A Hf-doped dual-phase high-entropy alloy: phase evolution and wear features AITranslate
Abstract AITranslate
Initially defined high entropy alloys(HEAs)usually exhibit a single-phase solid-solution structure.However,two and/or more types of phases in HE As possibly induce the desired microstructure features,which contribute to improving the wear properties of HE As.Here,we prepare a series of(AlCoCrFeNi)100-xHfx(x=0,2,4and 6;at%) HEAs and concern their phase compositions,micro structures and wear properties.Hf leads to the formation of(Ni,Co)2Hf-type Laves phase and tailors the microstructure from a body-centered cubic(BCC) singlephase structure to a hypoeutectic structure.An increased hardness from~HV 512.3 to~HV 734.1 is due to solid-solution strengthening,grain refinement strengthening and precipitated phase strengthening.And a few oxides(Al2O3+Cr2O3) caused by the wear heating contribute to an 85.5% decrease in wear rate of the HEA system from6.71×10-5 to 0.97×10-5 m3·N-1·m-1.In addition,Hf addition changes the wear mechanism from abrasive wear,mild oxidative wear and adhesive wear to oxidative wear and adhesive wear.
KeyWords AITranslate
1卢思颖,苗军伟,卢一平.多主元高熵合金的强韧化[J].稀有金属,2021,45(5):530-540. 被引量:18
2卢煜,李春燕,田霖,翟建树,寇生中.高熵合金的性能研究进展[J].稀有金属,2022,46(10):1352-1364. 被引量:10
3Jin-Xiong Hou,Bo-Xuan Cao,Bo Xiao,Zeng-Bao Jiao,Tao Yang.Compositionally complex coherent precipitation-strengthened high-entropy alloys:a critical review[J].Rare Metals,2022,41(6):2002-2015. 被引量:2
4Hang Wang,Quan-Feng He,Yong Yang.High-entropy intermetallics:from alloy design to structural and functional properties[J].Rare Metals,2022,41(6):1989-2001. 被引量:5
5Xin Xian,Zhi-Hong Zhong,Li-Jing Lin,Zhi-Xiong Zhu,Chang Chen,Yu-Cheng Wu.Tailoring strength and ductility of high-entropy CrMnFeCoNi alloy by adding Al[J].Rare Metals,2022,41(3):1015-1021. 被引量:5
6Jun-Jie Wang,Zong-De Kou,Shu Fu,Shang-Shu Wu,Si-Nan Liu,Meng-Yang Yan,Di Wang,Si Lan,Horst Hahn,Tao Feng.Microstructure and magnetic properties evolution of Al/CoCrFeNi nanocrystalline high-entropy alloy composite[J].Rare Metals,2022,41(6):2038-2046. 被引量:3
7张蔚冉,Peter K.Liaw,张勇.高熵合金材料研究进展(英文)[J].Science China Materials,2018,61(1):2-22. 被引量:81
8Hong-Ge Li,Peng-Cheng Che,Xiao-Kun Yang,Yong-Jiang Huang,Zhi-Liang Ning,Jian-Fei Sun,Hong-Bo Fan.Enhanced tensile properties and wear resistance of additively manufactured CoCrFeMnNi high-entropy alloy at cryogenic temperature[J].Rare Metals,2022,41(4):1210-1216. 被引量:4
9Hui Jiang,Li Jiang,Dongxu Qiao,Yiping Lu,Tongmin Wang,Zhiqiang Cao,Tingju Li.Effect of Niobium on Microstructure and Properties of the CoCrFeNb_xNi High Entropy Alloys[J].Journal of Materials Science & Technology,2017,33(7):712-717. 被引量:19
10Bingqian Jin,Nannan Zhang,Shuo Yin.Strengthening behavior of AlCoCrFeNi(TiN)_(x) high-entropy alloy coatings fabricated by plasma spraying and laser remelting[J].Journal of Materials Science & Technology,2022(26):163-173. 被引量:5
1Peng Li,Jinhang Fan,Kaifa Du,Peilin Wang,Ao Liu,Huayi Yin,Dihua Wang.Eliminating carbon contamination with improved one-step electrochemical preparation of refractory high-entropy alloy TiZrHfNbTa[J].Journal of Materials Science & Technology,2023(32):132-139.
2Fei Sun,Shengtao Deng,Jianan Fu,Jiahua Zhu,Dandan Liang,Pengfei Wang,Hang Zhao,Feng Gong,Jiang Ma,Yanhui Liu,Jun Shen.Superior high-temperature wear resistance of an Ir-Ta-Ni-Nb bulk metallic glass[J].Journal of Materials Science & Technology,2023(27):121-132.
3Wentao Jiang,Hao Lu,Xuemei Liu,Haibin Wang,Dongyang Li,Chao Liu,Mingsheng Wang,Xiaoyan Song.Outstanding high-temperature oxidation-and wear-resistance of WC based cermets[J].Journal of Materials Science & Technology,2023(24):33-46.
4Yuntian Liao,Rongtao Zhu,Wenjun Zhang,Haiyang Zhu,Yang Sun,Jiale Chen,Zhenhua Dong,Ronghuan Lv.Transient synthesis of carbon-supported high-entropy alloy sulfide nanoparticles via flash Joule heating for efficient electrocatalytic hydrogen evolution[J].Nano Research,2024,17(4):3379-3389. 被引量:1
5Hong BIAN,Yanyu SONG,Duo LIU,Yuzhen LEI,Xiaoguo SONG,Jian CAO.Joining of SiO2 ceramic and TC4 alloy by nanoparticles modified brazing filler metal[J].Chinese Journal of Aeronautics,2020,33(1):383-390. 被引量:11
6Y.Lei,J.Sun,X.G.Song,M.X.Yang,T.L.Yang,J.Yin.Eutectic-reaction brazing of Al_(0.3)CoCrFeNi high-entropy alloys using Ni/Nb/Ni interlayers[J].Journal of Materials Science & Technology,2022(26):245-255. 被引量:1
7Nataniel Yong Syn Tham,Grace Rui Si Tay,Bingqing Yao,Kaiqiang Wu,ZhiLi Dong.Effect of Aging Parameters on Inconel 718 Fabricated by Laser Directed Energy Deposition[J].Chinese Journal of Mechanical Engineering(Additive Manufacturing Frontiers),2023,2(4):112-121.
8Hongxiang Wang,Jiajia Shen,Weipeng Zhang,Zhentao Xu,Jingjing Zheng,Yong Luo.Synthesis of titanium carbide coating on Ti15Mo alloy and its tribological behaviour[J].Biosurface and Biotribology,2023,9(4):176-186.
9Xiong Liu,Chaojiang Niu.Bilayer solid-electrolyte interphase structure enables a 440 Wh kg^(-1) lithium metal pouch cell to achieve 130 cycles[J].Science China Chemistry,2024,67(3):751-752.
10Cijun Shuai,Desheng Li,Xiong Yao,Xia Li,Chengde Gao.Additive manufacturing of promising heterostructure for biomedical applications[J].International Journal of Extreme Manufacturing,2023,5(3):363-405. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG139[一般工业技术—材料科学与工程]
Citation Information:
Initially defined high entropy alloys(HEAs)usually exhibit a single-phase solid-solution structure.However,two and/or more types of phases in HE As possibly induce the desired microstructure features,which contribute to improving the wear properties of HE As.Here,we prepare a series of(AlCoCrFeNi)100-xHfx(x=0,2,4and 6;at%) HEAs and concern their phase compositions,micro structures and wear properties.Hf leads to the formation of(Ni,Co)2Hf-type Laves phase and tailors the microstructure from a body-centered cubic(BCC) singlephase structure to a hypoeutectic structure.An increased hardness from~HV 512.3 to~HV 734.1 is due to solid-solution strengthening,grain refinement strengthening and precipitated phase strengthening.And a few oxides(Al2O3+Cr2O3) caused by the wear heating contribute to an 85.5% decrease in wear rate of the HEA system from6.71×10-5 to 0.97×10-5 m3·N-1·m-1.In addition,Hf addition changes the wear mechanism from abrasive wear,mild oxidative wear and adhesive wear to oxidative wear and adhesive wear.
quote
| GB/T 7714-2015 | [1] Hao Ren, Rui-Run Chen, Xue-Feng Gao, et al. Rare Metals, 2024(1): 324-333. |
| MLA | [1] Hao Ren, et al., Rare Metals, no. 1, 2024, pp. 324-333. |
| APA | [1] Hao Ren, Rui-Run Chen, Xue-Feng Gao, Tong Liu, Gang Qin, Yu-Lung Chiu, Shi-Ping Wu, & Jing-Jie Guo. (2024). Rare Metals(1), 324-333. |
| IEEE | [1] Hao Ren, Rui-Run Chen, Xue-Feng Gao, Tong Liu, Gang Qin, Yu-Lung Chiu, Shi-Ping Wu, and Jing-Jie Guo, Rare Metals, no. 1, pp. 324-333, 2024. |