Study on Injection Molding Process of WC-10Co Ultrafine Grained Cemented Carbide AITranslate
Abstract AITranslate
Various factors influencing injection molding of WC-10Co ultrafine grained cemented carbide were studied. The processes of ball milling, injection, debinding and sintering were optimized. The results indicate that injection molding WC-10Co ultrafine grained cemented carbide sintered parts have the best performance after 1.0 h vacuum sintering at 1440 ℃ ,with cemented carbide grain size of 0. 465μm,density of 13.99 g/cm^3 and HRA hardness of 90.1.
KeyWords AITranslate
1邬荫芳.粘结相相变机制的研究[J].硬质合金,2004,21(2):65-69. 被引量:4
2汪中玮.高抗腐蚀、耐磨损、镍粘结相硬质合金的研究[J].中国钨业,2011,26(4):40-43. 被引量:3
3朱运锋,叶金文,刘颖,朱军,马世卿,张蛟.(V,Ti)(C,N)固溶体粉末对WC-8%Co硬质合金性能的影响[J].功能材料,2013,44(15):2239-2243. 被引量:6
4左洪松,栾道成,王正云,李亚军,秦琴.不同含量复式碳化物对细晶硬质合金性能的影响[J].中国钨业,2011,26(6):27-30. 被引量:6
5饶承毅,龙坚战,袁红梅.Ni含量对粗晶WC-Co-Ni硬质合金组织和性能的影响[J].硬质合金,2012,29(1):11-14. 被引量:9
6付龙,柳学全,李一,丁存光,李立鑫,姜丽娟.国内外矿用高耐磨、高韧性硬质合金新技术[J].硬质合金,2012,29(4):254-261. 被引量:31
7刘超,吝楠,贺跃辉,王宇川,张翔.添加粗晶WC对WC-Co硬质合金组织与力学性能的影响[J].粉末冶金材料科学与工程,2014,19(1):123-129. 被引量:15
8白英龙,吴冲浒,杨霞,徐猛,果世驹.粗细晶WC基体对WC-Co非均匀结构显微组织形成的影响[J].粉末冶金技术,2012,30(2):89-97. 被引量:14
9魏崇斌,宋晓艳,付军,吕效森,陆庆忠,高杨,王海滨.烧结方法对WC-Co硬质合金性能的影响[J].粉末冶金材料科学与工程,2012,17(3):315-320. 被引量:14
10潘永智,艾兴,赵军,李光业,宋良煜.超细晶粒硬质合金的高速摩擦磨损特性研究[J].摩擦学学报,2008,28(1):78-82. 被引量:21
1谢兴铖,曹瑞军,林中坤,李卿.WC粒度对WC/10Co注射成形工艺的影响[J].稀有金属材料与工程,2020,49(1):147-152. 被引量:1
2杨宇,袁建坤,陈鹏起,郎宏彬,霍俊豪,程继贵.微晶蜡基粘结剂应用于YG10硬质合金注射成形的研究[J].粉末冶金工业,2022,32(6):10-15. 被引量:1
3康俊,张越,周永贵,姚艳斌,林炽余.超细硬质合金数控螺纹刀片注射成形工艺质量及缺陷控制[J].粉末冶金工业,2022,32(6):121-126.
4罗学全,刘孙和,温光华.超细硬质合金注射成形的溶剂脱脂及脱脂临界厚度[J].粉末冶金技术,2023,41(2):131-136.
5祝贤智,成会朝,周承商,刘咏.挤出式3D打印工艺制备WC-10Co硬质合金的显微结构与力学性能[J].粉末冶金材料科学与工程,2023,28(2):141-150.
1林驰皓,胡可,王明辉,雷久淮,林波.铜粉对MIM钨铜合金组织和性能的影响[J].粉末冶金工业,2023,33(1):24-30.
2黄永强,申小平,康利梅.烧结钎焊粉末冶金铁基零件的材料成分与结构优化[J].粉末冶金工业,2023,33(4):32-37.
1杨佩,李维,张智.热处理制度对纯钛棒材晶粒度的影响[J].机械工程与自动化,2017,0(6):124-125.
2宋心英.浅谈逻辑控制器在球磨机油路保护系统中的应用[J].南方金属,2017(6):44-46.
3卢利平,毕巍巍.应变比对汽车前罩内板成形性能影响的数值模拟[J].热加工工艺,2017,46(21):140-143. 被引量:2
4孙华,周蕾,王占花,刘磊,李慎,赵秀明,毛向阳.正火处理对胀断连杆用C70S6非调质钢组织和力学性能的影响[J].金属热处理,2017,42(11):93-97. 被引量:5
5周志明,杨波,袁林,黄灿,李成信,谷成渝,陈曦,刘伟.双锥形铝合金挤压件成形工艺及数值模拟[J].热加工工艺,2017,46(21):94-97. 被引量:2
6唐全波.铝合金薄壁筒形零件尺寸稳定化加工工艺[J].特种铸造及有色合金,2017,37(11):1189-1191. 被引量:3
7卢云,吴志林,李灿灿.AZ80镁合金管材反挤压成形的数值模拟与试验研究[J].特种铸造及有色合金,2017,37(11):1201-1205. 被引量:3
8陈继平,钱健清,王会廷.渐进成形锥形件壁厚的正弦定理预测精度研究[J].中国机械工程,2017,28(22):2760-2766. 被引量:5
9杨钦鑫,童国权,何泽洲.钛合金二层板结构超塑成形/扩散连接试验研究[J].稀有金属,2017,41(12):1305-1310. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]
Citation Information:
Various factors influencing injection molding of WC-10Co ultrafine grained cemented carbide were studied. The processes of ball milling, injection, debinding and sintering were optimized. The results indicate that injection molding WC-10Co ultrafine grained cemented carbide sintered parts have the best performance after 1.0 h vacuum sintering at 1440 ℃ ,with cemented carbide grain size of 0. 465μm,density of 13.99 g/cm^3 and HRA hardness of 90.1.
quote
| GB/T 7714-2015 | [1] SHANG Feng, FU Jie, QIAO Bin, et al. Study on Injection Molding Process of WC-10Co Ultrafine Grained Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2017(5): 63-68. |
| MLA | [1] SHANG Feng, et al., "Study on Injection Molding Process of WC-10Co Ultrafine Grained Cemented Carbide." Rare Metals and Cemented Carbides, no. 5, 2017, pp. 63-68. |
| APA | [1] SHANG Feng, FU Jie, QIAO Bin, LI Hua-qiang, CAO Zhen-wei, & SUN Wei. (2017). Study on Injection Molding Process of WC-10Co Ultrafine Grained Cemented Carbide. Rare Metals and Cemented Carbides(5), 63-68. |
| IEEE | [1] SHANG Feng, FU Jie, QIAO Bin, LI Hua-qiang, CAO Zhen-wei, and SUN Wei, "Study on Injection Molding Process of WC-10Co Ultrafine Grained Cemented Carbide," Rare Metals and Cemented Carbides, no. 5, pp. 63-68, 2017. keywords: {ultrafine grained cemented carbide;WC-10Co;inj eetion molding;debinding;sintering;process} |