daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A New Technology for WC Powder Preparation AITranslate

School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Description is made of a new technology for preparing WC powder by carburizing in a mixture gas medium developed by professor V.P.Bondarenko research group of Institute for Superhard Materials of the National Academy of Sciences in Ukraine.WC powders is prepared with CH_4 as the raw material instead of the solid carbon black powder.Upon gas carburization,C-controllable WC powder is prepared,followed by normal compaction,sintering to obtain cemented carbide.The properties of the alloy products are in accordance with the former Soviet Union State Standard(GOST)3882—74.Description is also made of the basic principle of the technology,powder and alloy properties.

KeyWords AITranslate

WC powder gas carburization cemented carbide CH_4

1Bondareko V P, et al. Advanced technologies d production of cemented carbides and ccxnposite material based on them[A].Proceeding d the 15th International Plansee Seminar [ C].Routte: Plansee Holding AG, 2001. 189.

2Bondarenko V P, et o2. Production of tungsten - cobalt cemented carbldes[J] .Materials Technolcgy, 2002, 17(1) :30.

3Bondarenko V P, et al.Optimizing conditions for obtaining a solid solution of tungsten carbide in titanitun carbide by preparing it in a precisely controlled gas meditun [ J ] . International Journal of Hydrogen Energy, 1999, 24: 845.

4Bondarenko V P, et al. Use of a precisely controlled methanehydrogen gas meditrn when regenerating tungsten - base hard alloy waste[J ]. International Journal of Hydrogen Energy, 1999,24: 853.

5Bondarenko V P, et al. The effect d temperature and holding time on the degree of regeneration of T5K10 alloy waste in hydrogen containing equilibritrn amounts of methane [J]. International Journal of Hydrogen Energy, 1999, 24: 849.

1闫波,孙彦平,王俊文,陈新谋.RF-PCVD法碳化钨纳米粉的制备[J].中国钨业,2006,21(4):38-40. 被引量:5

2孙明君.硬质合金多孔材料的研制[J].稀有金属与硬质合金,2007,35(2):14-17. 被引量:4

3曾江华,袁定胜,刘应亮,陈景星,谭三香.碳化钨纳米晶合成及其电化学性能[J].催化学报(英文),2008,29(7):607-611. 被引量:7

4尹晓星.碳化钨、硬质合金文献调研[J].中国钨业,2008,23(5):7-10. 被引量:2

5羊建高,戴煜.硬质合金的发展趋势及特殊粉末的制备技术[J].稀有金属与硬质合金,2011,39(1):48-51. 被引量:9

6刘璐超,娄丽,吴胜男,杨丽观.无粘结剂硬质合金研究进展与制备[J].材料开发与应用,2015,30(4):93-97. 被引量:1

7李通,向杰,陈磊,李超,黎松,邹建新.川渝地区硬质合金生产现状与展望[J].四川冶金,2020,42(3):4-7. 被引量:1

1杨瑞嵩,王莹,鲁越.机械活化辅助熔盐法制备WC粉末的研究[J].稀有金属与硬质合金,2015,43(2):14-16.

2王占岭,孙彦平,王俊文.RF-PCVD法制备一种新颖纳米碳粒及其微结构表征[J].炭素技术,2008,27(5):37-40.

3王博,刘淼,翟皖予,李翠霞.等离子技术制备超细粉体的最新研究进展[J].陶瓷,2009(2):13-16. 被引量:1

4谢中华,陈树茂,王文华,张秋和,赵会团,刘斌.球形钨粉的制备工艺研究[J].中国钨业,2009,24(4):40-42. 被引量:12

5郦剑,罗娟,罗来马,俞佳,朱流.硬质合金与钢基体钎焊技术的研究进展[J].材料科学与工程学报,2009,27(6):955-958. 被引量:17

6郝立伟,肖简正,洪小虎.激光粒度分布仪检测细碳化钨粉方法[J].中国钨业,2010,25(4):47-50. 被引量:4

7傅小明.纳米碳化钨的制备技术及研究现状[J].稀有金属与硬质合金,2011,39(1):57-60. 被引量:4

8沈志农,杨立.细WC配比对非均匀YG20C合金性能的影响[J].硬质合金,2011,28(3):163-165. 被引量:9

9詹鹏,徐瑞东,黄利平,陈步明,周建峰.聚苯胺对锌电积用复合惰性阳极材料电化学性能的影响(英文)[J].中国有色金属学报:英文版,2012,22(7):1693-1700. 被引量:3

10付龙,柳学全,李一,丁存光,李立鑫,姜丽娟.国内外矿用高耐磨、高韧性硬质合金新技术[J].硬质合金,2012,29(4):254-261. 被引量:31

1R.K.Saclangi,周定良.晶粒长大抑制剂—亚微碳化钒和碳化铬的合成和特性[J].国外难熔金属与硬质材料,2000,16(2):50-56. 被引量:1

2祖庸,李晓娥.气相法制备纳米二氧化钛[J].钛工业进展,1996(4):2-5. 被引量:5

3刘沙,刘刚,杨贵彬,黄泽兰.一种废硬质合金环保再生新技术[J].稀有金属与硬质合金,2004,32(2):21-23. 被引量:3

4管伟明,张国庆,郑福前,谢明,刘建良.熔融金属喷射沉积技术的发展与应用[J].贵金属,1999,20(2):48-51. 被引量:4

5陆寿先.提高24m^2烧结机料层厚度的操作实践[J].柳钢科技,1998(3):6-10.

6蔺恩惠,李新勇,郭跃华,张昌言.激光气相法制备TiO_2超精细粉末[J].西北师范大学学报:自然科学版,1995,31(1):18-21. 被引量:4

7刘克明,谌昀,谢仕芳,万珍珍,陆德平.钨铜复合材料研究现状与展望[J].热处理技术与装备,2012,33(5):40-42. 被引量:8

8高玉来,沈军,孙剑飞,周彼德,李庆春.大块非晶合金制备新技术——非晶粉末固结成形法[J].材料导报,2002,16(10):31-34. 被引量:3

9岑永权,陈麒忠,孙丹.微粉脱硫剂的开发[J].上海金属,2001,23(4):10-13.

10浙江丰业集团有限公司[J].不锈:市场与信息,2005(8):35-35.

Basic Information:

DOI:

Chinese Library Classification Number:TF123.31[冶金工程—粉末冶金]

Citation Information:

Description is made of a new technology for preparing WC powder by carburizing in a mixture gas medium developed by professor V.P.Bondarenko research group of Institute for Superhard Materials of the National Academy of Sciences in Ukraine.WC powders is prepared with CH_4 as the raw material instead of the solid carbon black powder.Upon gas carburization,C-controllable WC powder is prepared,followed by normal compaction,sintering to obtain cemented carbide.The properties of the alloy products are in accordance with the former Soviet Union State Standard(GOST)3882—74.Description is also made of the basic principle of the technology,powder and alloy properties.

quote

GB/T 7714-2015 [1] LIU Sha, LIU Gang, YANG Gui-bin, et al. A New Technology for WC Powder Preparation[J]. Rare Metals and Cemented Carbides, 2005(1): 29-32.
MLA [1] LIU Sha, et al., "A New Technology for WC Powder Preparation." Rare Metals and Cemented Carbides, no. 1, 2005, pp. 29-32.
APA [1] LIU Sha, LIU Gang, YANG Gui-bin, & HUANG Ze-lan. (2005). A New Technology for WC Powder Preparation. Rare Metals and Cemented Carbides(1), 29-32.
IEEE [1] LIU Sha, LIU Gang, YANG Gui-bin, and HUANG Ze-lan, "A New Technology for WC Powder Preparation," Rare Metals and Cemented Carbides, no. 1, pp. 29-32, 2005. keywords: {WC powder;gas carburization;cemented carbide;CH_4}