Microwave Radiation Synthesis and Characterization of Silver Nanoparticles AITranslate
Abstract AITranslate
Silver nanoparticles with an average diameter of 30 nm were prepared by microwave radiation, with silver nitrate as the silver source,hexamine as the reducer and polyvinylpyrrolidone as the surfactant and stabilizer. Crystal structure and morphology of the samples were characterized by XRD and TEM. The structure of the samples was qualitatively analyzed by IR spectra, and the optical properties were studied by UV-Vis spectrophotometer. The results show that the above method is simple and fast, and the prepared silver nanoparticles are pure cubic polyerystal with small size, narrow particle size distribution and good dispersibility.
KeyWords AITranslate
1Slocik J M, Wright D W. Biomimetic mineralization of noble metal nanoclusters[J].Biomacromolecules, 2003,4 (5) ..1 135-1 141.
2E1-Sayed M A. Some interesting properties of metals confined intime and nanometer space of different shapes [J].Accounts of Chemical Research, 2001,34 (4) : 257- 264.
3Ruslan Z V. Structure and mechanical properties of ul- trafine-grained metals[J]. Matel Sci Eng(A), 1997,234- 236 : 50-66.
4Omer M,Ahmed E, Leong W K, et al. Colloidal silver nanoparticles stailized by a water- soluble triosmium cluster[J]. Journal of Organometallic Chemistry, 2006, 691(5) :1 055-1 060.
5刘春华,杨秀培,吴莉宇,肖丹.纳米银胶体粒子的制备及对牛血清蛋白的检测[J].化学研究与应用,2008,20(6):786-789. 被引量:5
6Liu C H,Zhou Z D,Yu X,et al. Preparation and characterization of Fe304/Ag composite magnetic nanoparticles [J]. Inorganic Materials, 2008,44 (1) .. 1-5.
7顾大明,高农,程谨宁.次磷酸盐液相还原法快速制备纳米银粉[J].精细化工,2002,19(11):634-635. 被引量:33
8Xiong Y J,Washio I,Chen J Y,et al. Poly(vinyl pyrroli done):a dual functional reductant and stabilizer for the facile synthesis of noble metal nanoplates in aqueous so- lutions[J]. Langmuir,2006,22(20):8 563-8 570.
9郭宏,杨慧萍.制备纳米银的液相还原法的条件优化研究[J].环境与健康杂志,2008,25(6):536-538. 被引量:8
10郭斌,唐永建,罗江山,程建平.双还原剂法制备的三角形银纳米盘的吸收和发射光谱研究[J].贵金属,2008,29(2):5-10. 被引量:16
1樊新,黄可龙,刘素琴,于金刚,尹良果.化学还原法制备纳米银粒子及其表征[J].功能材料,2007,38(6):996-999. 被引量:44
2林峰,苏伟,许利剑,汤建新.纳米银粒子在微乳液中的制备及其抗菌性能[J].包装学报,2010,2(1):28-32. 被引量:7
3段学臣,贺玮,朱磊.超细铜粉的新型电沉积制备及表征[J].粉末冶金材料科学与工程,2009,14(3):169-173. 被引量:9
4柳旭,王鑫,彭家庆,王力军,陈松,吴延科,陈洋.氯铪酸钾的制备及表征[J].稀有金属材料与工程,2014,43(2):450-454. 被引量:2
5刘秀然,余高奇,王玲.超细氧化钴粉体的制备及表征[J].贵州大学学报:自然科学版,2001,18(3):194-195. 被引量:6
6林健凉,王零森,尹邦跃,杨勇,李笃信.ZrO_2纳米复合粉末的制备及表征[J].硬质合金,2000,17(1):13-17. 被引量:15
7闫晋钢,赵杰,艾勇,史知奇.氧化铝生产中物料的红外光谱分析研究[J].轻金属,2001(2):14-17. 被引量:7
8李先学,韩跃新,印万忠.纳米银粉制备过程中表面保护剂的作用研究[J].矿冶,2004,13(3):51-53. 被引量:7
9谭帼馨,谭英,宁成云,周蕾,黄俊鹏,何天瑞,王航,廖景文,陈晓峰.多孔钛表面聚多巴胺层修饰及其载银研究[J].稀有金属材料与工程,2015,44(5):1234-1238. 被引量:2
10汪峰涛,吴玉程,王涂根,任榕.W-Cu纳米晶粉体的制备及表征[J].功能材料,2007,38(A06):2062-2065. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF123.72[冶金工程—粉末冶金]
Citation Information:
Silver nanoparticles with an average diameter of 30 nm were prepared by microwave radiation, with silver nitrate as the silver source,hexamine as the reducer and polyvinylpyrrolidone as the surfactant and stabilizer. Crystal structure and morphology of the samples were characterized by XRD and TEM. The structure of the samples was qualitatively analyzed by IR spectra, and the optical properties were studied by UV-Vis spectrophotometer. The results show that the above method is simple and fast, and the prepared silver nanoparticles are pure cubic polyerystal with small size, narrow particle size distribution and good dispersibility.
quote
| GB/T 7714-2015 | [1] CHAI Duo-li, ZHANG Meng-ru, YUAN Xin-song, et al. Microwave Radiation Synthesis and Characterization of Silver Nanoparticles[J]. Rare Metals and Cemented Carbides, 2012(4): 68-72. |
| MLA | [1] CHAI Duo-li, et al., "Microwave Radiation Synthesis and Characterization of Silver Nanoparticles." Rare Metals and Cemented Carbides, no. 4, 2012, pp. 68-72. |
| APA | [1] CHAI Duo-li, ZHANG Meng-ru, YUAN Xin-song, CHEN Xin-hua, & YANG Shao-dong. (2012). Microwave Radiation Synthesis and Characterization of Silver Nanoparticles. Rare Metals and Cemented Carbides(4), 68-72. |
| IEEE | [1] CHAI Duo-li, ZHANG Meng-ru, YUAN Xin-song, CHEN Xin-hua, and YANG Shao-dong, "Microwave Radiation Synthesis and Characterization of Silver Nanoparticles," Rare Metals and Cemented Carbides, no. 4, pp. 68-72, 2012. keywords: {silver nanopartiele hexamine polyvinylpyrrolidone microwave radiation} |