Effect of Arc Current on Microstructure and Mechanical Properties of Cr Coatings Deposited by Multi-arc Ion Plating AITranslate

School of Mechanical Engineering, Nanhua University;School of Mechanical Engineering, Nanhua University;School of Mechanical Engineering, Nanhua University;School of Mechanical Engineering, Nanhua University;School of Mechanical Engineering, Nanhua University;School of Mechanical Engineering, Nanhua University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The pure Cr coatings were deposited on the surface of zirconium alloy by multi-arc ion plating technology. The effects of arc current on surface morphology, phase composition and interracial adhesion were analyzed by scanning electron microscopy (SEM) ,X-ray diffractometer (XRD) and scratch tester. Image J image processing software was used for statistics and analysis of the distribution of the micro particles in the surface of pure Cr coatings. The results show that with the increase of arc current, the size of microparticles in pure Cr coating surface increases firstly and then decreases,while the number of microparticles in the unit area decreases firstly and then increases. Meanwhile,preferred orientation of the pure Cr coatings changes from (110) crystal face to (200) crystal face, and interracial adhesion of pure Cr coatings to Zr alloy substrate decreases at first and then increases with the increase of arc current.

KeyWords AITranslate

pure Cr coating multi-arc ion plating arc current SEM morphology phase composition interracial adhesion

1李洪涛,蒋百灵,曹政,陈雪,乔泳彭.偏压对磁控溅射纯Cr镀层组织形貌及耐腐蚀性能的影响[J].西安理工大学学报,2009,25(2):141-145. 被引量:8

2魏祥飞,张平则,魏东博,周鹏,张扬,陈小虎,王琼,王若男.多弧离子镀Cr涂层对γ-TiAl合金高温氧化性能的影响[J].稀有金属材料与工程,2014,43(3):707-711. 被引量:8

3陈昌浩,金永中,刘东亮,余学金.负偏压对多弧离子镀TiN涂层大颗粒形貌及像素分布的影响[J].表面技术,2015,44(11):29-34. 被引量:4

4龚才,代明江,陈明安,韦春贝,侯惠君.基体材料对TiN薄膜表面液滴及薄膜结合力的影响[J].中国表面工程,2013,26(1):27-33. 被引量:15

1周军,樊湘芳,李涛,邱长军,李怀林.弧电流对多弧离子镀TiAlN涂层表面形貌和性能的影响[J].材料保护,2018,51(6):74-78. 被引量:3

1王梦超,王丽君,陈辉.U71Mn钢轨铣削用PVD-TiAlN涂层刀片失效分析[J].表面技术,2020,49(3):300-308. 被引量:1

2方波,张林,蔡飞,张世宏.冷作模具钢等离子渗镀CrVN复合涂层摩擦磨损性能研究[J].真空,2020,57(2):33-39. 被引量:2

3吴浩龙,王天国.氮氩比对模具钢表面镀TiAlN薄膜形貌和性能的影响[J].材料保护,2020,53(8):43-47. 被引量:2

1潘成刚,冯斯琦,赵川翔,常庆明.预热温度对自蔓延TiC/Ni功能梯度涂层的影响[J].特种铸造及有色合金,2017,37(11):1170-1175. 被引量:2

2王璐,金永中,林修洲,陈昌浩.基片偏压占空比对多弧离子镀TiAlSiN涂层形貌及力学性能的影响[J].表面技术,2017,46(11):237-240. 被引量:5

3白雪冰,李金龙,朱丽慧,王永欣,王立平.多弧离子镀制备TiSiN-Cu涂层的结构和摩擦学性能[J].表面技术,2017,46(11):96-103. 被引量:4

4《黑龙江科技大学学报》稿约[J].黑龙江科技大学学报,2017,27(4):448-448.

5程娟.壳聚糖对脆弱丝绸的加固保护初探[J].广州化工,2017,45(18):54-56.

6关晓艳,王永欣,李泽超,李金龙,鲁侠,王立平,薛群基.金属Cr层对Cr/Cr_2N纳米多层涂层的性能影响[J].表面技术,2017,46(11):15-21. 被引量:2

7刘晓燕,王爱兵,贾丽娜.工程车活塞杆用45~#钢电沉积Ni-WC纳米复合镀层的研究[J].电镀与环保,2017,37(6):5-7. 被引量:1

8顾建余.简析紫砂泥料特性和茶文化的关系[J].陶瓷科学与艺术,2017,0(10):94-94. 被引量:14

9宋力刚,朱特,曹兴忠,张仁刚,况鹏,靳硕学,张鹏,龚毅豪,王宝义.硫化温度对ZnS薄膜生长质量的影响[J].原子核物理评论,2017,34(3):651-655. 被引量:2

10李威,顾巍.长链非编码RNA MACC1-AS1对乳腺癌细胞增殖和侵袭的影响[J].汕头大学医学院学报,2017,30(3):129-132.

Basic Information:

DOI:

Chinese Library Classification Number:TG144[金属学及工艺—金属材料]

Citation Information:

The pure Cr coatings were deposited on the surface of zirconium alloy by multi-arc ion plating technology. The effects of arc current on surface morphology, phase composition and interracial adhesion were analyzed by scanning electron microscopy (SEM) ,X-ray diffractometer (XRD) and scratch tester. Image J image processing software was used for statistics and analysis of the distribution of the micro particles in the surface of pure Cr coatings. The results show that with the increase of arc current, the size of microparticles in pure Cr coating surface increases firstly and then decreases,while the number of microparticles in the unit area decreases firstly and then increases. Meanwhile,preferred orientation of the pure Cr coatings changes from (110) crystal face to (200) crystal face, and interracial adhesion of pure Cr coatings to Zr alloy substrate decreases at first and then increases with the increase of arc current.

quote

GB/T 7714-2015 [1] CENG Xiao-an, HUANG He, ZHANG Wen, et al. Effect of Arc Current on Microstructure and Mechanical Properties of Cr Coatings Deposited by Multi-arc Ion Plating[J]. Rare Metals and Cemented Carbides, 2017(5): 53-56.
MLA [1] CENG Xiao-an, et al., "Effect of Arc Current on Microstructure and Mechanical Properties of Cr Coatings Deposited by Multi-arc Ion Plating." Rare Metals and Cemented Carbides, no. 5, 2017, pp. 53-56.
APA [1] CENG Xiao-an, HUANG He, ZHANG Wen, WANG Hao-ran, LIU Zan, & QIU Zhang-jun. (2017). Effect of Arc Current on Microstructure and Mechanical Properties of Cr Coatings Deposited by Multi-arc Ion Plating. Rare Metals and Cemented Carbides(5), 53-56.
IEEE [1] CENG Xiao-an, HUANG He, ZHANG Wen, WANG Hao-ran, LIU Zan, and QIU Zhang-jun, "Effect of Arc Current on Microstructure and Mechanical Properties of Cr Coatings Deposited by Multi-arc Ion Plating," Rare Metals and Cemented Carbides, no. 5, pp. 53-56, 2017. keywords: {pure Cr coating;multi-arc ion plating;arc current;SEM morphology;phase composition;interracial adhesion}