated magnetization value is about 4π times of the normal value.Corresponding description is also made of the definition of the related physical quantity and corresponding unit conversion expression are presented for the convenience of discussion.

quote

GB/T 7714-2015 [1] WANG Xing-lin. Discussion on Specific Saturated Magnetization Value of PureNi,Co and WC-Co Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2005(1): 33-38.
MLA [1] WANG Xing-lin. "Discussion on Specific Saturated Magnetization Value of PureNi,Co and WC-Co Cemented Carbide." Rare Metals and Cemented Carbides, no. 1, 2005, pp. 33-38.
APA [1] WANG Xing-lin. (2005). Discussion on Specific Saturated Magnetization Value of PureNi,Co and WC-Co Cemented Carbide. Rare Metals and Cemented Carbides(1), 33-38.
IEEE [1] WANG Xing-lin, "Discussion on Specific Saturated Magnetization Value of PureNi,Co and WC-Co Cemented Carbide," Rare Metals and Cemented Carbides, no. 1, pp. 33-38, 2005. keywords: {pure Ni;pure Co;WC-Co cemented carbide;specific saturated magnetization;unit conversion expression}