Effects of Carbon Content on WC Grain Growth Activation Energy of WC-6Co Ultrafine Cemented Carbides AITranslate
Abstract AITranslate
WC-6Co ultrafine cemented carbides were prepared at different sintering temperature and using the mixtures with different total carbon content (6.11%,6.13%,6.15%,6.17%, 6.19%, 6.21%,6.23% and 6.25%). The magnetic properties and microstructure of the samples were analyzed, and the effects were studied of carbon content on WC grain growth activation energy of WC-6Co cemented carbides. The results show that with the increase of total carbon content,cobalt magnetism (Com) of the alloy sample is also gradually increased. For WC-6Co sintered at different temperature, corecive force (He) firstly increa- ses and then decreases,and WC grain size decreases at first and then increases with the increase of Com. When the Corn value is about 5 %, Hc reaches the maximum and WC grain size reaches the minimum. WC grain growth activation energy firstly increases and then decreases with Com increasing, and reaches the maximum when Corn is about 5.2%. With the increase of carbon content in a low range,more (Crx ,Vy)Cx carbide (a grain growth inhibitor) is generated on the WC grain surface. But with the further increase of carbon content,the production amount of (Crx, Vy)Cz carbide has reached the extreme value, while the temperature for generating liquid phase further declines and liquid volume dramatically increases, resulting in decreased WC grain growth activation energy.
KeyWords AITranslate
1谢海根,易丹青,黄道远,李荐,刘刚,刘瑞.超细晶硬质合金的制备[J].稀有金属与硬质合金,2007,35(4):14-17. 被引量:15
2刘小胡,时凯华,闵召宇,杨新宇,廖军,吴翔.合金碳含量和烧结气氛对WC-6%Co超细硬质合金表面形貌及成分的影响[J].稀有金属,2015,39(9):799-806. 被引量:2
3肖逸锋,贺跃辉,丰平,谢宏,张丽娟,黄自谦,黄伯云.碳含量对缺碳硬质合金组织和性能的影响[J].中国有色金属学报,2007,17(1):39-44. 被引量:26
4吴悦梅,熊计,赖人铭.碳含量对WC-Co硬质合金显微组织的影响及其控制[J].硬质合金,2008,25(3):179-185. 被引量:25
5张梅琳,朱世根,朱守星.超细及纳米硬质合金中碳含量的变化及对组织性能的影响[J].材料导报,2006,20(8):65-68. 被引量:24
6钱开友,王兴庆,何宝山,郭海亮,白佳声.碳含量对纳米硬质合金组织和性能的影响[J].上海大学学报:自然科学版,2002,8(5):433-436. 被引量:21
7肖仲文,杨慧敏,白佳声.硬质合金气氛烧结过程中碳含量调整[J].硬质合金,2003,20(4):204-207. 被引量:7
8张守全.碳含量对WC-10Co-0.6Cr_3C_2硬质合金组织结构与性能的影响[J].粉末冶金材料科学与工程,2014,19(3):446-450. 被引量:14
9李重典,时凯华,王海霞,廖军,闵召宇,徐志超.碳含量对WC-8.0%Co硬质合金性能及微观组织的影响[J].四川冶金,2015,37(4):9-13. 被引量:2
10黄翔,易丹青,王斌,刘会群,陈丽勇,李会会,朱慧娟.V和Cr对超细WC-Co硬质合金Co粘结相成分与WC/Co界面组织结构的影响[J].粉末冶金材料科学与工程,2016,21(1):95-102. 被引量:8
1郑清宏,敖小龙,辛海燕,黄伟,林应镁.淬火及深冷处理对渗碳硬质合金组织结构与力学性能的影响[J].稀有金属与硬质合金,2021,49(1):88-91. 被引量:3
2唐彦渊,钟志强,羊求民,王红云,徐国钻.碳含量对WC-10Co硬质合金微观组织及力学性能的影响[J].稀有金属与硬质合金,2021,49(6):73-78. 被引量:6
3李云龙.氧化预处理对超细晶硬质合金材料性能的影响[J].稀有金属与硬质合金,2022,50(6):83-89.
1王焕敏,侯兆敏.传动套中渗碳淬火变形及工艺控制研究[J].中国金属通报,2021(6):279-280.
2易晓鸥,王方方,梁自强,陶星豪,辛浩翔.WC-Co硬质合金的深冷处理改性与显微机制[J].硬质合金,2021,38(3):219-228. 被引量:1
3倪莹驰,江佳阳,董凯林,时凯华.不同添加剂对(W,Mo)C-6%Ni合金性能的影响[J].硬质合金,2022,39(2):118-126.
4罗威,杨诚辉,陈邦明,钟志强,唐彦渊.高频燃烧红外吸收法测定碳化钨粉总碳量[J].硬质合金,2022,39(6):490-494.
5孙化鑫,徐淑波,李辉,郑君姿,卢庆亮.Ni含量对WC-Co-Ni硬质合金的力学性能和耐腐蚀性能的影响[J].稀有金属与硬质合金,2022,50(6):77-82.
6胡启明,廖宇.贫碳WC-12%(Co+Ni)硬质合金微观组织与性能[J].硬质合金,2023,40(1):66-72.
7秦永强,袁健,罗来马,田宇,彭宇强,吴玉程.热处理对Y_(2)O_(3)掺杂WC-Co硬质合金显微组织及性能的影响[J].材料热处理学报,2023,44(4):40-46.
8苏畅,杨冰,宋江杰,肖守讷,阳光武,朱涛.深冷处理对EA4T车轴钢马氏体组织及短裂纹行为的影响[J].中南大学学报:自然科学版,2023,54(4):1300-1310.
9江佳阳,廖军,顾金宝,梁靖岳.WC粒度、配碳量对WC-9%Ni硬质合金组织与性能的影响[J].硬质合金,2023,40(4):288-295.
1李琴堂.怎样证明条件等式[J].数学教学通讯,1986,0(4):27-28.
2叶子.膝骨关节炎与代谢综合征患者瘦素、脂联素、TNF-α与胰岛素抵抗水平变化及相关因素分析[J].浙江医学,2017,39(21):1901-1903. 被引量:1
3尚桂凤,李建坤.强化养殖污染治理促进低碳畜牧业发展[J].中国畜牧兽医文摘,2017,33(10):16-16. 被引量:1
4张雪辉,黄柱,徐畅,李晓闲,蔡志勇,陈颢.Cr_3C_2对SPS烧结WC-6Co硬质合金组织与性能的影响[J].中国有色金属学报,2017,27(8):1580-1588. 被引量:10
5于涛,贺鸣,罗学全,温光华,陈响明,王社权.WC在湿磨中的分散与破碎过程研究[J].硬质合金,2017,34(3):155-166. 被引量:10
6张瀚龙,朱晓东,薛鹏.退火工艺对超高强冷轧马氏体钢板力学性能的影响[J].宝钢技术,2017,10(5):27-32. 被引量:3
7一种高强度钢、钢管及其制造方法[J].宝钢技术,2017,0(5):54-54.
8孙丹萍.清热降脂方联合奥利司他治疗单纯性肥胖临床研究[J].陕西中医药大学学报,2017,40(6):47-49. 被引量:2
9郭庆云,王强.制氢转化炉下猪尾管变形失效分析[J].石油化工设备技术,2017,38(5):35-39.
10欧阳熙琴.数学问题2313号的简证与探究[J].数学通报,2017,56(11):53-54. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
WC-6Co ultrafine cemented carbides were prepared at different sintering temperature and using the mixtures with different total carbon content (6.11%,6.13%,6.15%,6.17%, 6.19%, 6.21%,6.23% and 6.25%). The magnetic properties and microstructure of the samples were analyzed, and the effects were studied of carbon content on WC grain growth activation energy of WC-6Co cemented carbides. The results show that with the increase of total carbon content,cobalt magnetism (Com) of the alloy sample is also gradually increased. For WC-6Co sintered at different temperature, corecive force (He) firstly increa- ses and then decreases,and WC grain size decreases at first and then increases with the increase of Com. When the Corn value is about 5 %, Hc reaches the maximum and WC grain size reaches the minimum. WC grain growth activation energy firstly increases and then decreases with Com increasing, and reaches the maximum when Corn is about 5.2%. With the increase of carbon content in a low range,more (Crx ,Vy)Cx carbide (a grain growth inhibitor) is generated on the WC grain surface. But with the further increase of carbon content,the production amount of (Crx, Vy)Cz carbide has reached the extreme value, while the temperature for generating liquid phase further declines and liquid volume dramatically increases, resulting in decreased WC grain growth activation energy.
quote
| GB/T 7714-2015 | [1] HUANG Tian-zhen, WU En-xi, LI Yong-xia, et al. Effects of Carbon Content on WC Grain Growth Activation Energy of WC-6Co Ultrafine Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2017(5): 57-62. |
| MLA | [1] HUANG Tian-zhen, et al., "Effects of Carbon Content on WC Grain Growth Activation Energy of WC-6Co Ultrafine Cemented Carbides." Rare Metals and Cemented Carbides, no. 5, 2017, pp. 57-62. |
| APA | [1] HUANG Tian-zhen, WU En-xi, LI Yong-xia, ZOU Dan, & XIE Yuan-yan. (2017). Effects of Carbon Content on WC Grain Growth Activation Energy of WC-6Co Ultrafine Cemented Carbides. Rare Metals and Cemented Carbides(5), 57-62. |
| IEEE | [1] HUANG Tian-zhen, WU En-xi, LI Yong-xia, ZOU Dan, and XIE Yuan-yan, "Effects of Carbon Content on WC Grain Growth Activation Energy of WC-6Co Ultrafine Cemented Carbides," Rare Metals and Cemented Carbides, no. 5, pp. 57-62, 2017. keywords: {ultrafine cemented carbide;WC-6Co;total carbon;Corn;WC grain size;WC grain growth activa-tion energy} |