Heteroepitaxial growth of Au@Pd core–shell nanocrystals with intrinsic chiral surfaces for enantiomeric recognition AITranslate
Abstract AITranslate
Noble metal surfaces with intrinsic chirality serve as an ideal candidate for investigating enantioselective chemistry due to their superior chemical durability and high catalytic activity.Recently,significant advance has been made in synthesizing metal nanocrystals with intrinsic chirality.Nonetheless,the majority reports are limited to gold.Herein,through a heteroepitaxial growth strategy,the synthesis of metal nanocrystals with intrinsic chirality to palladium was extended for the first time and their application in enantioselective recognition was demonstrated.The heteroepitaxial growth strategy allows for transferring the chirality of homochiral Au nanocrystals to Au@Pd core–shell nanocrystals.By employing the chiral Au@Pd nanocrystals as enantiomeric recognizing elements,a series of electrochemical sensors for chiral discrimination were developed.Under optimal conditions,the peak potential between D-dihydroxyphenylalanine(D-DOPA)and L-dihydroxyphenylalanine(L-DOPA)is about 80 m V,and the peak current of D-DOPA is 2 times as much as that of L-DOPA,which enables the determination of the enantiomeric excess(EE,%)of L-DOPA.Overall,this report not only introduces a heteroepitaxial growth strategy to synthesize metal nanocrystals with intrinsic chirality,but also demonstrates the superior capability of integrating intrinsic chirality and catalytic properties into metal nanocrystals for chiral recognition.
KeyWords AITranslate
1Qing-Wei Ding,Qing Luo,Liang Lin,Xing-Ping Fu,Lai-Sen Wang,Guang-Hui Yue,Jie Lin,Qing-Shui Xie,Dong-Liang Peng.Facile synthesis of PdCu nanocluster-assembled granular films as highly efficient electrocatalysts for formic acid oxidation[J].Rare Metals,2022,41(8):2595-2605. 被引量:3
2Chun-Jie Li,Guang-Cun Shan,Chun-Xian Guo,Ru-Guang Ma.Design strategies of Pd-based electrocatalysts for efficient oxygen reduction[J].Rare Metals,2023,42(6):1778-1799. 被引量:3
3李丽,石永霞,侯曼,张志成.铜基材料电催化二氧化碳还原反应的研究进展[J].稀有金属,2022,46(6):681-694. 被引量:9
4Jing-Jing Fang,Qi-Ming Liu,Xiong-Wu Kang,Shao-Wei Chen.Selective hydrogenation of 4-nitrostyrene to 4-nitroethylbenzene catalyzed by Pd@Ru core–shell nanocubes[J].Rare Metals,2022,41(4):1189-1194. 被引量:1
5Dong Wang,Hua-Min Zhao,Li Guo,Long Zhang,Hong-Bin Zhao,Xuan Fang,Sheng Li,Gong Wang.Facile synthesis of CuO-Co_(3)O_(4)prickly-sphere-like composite for non-enzymatic glucose sensors[J].Rare Metals,2022,41(6):1911-1920. 被引量:1
6Sulaiman Umar Abbas,Jun-Jun Li,Xing Liu,Ayesha Siddique,Yong-Xia Shi,Man Hou,Kai Yang,Farhat Nosheen,Xiao-Ya Cui,Guang-Chao Zheng,Zhi-Cheng Zhang.Chiral metal nanostructures:synthesis,properties and applications[J].Rare Metals,2023,42(8):2489-2515. 被引量:4
1Meng-Xin Sun,Chuan-Zhi Ni,Fang-Qi Zhang,Yuan-Yuan Zhu,Jie Zeng,Shuang-Xi Gu.Chiral amino acid recognition in water:A BINOL-based fluorescent probe[J].Chinese Chemical Letters,2023,34(12):136-140. 被引量:1
2Zhi Du,Yijia Guan,Nan Gao,Jinsong Ren,Xiaogang Qu.Cross-fibrillation of insulin and amyloid β on chiral surfaces: Chirality affects aggregation kinetics and cytotoxicity[J].Nano Research,2018,11(8):4102-4110. 被引量:2
3Junli Guo,Yuanfei Xue,Chenxi Zhao,Junjian Zhao,Zhida Gao,Ye Mei,Yan-Yan Song.Integrated separation-electrochemical detection device based on wood column for online identification of enantiomer[J].Nano Research,2024,17(3):1893-1901.
4Claudia Garnero,Carolina Aloisio,Marcela Longhi.Ibuprofen-Maltodextrin Interaction: Study of Enantiomeric Recognition and Complex Characterization[J].Pharmacology & Pharmacy,2013,4(1):18-30. 被引量:1
5Xiugang Li,Qilu Yao,Rongwei Shi,Minsong Huang,Zhang‐Hui Lu.A step‐growth strategy to grow vertical porous aromatic framework nanosheets on graphene oxide:Hybrid material‐confined Co for ammonia borane methanolysis[J].Carbon Energy,2023,5(10):64-76.
6Andrew J.Gellman.An Account of Chiral Metal Surfaces and Their Enantiospecific Chemistry[J].Accounts of Materials Research,2021,2(11):1024-1032.
7Jia-Qi Chen,Han-Bo Li,Xi Lu,Xiao-Yang Liu,Wei Feng,Pan Wang,Jian-Qiang Zhao,Zhen-Yu Zhu,Guang-Chao Zheng,Xiao-Chun Wu.Two-thiols-regulated fabrication of plasmonic nanoparticles with co-enhanced Raman scattering and circular dichroism responses[J].Rare Metals,2023,42(11):3673-3681.
8Weigao Han,Shilin Wu,Fang Dong,Weiliang Han,Yinghao Chu,Linghui Su,Zhicheng Tang.A confined growth strategy to construct 3DOM SiO_(2) nanoreactor insitu embedded Co_(3)O_(4) nanoparticles catalyst for the catalytic combustion of VOCs:Superior H_(2)O and SO_(2) resistance[J].Nano Research,2024,17(1):207-220.
9Rui Hu,Yuncong Yuan,Meijia Gu,You-Quan Zou.Recent advances in chiral aggregation-induced emission fluorogens[J].Engineered Regeneration,2022,3(3):323-338.
10屠美玲,王祁宁,李琰君,张建庭,贾继宁,杨阿三.手性δ-取代己内酰胺化学/酶串联一锅法合成及立体构型调控[J].浙江大学学报(理学版),2024,51(1):55-63.
Basic Information:
DOI:
Chinese Library Classification Number:TB383.1[一般工业技术—材料科学与工程]
Citation Information:
Noble metal surfaces with intrinsic chirality serve as an ideal candidate for investigating enantioselective chemistry due to their superior chemical durability and high catalytic activity.Recently,significant advance has been made in synthesizing metal nanocrystals with intrinsic chirality.Nonetheless,the majority reports are limited to gold.Herein,through a heteroepitaxial growth strategy,the synthesis of metal nanocrystals with intrinsic chirality to palladium was extended for the first time and their application in enantioselective recognition was demonstrated.The heteroepitaxial growth strategy allows for transferring the chirality of homochiral Au nanocrystals to Au@Pd core–shell nanocrystals.By employing the chiral Au@Pd nanocrystals as enantiomeric recognizing elements,a series of electrochemical sensors for chiral discrimination were developed.Under optimal conditions,the peak potential between D-dihydroxyphenylalanine(D-DOPA)and L-dihydroxyphenylalanine(L-DOPA)is about 80 m V,and the peak current of D-DOPA is 2 times as much as that of L-DOPA,which enables the determination of the enantiomeric excess(EE,%)of L-DOPA.Overall,this report not only introduces a heteroepitaxial growth strategy to synthesize metal nanocrystals with intrinsic chirality,but also demonstrates the superior capability of integrating intrinsic chirality and catalytic properties into metal nanocrystals for chiral recognition.
quote
| GB/T 7714-2015 | [1] Feng-Xia Wu, Feng-Hua Li, Xia-Li Lv, et al. Rare Metals, 2024(1): 225-235. |
| MLA | [1] Feng-Xia Wu, et al., Rare Metals, no. 1, 2024, pp. 225-235. |
| APA | [1] Feng-Xia Wu, Feng-Hua Li, Xia-Li Lv, Qi-Xian Zhang, Guo-Bao Xu, & Wen-Xin Niu. (2024). Rare Metals(1), 225-235. |
| IEEE | [1] Feng-Xia Wu, Feng-Hua Li, Xia-Li Lv, Qi-Xian Zhang, Guo-Bao Xu, and Wen-Xin Niu, Rare Metals, no. 1, pp. 225-235, 2024. |