Selective Laser Sintering 4D Printing of Dynamic Cross-linked Polyurethane Containing Diels–Alder Bonds AITranslate

Sichuan University; Sichuan University; Sichuan University; Sichuan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Selective laser sintering (SLS) four-dimensional (4D) printing of smart materials remains a big challenge and largely unexplored due to the lack of suitable materials. Here, we developed one kind of polyurethane containing reversible Diels–Alder bond (PUDA) covalent adaptable network (CAN) with self-healing and shape memory functions for SLS 4D printing. The dynamic mechanism of the Diels–Alder bonds was confirmed by 1H NMR and in situ FTIR. Furthermore, the kg-scale PUDA materials as well as their carbon nanotube (CNT) composite powders were prepared by the freeze-grinding method. The SLS printed PUDA materials show nearly isotropic mechanical properties due to the improved interlayer interaction by dynamic cross-linking. The SLS printed PUDA/CNT composites possess NIR-triggered self-healing and shape memory functions. This study provides a paradigm for designing dynamic polymers/composites for SLS 4D printing.

KeyWords AITranslate

selective laser sintering 4D printing selfhealing shape memory Diels−Alder NIRlight responsive
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00565

Chinese Library Classification Number:

Citation Information:

Selective laser sintering (SLS) four-dimensional (4D) printing of smart materials remains a big challenge and largely unexplored due to the lack of suitable materials. Here, we developed one kind of polyurethane containing reversible Diels–Alder bond (PUDA) covalent adaptable network (CAN) with self-healing and shape memory functions for SLS 4D printing. The dynamic mechanism of the Diels–Alder bonds was confirmed by 1H NMR and in situ FTIR. Furthermore, the kg-scale PUDA materials as well as their carbon nanotube (CNT) composite powders were prepared by the freeze-grinding method. The SLS printed PUDA materials show nearly isotropic mechanical properties due to the improved interlayer interaction by dynamic cross-linking. The SLS printed PUDA/CNT composites possess NIR-triggered self-healing and shape memory functions. This study provides a paradigm for designing dynamic polymers/composites for SLS 4D printing.

quote

GB/T 7714-2015 [1] Hao Ouyang, Xue Li, Xili Lu, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00565.
MLA [1] Hao Ouyang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00565.
APA [1] Hao Ouyang, Xue Li, Xili Lu, & Hesheng Xia. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00565
IEEE [1] Hao Ouyang, Xue Li, Xili Lu, and Hesheng Xia, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00565. keywords: {selective laser sintering;4D printing;selfhealing;shape memory;Diels−Alder;NIRlight responsive}