Investigation on the Production Technoligical Conditions and Quality Control of Ultrafine Niobium (Tantalum) Carbide Powder for Cemented Carbide AITranslate
Abstract AITranslate
Based on tantalum (niobium) carbide production by carbonation, production technoligical factors are analyzed of ultrafine tantalum (niobium) carbide powder for cemented carbides. Quality control key elements of the product are summarized, and specific improvement measures are suggested.
KeyWords AITranslate
1何坤池.超细碳化铌粉的研制生产[A].稀有金属冶金学会1998年年会论文集[C].石嘴山:稀有金属冶金学会,1998.131-134.
2张启修,赵秦生.钨钼冶金[M].北京:冶金工业出版社,2007.
3汤仁中.两次碳化法制取细颗粒碳化钽的工艺研究[J].稀有金属与硬质合金,2000,28(1):5-9. 被引量:5
4陈为亮,钟海云,戴永年.超细碳化物粉末的制取方法[J].稀有金属与硬质合金,1998,26(4):36-41. 被引量:9
5曹茂盛.纳米材料导论[M].哈尔滨:哈尔滨工业大学出版社,2004.
6张浩,朱芳.钽、铌碳化物制备技术的研究进展[J].稀有金属与硬质合金,2009,37(2):47-49. 被引量:8
1杨家富,陈伟鹏,赵增武,郑坤灿,庞雅丹,赵光进.真空碳热还原制备碳化钛和碳化铌粉体的研究[J].稀有金属与硬质合金,2020,48(4):28-32. 被引量:1
1崔健,张国华.高纯超细碳化钛粉体制备[J].江西冶金,2023,43(4):265-272.
1何旭初,范鹏,周渝生,杨天钧,董一诚.高炉中铌还原产生的碳化铌滞留带[J].北京科技大学学报,1990,12(6):504-509. 被引量:7
2任先廷,李威,郭智峰.碳化法生产拟薄水铝石工业实践[J].有色金属:冶炼部分,2005(5):39-40. 被引量:4
3章桥新,张东明.NbC粉末的机械合金化合成[J].中国有色金属学报,1995,5(1):87-89. 被引量:7
4方磊,丁松,黄桂斌,刘宏亮,刘承军.铌在高碳钢凝固过程中行为特性的模型分析[J].工业加热,2007,36(6):36-38. 被引量:1
5张新宝.大型钢锭中碳化铌的形成及固溶行为[J].上海钢研,2005(1):53-53.
6何坤池.间接碳还原法生产铌时原料粒度对还原周期的影响[J].稀有金属与硬质合金,1998,26(4):6-10.
7张波,李春龙,姜茂发.熔分过程中铌、磷在渣铁两相间的分配比[J].东北大学学报:自然科学版,2014,35(7):983-986. 被引量:4
8黄新,孙亚丽,颜杰,唐凯,刘清才,何宪峰,李伟.两步碳化法生产优质粗颗粒WC粉末[J].中国钨业,2007,22(6):39-42. 被引量:4
9章桥新,张东明.机械合金化制备金属铌的难熔化合物[J].无机材料学报,1995,10(2):253-256. 被引量:1
10周永贵,胡乐中.一步碳化法生产优质(W、Ti)C固溶体[J].硬质合金,1998,15(1):25-27. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF123.72[冶金工程—粉末冶金]
Citation Information:
Based on tantalum (niobium) carbide production by carbonation, production technoligical factors are analyzed of ultrafine tantalum (niobium) carbide powder for cemented carbides. Quality control key elements of the product are summarized, and specific improvement measures are suggested.
quote
| GB/T 7714-2015 | [1] LIANG Chang-ming. Investigation on the Production Technoligical Conditions and Quality Control of Ultrafine Niobium (Tantalum) Carbide Powder for Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2012(4): 63-67. |
| MLA | [1] LIANG Chang-ming. "Investigation on the Production Technoligical Conditions and Quality Control of Ultrafine Niobium (Tantalum) Carbide Powder for Cemented Carbide." Rare Metals and Cemented Carbides, no. 4, 2012, pp. 63-67. |
| APA | [1] LIANG Chang-ming. (2012). Investigation on the Production Technoligical Conditions and Quality Control of Ultrafine Niobium (Tantalum) Carbide Powder for Cemented Carbide. Rare Metals and Cemented Carbides(4), 63-67. |
| IEEE | [1] LIANG Chang-ming, "Investigation on the Production Technoligical Conditions and Quality Control of Ultrafine Niobium (Tantalum) Carbide Powder for Cemented Carbide," Rare Metals and Cemented Carbides, no. 4, pp. 63-67, 2012. keywords: {tantalum (niobium) carbide ultrafine powder;production process;quality control} |