Transparent, Antifreezing, Ionic Conductive Carboxymethyl Chitosan Hydrogels as Multifunctional Sensors AITranslate

South China Agricultural University; South China Agricultural University; South China Agricultural University; South China Agricultural University; South China Agricultural University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

By a simple strategy of immersion in a CaCl2 solution, carboxymethyl chitosan hydrogels exhibited ultralow-temperature freezing resistance below −50 °C. In addition, the introduction of electrolyte ions endowed the hydrogels with electrical conductivity, showing stable and reversible sensitivity to human activity, such as finger bending, pressing, and pharyngeal swallowing. The conductive carboxymethyl chitosan hydrogels could even be assembled into a two-dimensional integrated array of contact sensors, which successfully perceived the contour and pressure distribution of an object with a certain resolution. These transparent biological-based antifreezing conductive hydrogels are promising to find applications in integrated wearable sensing devices under extremely low temperature environments.

KeyWords AITranslate

carboxymethyl chitosan antifreezing biobased material conductive hydrogel sensor
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00487

Chinese Library Classification Number:

Citation Information:

By a simple strategy of immersion in a CaCl2 solution, carboxymethyl chitosan hydrogels exhibited ultralow-temperature freezing resistance below −50 °C. In addition, the introduction of electrolyte ions endowed the hydrogels with electrical conductivity, showing stable and reversible sensitivity to human activity, such as finger bending, pressing, and pharyngeal swallowing. The conductive carboxymethyl chitosan hydrogels could even be assembled into a two-dimensional integrated array of contact sensors, which successfully perceived the contour and pressure distribution of an object with a certain resolution. These transparent biological-based antifreezing conductive hydrogels are promising to find applications in integrated wearable sensing devices under extremely low temperature environments.

quote

GB/T 7714-2015 [1] Caimei Zhao, Xinhu Gong, Lan Shen, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00487.
MLA [1] Caimei Zhao, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00487.
APA [1] Caimei Zhao, Xinhu Gong, Lan Shen, Yang Wang, & Chaoqun Zhang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00487
IEEE [1] Caimei Zhao, Xinhu Gong, Lan Shen, Yang Wang, and Chaoqun Zhang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00487. keywords: {carboxymethyl chitosan;antifreezing;biobased material;conductive hydrogel;sensor}