Study of WC Leaching Mechanism from Cemented Carbide Blade AITranslate

School of Mechanical Engineering, Hebei United University;School of Mechanical Engineering, Hebei United University;School of Mechanical Engineering, Hebei United University;School of Mechanical Engineering, Hebei United University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

WC powder and cemented carbide blade were soaked in distilled water and sodium carbonate solution in the experiment. Influencing factors and mechanisms of WC leaching from cemented carbide were researched by SEM and EDX. The results show that both water and sodium carbonate can lead to WC leac- hing from cemented carbide,and the effect of sodium carbonate is more obvious at higher temperature. WC leaching can be attributed to the presence of such ions as H+ ,OH- and HCO3- in cutting fluid, and tungsten enters into the solution finally in the form of WO4^2- detached from the blade surface.

KeyWords AITranslate

cemented carbide cutting tools WC leaching distilled water sodium carbonate solution mechanism

1邵芳,刘战强,万熠,张宝国.基于热力学的硬质合金刀具扩散磨损[J].武汉理工大学学报,2008,30(10):113-116. 被引量:8

2王英姿,陶文宏,杨中喜,李友生.高速切削刀具的扩散磨损检测研究[J].制造技术与机床,2009(1):116-118. 被引量:5

3李俊萌.中国钨矿资源浅析[J].中国钨业,2009,24(6):9-13. 被引量:60

4张立,陈述,熊湘君,黄伯云,张传福.电化学回收WC粉末质量控制问题的探讨[J].硬质合金,2006,23(2):103-106. 被引量:13

5Anna Warren. Oxidation of tungsten and tungsten car bide in dry and humid atmosphere[J]. Lubrication Engi- neering,2006,10(9) :345-353.

6Ma Chun-an,Gan Yong-ping,Chu You-qun, et al. Elec- tro- oxidation behavior of tungsten carbideelectrode in different electrolytes[J].Trans Nonferrous Met Soc Chi- na,2004,14(1) : 11-14.

7赵中伟,曹才放,李洪桂.碳酸钠分解白钨矿的热力学分析[J].中国有色金属学报,2008,18(2):356-360. 被引量:16

1张好强,贾晓鸣,王莉娜,宋月星.线切割加工硬质合金模具的WC浸出机理及抑制研究[J].硬质合金,2012,29(2):111-115. 被引量:6

2黄悦,王珺,刘秉余.AZ31镁合金化学镀镍工艺研究[J].辽宁工业大学学报:自然科学版,2017,37(1):37-40.

3刘建华,文陈,于美,李松梅,王兵.Effect of anions on stress corrosion cracking behaviors of ultra-high strength steel 23Co14Ni12Cr3Mo[J].中南大学学报:英文版,2014,21(6):2117-2124. 被引量:1

4廖俊生,孙颖,邱绍宇,丁平,蔡定洲,盛钟琦.奥氏体不锈钢在含铀碳酸钠溶液中的腐蚀行为[J].材料保护,2004,37(9):12-14.

5吴丹,杨湘杰,叶寒.预处理工艺对AZ91D镁合金锡酸盐转化膜的影响[J].机械工程材料,2008,32(12):15-18. 被引量:1

6贾鹏,周明.Scratching and Turning Experiments on Machinability of Optical Glass SF6 in Diamond Cutting Process[J].天津大学学报:英文版,2011,17(4):280-283. 被引量:1

7王凤华.漂白用金属螯合剂DTPA的实验研究[J].齐齐哈尔大学学报:自然科学版,2006,22(1):45-45.

8梁倩倩,贾晓鸣.硬质合金刀具钴和碳化钨的浸出研究[J].硬质合金,2012,29(4):221-225. 被引量:2

9刘荣佩,左孝青,杨晓源,顾昆.泡沫金属渗流铸造工艺及填料的研究[J].昆明理工大学学报:理工版,2000,25(4):29-31. 被引量:3

10周明,贾鹏.切削液对光学玻璃SF6在金刚石切削加工中可加工性的影响(英文)[J].纳米技术与精密工程,2011,9(4):350-356. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]

Citation Information:

WC powder and cemented carbide blade were soaked in distilled water and sodium carbonate solution in the experiment. Influencing factors and mechanisms of WC leaching from cemented carbide were researched by SEM and EDX. The results show that both water and sodium carbonate can lead to WC leac- hing from cemented carbide,and the effect of sodium carbonate is more obvious at higher temperature. WC leaching can be attributed to the presence of such ions as H+ ,OH- and HCO3- in cutting fluid, and tungsten enters into the solution finally in the form of WO4^2- detached from the blade surface.

quote

GB/T 7714-2015 [1] ZHANG Hao-qiang, WANG Li-na, JIA Xiao-ming, et al. Study of WC Leaching Mechanism from Cemented Carbide Blade[J]. Rare Metals and Cemented Carbides, 2012(4): 59-62.
MLA [1] ZHANG Hao-qiang, et al., "Study of WC Leaching Mechanism from Cemented Carbide Blade." Rare Metals and Cemented Carbides, no. 4, 2012, pp. 59-62.
APA [1] ZHANG Hao-qiang, WANG Li-na, JIA Xiao-ming, & SONG Yue-xing. (2012). Study of WC Leaching Mechanism from Cemented Carbide Blade. Rare Metals and Cemented Carbides(4), 59-62.
IEEE [1] ZHANG Hao-qiang, WANG Li-na, JIA Xiao-ming, and SONG Yue-xing, "Study of WC Leaching Mechanism from Cemented Carbide Blade," Rare Metals and Cemented Carbides, no. 4, pp. 59-62, 2012. keywords: {cemented carbide cutting tools WC leaching distilled water sodium carbonate solution mechanism}