Structural Polyfluorene Derivative Nanocarriers with Promising Fluorescence Emission and Antifouling Properties AITranslate

Zhejiang University of Technology; Zhejiang University of Technology; Zhejiang University of Technology; UCSI University; Zhejiang University of Technology; Zhejiang University of Technology; The University of Akron
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Herein, a zwitterionic PF-based copolymer, polyfluorene-a-polybenzothiadiazole-g-polycaprolactone-b-poly[3-dimethyl(methacryloxyethyl)-propaneammoniumsulfonate] [PF-a-PBTH-g-(PCL-b-PDMAPS)], was synthesized by combining multiple polymerization techniques and further quaternization. The resultant copolymer with optimized structures (P5) was able to form stabilized unimolecular micelles in an aqueous solution with a diameter of approximately 110 nm. The unique donor–acceptor structure between fluorene and benzothiadiazole group along the conjugated main chains endows copolymers with yellow-green fluorescence, while the PDMAPS chains with a unique zwitterionic nature enabled not only to enhance water solubility, drug loading efficiency (DLE), and drug loading capacity (DLC) of the whole copolymers but also to present promising antifouling property by preventing nonspecific protein/bacteria adhesion. Further in vivo and in vitro experiments demonstrate that the resultant P5 micelles also present lower cytotoxicity and efficient cellular uptake with the incubation of HeLa and HUVEC cells, which tends to prolong the circulation time of drugs. Our work not only provides a rational combination of zwitterions and polyfluorenes to significantly enhance the water solubility of hydrophobic fluorophores but also exhibits the potential of promising bioimaging for dual stimuli-responsive micelles in vitro (simulated body fluids) and in vivo (open).

KeyWords AITranslate

antifouling zwitterionic polyfluorene colloids fluorescent polymers
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00479

Chinese Library Classification Number:

Citation Information:

Herein, a zwitterionic PF-based copolymer, polyfluorene-a-polybenzothiadiazole-g-polycaprolactone-b-poly[3-dimethyl(methacryloxyethyl)-propaneammoniumsulfonate] [PF-a-PBTH-g-(PCL-b-PDMAPS)], was synthesized by combining multiple polymerization techniques and further quaternization. The resultant copolymer with optimized structures (P5) was able to form stabilized unimolecular micelles in an aqueous solution with a diameter of approximately 110 nm. The unique donor–acceptor structure between fluorene and benzothiadiazole group along the conjugated main chains endows copolymers with yellow-green fluorescence, while the PDMAPS chains with a unique zwitterionic nature enabled not only to enhance water solubility, drug loading efficiency (DLE), and drug loading capacity (DLC) of the whole copolymers but also to present promising antifouling property by preventing nonspecific protein/bacteria adhesion. Further in vivo and in vitro experiments demonstrate that the resultant P5 micelles also present lower cytotoxicity and efficient cellular uptake with the incubation of HeLa and HUVEC cells, which tends to prolong the circulation time of drugs. Our work not only provides a rational combination of zwitterions and polyfluorenes to significantly enhance the water solubility of hydrophobic fluorophores but also exhibits the potential of promising bioimaging for dual stimuli-responsive micelles in vitro (simulated body fluids) and in vivo (open).

quote

GB/T 7714-2015 [1] Liangliang Zhu, Zejian He, Yifan Zhang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00479.
MLA [1] Liangliang Zhu, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00479.
APA [1] Liangliang Zhu, Zejian He, Yifan Zhang, Moontarij Jahan Orvy, Jintao Yang, Mi Zhou, & Dong Zhang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00479
IEEE [1] Liangliang Zhu, Zejian He, Yifan Zhang, Moontarij Jahan Orvy, Jintao Yang, Mi Zhou, and Dong Zhang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00479. keywords: {antifouling;zwitterionic;polyfluorene;colloids;fluorescent polymers}