Discussion on the Mechanical Alloying for Fabrication ofSuperfine/Nanosized CuCr Contact Materials AITranslate
Abstract AITranslate
Analysis and discussion is made of the major concerns such as grain size,oxygen content and density controls in the mechanical alloying for fabrication of superfine or nanosized CuCr contact materials.Furthermore,a new idea of normal vacuum sintering technique with the addition of high-property grain growth inhibitor to fabricate high-property CuCr contact materials at lower cost.
KeyWords AITranslate
1王亚平,张丽娜,杨志懋,丁秉钧,周敬恩.细晶—超细晶CuCr触头材料的研究进展[J].高压电器,1997,33(2):34-39. 被引量:26
2吕大铭,凌贤野,周武平,周文元.用热等静压制取铜铬系真空触头材料[J].粉末冶金工业,1997,7(1):17-22. 被引量:10
3周文元,吕大铭,周武平.热处理对CuCr、CuCrFe真空触头材料组织及性能的影响[J].高压电器,1998,34(2):14-17. 被引量:8
4李秀勇,王亚平,丁秉钧.微晶、纳米晶 CuCr 触头材料的组织及性能[J].稀有金属,1999,23(5):363-365. 被引量:13
5王强,梁淑华,范志康.CuCr系合金材料制造工艺的新进展[J].材料导报,2000,14(8):22-24. 被引量:30
6张程煜,王江,张晖,丁秉钧.Ni或Co的加入对CuCr25合金组织与性能的影响[J].稀有金属材料与工程,2001,30(4):286-289. 被引量:7
7李翥贵,农荣达,周灼光,陈晓东.Cu-Cr二元合金状态图与Cu-Cr触头的工艺探索[J].电工合金,1997(2):23-29. 被引量:13
8范景莲,黄伯云,汪登龙.过程控制剂对机械合金化过程与粉末特征的影响[J].粉末冶金工业,2002,12(2):7-12. 被引量:23
9王亚平,崔建国,杨志懋,丁秉钧,周敬恩.微晶CuCr材料的制备及电击穿性能的研究[J].西安交通大学学报,1997,31(3):76-80. 被引量:17
10李明怡,果世驹,林涛,康志君.铁粉特性对温压生坯密度的影响[J].粉末冶金技术,2000,18(3):172-177. 被引量:15
1朱建娟,田保红,刘平.Cu-Cr合金触头材料制备技术的研究进展[J].铸造,2006,55(11):1110-1113. 被引量:12
2朱建娟,田保红,刘平.Cu-Cr合金触头材料制备技术的研究[J].上海有色金属,2006,27(4):27-32. 被引量:2
3陈小龙.新型8位单片机M68HC08[J].电子产品世界,2002(02A):62-63. 被引量:1
1王德宝,吴玉程,王文芳,宗跃.机械合金化诱导难互溶系Cu-Cr合金固溶度扩展的研究[J].稀有金属,2008,32(1):17-22. 被引量:14
2周洪雷,田保红,刘勇,任凤章,贾淑果,刘平.压制力对A_2lO_3弥散强化Cu/Cr复合材料组织和性能的影响[J].金属热处理,2008,33(9):87-90. 被引量:2
3王德宝,吴玉程,王文芳,宗跃,黄新民.机械合金化制备Cu-Cr合金时效强化特性的研究[J].热处理,2009,24(1):30-33. 被引量:1
4王德宝,吴玉程,于福文,王文芳,解挺.过程控制剂对机械合金化制备Cu-Cr纳米晶的影响[J].材料科学与工程:中英文版,2008(1):28-33.
5王玉平,张润理,游一民.快速凝固法制备细晶超细晶Cu-Cr合金的进展[J].高压电器,2011,47(12):80-85. 被引量:3
6段文燕.高压和时效处理对铜铬合金电导率的影响[J].机械工程材料,2013,37(3):77-79. 被引量:1
7滕莹雪,郭菁.铜-铬合金电沉积的研究[J].电镀与涂饰,2013,32(8):4-7.
8王松,刘满门,陈永泰,孙旭东,谢明.合金化元素Zr、Y、Mo对Cu-Cr合金组织与性能的影响[J].电工材料,2013(4):3-6. 被引量:2
9江燕,杨敏鸽,杨增超,王俊勃,贺辛亥,刘松涛.中高压铜基电触头材料的研究现状[J].电工材料,2013(4):27-30. 被引量:2
10黄洲,宋群玲,金青林,杨天武,李再久,蒋业华.藕状多孔纯Cu及多孔Cu-1.8%Cr合金铸件的研究[J].铸造,2014,63(6):583-586. 被引量:3
1曹顺华,林信平,李炯义,李元元,邵明.模壁润滑温压工艺的研究[J].材料导报,2004,18(10):85-88. 被引量:1
2宁海霞.WC颗粒增强钢基复合材料的制备及耐磨性研究[J].铸造技术,2009,30(4):503-505. 被引量:4
3宁海霞,成小乐.WC颗粒增强钢基复合材料的制备及耐磨性研究[J].新技术新工艺,2010(1):61-63.
4余建芳.“圆形”WC晶粒的硬质合金[J].硬质合金,2005,22(3):178-178.
5徐源源,潘应君,柯德庆,杨林,王盼.晶粒长大抑制剂VC对原位生成WCoB-TiC-Co复相金属陶瓷的影响[J].材料科学与工艺,2017,25(2):59-65. 被引量:1
6钱开友,王兴庆,何宝山,郭海亮.纳米硬质合金制备工艺的研究与发展[J].上海大学学报:自然科学版,2001,7(2):133-136. 被引量:8
7赵来军,李震彪,王珂,邱安宁,李慧杰.纳米CuCr50触头材料电弧侵蚀特性[J].高压电器,2012,48(5):15-19. 被引量:6
8陈宝军,田文富,魏玉梅.稀土长余辉发光材料真空烧结的研究[J].机械工程师,2006(9):57-58.
9张为民,沙国江.缩微品背景密度控制问题的探讨[J].缩微技术,1993(1):11-14.
10Kear,BH,张汉林.纳米结构WC—Co材料的化学处理及性能[J].国外难熔金属与硬质材料,1995,11(1):4-11. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]
Citation Information:
Analysis and discussion is made of the major concerns such as grain size,oxygen content and density controls in the mechanical alloying for fabrication of superfine or nanosized CuCr contact materials.Furthermore,a new idea of normal vacuum sintering technique with the addition of high-property grain growth inhibitor to fabricate high-property CuCr contact materials at lower cost.
quote
| GB/T 7714-2015 | [1] LIU Fang, ZHOU Ke-chao, HE Han-wei, et al. Discussion on the Mechanical Alloying for Fabrication ofSuperfine/Nanosized CuCr Contact Materials[J]. Rare Metals and Cemented Carbides, 2005(1): 39-44. |
| MLA | [1] LIU Fang, et al., "Discussion on the Mechanical Alloying for Fabrication ofSuperfine/Nanosized CuCr Contact Materials." Rare Metals and Cemented Carbides, no. 1, 2005, pp. 39-44. |
| APA | [1] LIU Fang, ZHOU Ke-chao, HE Han-wei, & YUAN Tie-chui. (2005). Discussion on the Mechanical Alloying for Fabrication ofSuperfine/Nanosized CuCr Contact Materials. Rare Metals and Cemented Carbides(1), 39-44. |
| IEEE | [1] LIU Fang, ZHOU Ke-chao, HE Han-wei, and YUAN Tie-chui, "Discussion on the Mechanical Alloying for Fabrication ofSuperfine/Nanosized CuCr Contact Materials," Rare Metals and Cemented Carbides, no. 1, pp. 39-44, 2005. keywords: {superfine or nanosized CuCr alloy;oxygen content;density;pressure sintering;graingrowth inhibitor;warm compaction} |