Finite Element Simulation Study of EHM Cutting Performance of Cemented Carbide Cutting Tool AITranslate
Abstract AITranslate
On the basis of the formula of temperature rise caused by resistance Joule heat during EHM cutring process,cutting simulation tests were carried out using finite element analysis software DEFORM.and the cutting process was simulated of 45 steel by cemented carbide cutting tool with different current intensity. Temperature field of tool and tool-chip contact area and tool wear change rule with different current intensity were analyzed based on calculation. The results show that compared with the no-current cutting process.current input can reduce the tool temperature and tool wear,and with the current intensity increasing. the tool temperature is significantly reduced.
KeyWords AITranslate
1叶邦彦,周泽华.难加工材料导电加热切削机理的研究[J].华南理工大学学报:自然科学版,1994,22(5):93-99. 被引量:14
2徐兰英,叶邦彦,伍强,王伟文,彭锐涛.绿色切削的导电加热切削加工新工艺[J].机械与电子,2008,26(8):74-76. 被引量:3
3陈文戈,叶邦彦.导电加热切削技术综述[J].电加工,1999(2):28-31. 被引量:6
4吴拓,叶邦彦.导电加热切削刀具磨损特性及刀具适应性的研究[J].西江大学学报,1999,20(1):71-75. 被引量:1
5罗翔,陈文戈,叶邦彦.导电加热切削最佳加热电流的确定[J].机械制造,1998,36(5):18-20. 被引量:1
6吴拓,叶邦彦,赵学智.利用导电加热切削抑制积屑瘤和鳞刺的研究[J].工具技术,1998,32(12):8-10. 被引量:6
7刘新,徐文骥,孙晶,张琳.导电加热切削有限元仿真及试验研究[J].中国机械工程,2012,23(21):2556-2561. 被引量:5
8梁宇红.基于Deform的切削加工有限元仿真分析[J].机械工程与自动化,2013(5):45-47. 被引量:1
1赵世纬,李德玉.浅谈工程材料课的问题与改革[J].高等农业教育,1984,0(3):49-51.
2杨军胜,关悦,张昭,袁恒超,袁启明.P(BMA/2-EHM/St)高吸油树脂的制备及性能研究[J].陕西科技大学学报,2017,35(5):122-127. 被引量:2
3周久璘,贾广善,杨树崤.关于电源内部场强方向的讨论[J].物理教师,1985,0(4):36-37.
4王葛,刘胜强,胡鑫,陈博伟,李磊,李强.Cr5钢支承辊水-空交替淬火过程数值模拟与实验[J].材料热处理学报,2017,38(11):125-132. 被引量:4
5陈宝华.五轴联动数控工具磨床工作台运动方案与结构设计探究[J].内燃机与配件,2017(24):57-58. 被引量:3
6皮云云,夏伟.基于Deform的刃带宽度对大应变挤出切削过程的影响分析[J].机床与液压,2017,45(20):13-16. 被引量:1
7尹浩,郑雷.7075铝合金切削过程晶粒尺寸和硬度变化的研究[J].组合机床与自动化加工技术,2017(11):107-111. 被引量:2
8郭明君.电源路端电压的再讨论[J].物理教师,1986,0(3):39-40.
9周桂生,李举.自动扶梯节能运行控制系统设计[J].通信电源技术,2017,34(4):108-111. 被引量:2
10王海.对新物理课本中电阻和欧姆定律这部分内容改写的意见[J].物理教师,1984,0(2):35-36.
Basic Information:
DOI:
Chinese Library Classification Number:TG661[金属学及工艺—金属切削加工及机床]
Citation Information:
On the basis of the formula of temperature rise caused by resistance Joule heat during EHM cutring process,cutting simulation tests were carried out using finite element analysis software DEFORM.and the cutting process was simulated of 45 steel by cemented carbide cutting tool with different current intensity. Temperature field of tool and tool-chip contact area and tool wear change rule with different current intensity were analyzed based on calculation. The results show that compared with the no-current cutting process.current input can reduce the tool temperature and tool wear,and with the current intensity increasing. the tool temperature is significantly reduced.
quote
| GB/T 7714-2015 | [1] KANG Yu-hua, DONG Lin, XIANG Biao, et al. Finite Element Simulation Study of EHM Cutting Performance of Cemented Carbide Cutting Tool[J]. Rare Metals and Cemented Carbides, 2017(5): 69-73. |
| MLA | [1] KANG Yu-hua, et al., "Finite Element Simulation Study of EHM Cutting Performance of Cemented Carbide Cutting Tool." Rare Metals and Cemented Carbides, no. 5, 2017, pp. 69-73. |
| APA | [1] KANG Yu-hua, DONG Lin, XIANG Biao, & LIU Xiong. (2017). Finite Element Simulation Study of EHM Cutting Performance of Cemented Carbide Cutting Tool. Rare Metals and Cemented Carbides(5), 69-73. |
| IEEE | [1] KANG Yu-hua, DONG Lin, XIANG Biao, and LIU Xiong, "Finite Element Simulation Study of EHM Cutting Performance of Cemented Carbide Cutting Tool," Rare Metals and Cemented Carbides, no. 5, pp. 69-73, 2017. keywords: {cemented carbide cutting tool;electric hot machining;tool temperature;tool wear;DEFORM} |