daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Molybdenum-containing Wastewater Treatment Effect of Fly Ash and its Adsorption Mechanism AITranslate

Chinese University of Mining and Technology University of Mining and Technology;Chinese University of Mining and Technology University of Mining and Technology;Chinese University of Mining and Technology University of Mining and Technology;Chinese University of Mining and Technology University of Mining and Technology;Chinese University of Mining and Technology University of Mining and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Molybdenum removal experiments of simulated molybdenum-containing wastewater were carried out with fly ash as the absorbent. Influences of absorption pH and absorbent dosage on adsorption results were studied, and the adsorption isotherm equation and kinetics were discussed. The results show that the adsorption effect of fly ash for molybdenum is best with a molybdenum removal rate of 74.3 %, under the conditions of molybdenum initial concentration 10 mg/L and pH=8.1. The addtion of 2.5 g absorbent into 50 mL molybdenum-containing solution resultes in optium molybdenum removal up to 85.4%. Molybdenum adsorption on fly ash conforms with Langmuir adsorption isotherm equation, dominated by surface single-molecule layer adsorption. The adsorption kinetic data are fitted with second-order kinetic model, representing the characteristics of both physical adsorption and chemisorption.

KeyWords AITranslate

fly ash molybdenum removal adsorption adsorption isotherm equation secondorder kinetic model

1傅金祥,王作鹏,张雷,韩宇翔.钼污染饮用水的PAC吸附工艺[J].沈阳建筑大学学报:自然科学版,2009,25(5):954-958. 被引量:4

2练建军,许士国,于常武,韩成伟.重金属钼的迁移特性及人工湿地处理研究[J].环境保护科学,2010,36(6):7-10. 被引量:8

3李志鹏,任瑞晨,常志达.粉煤灰合成沸石方法与应用现状[J].辽宁工程技术大学学报:自然科学版,2009,28(A02):111-113. 被引量:4

4黄琴,吉伟英,陈端伟.改性粉煤灰在废水处理中的应用进展[J].上海应用技术学院学报:自然科学版,2008,8(1):71-75. 被引量:11

5鲁景,李多松.粉煤灰在重金属废水处理中的应用[J].资源开发与市场,2007,23(2):166-167. 被引量:12

6张明亮.粉煤灰对煤矸石酸性重金属淋滤液的修复作用[J].煤炭学报,2011,36(4):654-658. 被引量:21

7相会强,智艳生.改性粉煤灰在抗生素废水除磷脱色中的应用[J].中国非金属矿工业导刊,2005(3):44-47. 被引量:2

8林俊雄,詹树林,方明晖,吕大丰,杨建秀.三种吸附剂的改性与染料吸附特性比较研究[J].浙江大学学报:工学版,2006,40(12):2031-2036. 被引量:15

9沈王庆,兰子平,罗来辉,卓敏.粉煤灰吸附城市生活污水中磷的动力学研究[J].内江师范学院学报,2009,24(12):49-51. 被引量:3

10Lin J X,Zhan S L. Adsorption of basic dyes from aqueous solution onto fly ash[J]. J Environ Manage, 2007, 87( 1 ) : 193-200.

1陈昆昆,马光,孟晗琪,王治钧,王靖坤,吴永谦.D296树脂从含钼酸性溶液中吸附钼的试验研究[J].中国钼业,2014,38(2):47-50. 被引量:8

2贾艳萍,姜成,张羽汐,殷爱鸣,刘彬.粉煤灰的特性及其去除水中重金属的研究进展[J].硅酸盐通报,2015,34(7):1896-1902. 被引量:8

3钱冬旭,张亚雷,周雪飞,代朝猛,钱雅洁,苏益明.钼污染水体处理技术研究进展[J].化工进展,2016,35(2):617-623. 被引量:5

4李静,李鸿达,宋蕾,邢丽.微生物絮凝剂与粉煤灰联合处理水中Pb^(2+)的响应面优化[J].材料保护,2017,50(5):105-109. 被引量:1

5杨雨桐,于欣平,刘桂萍.酸改性轻烧镁/粉煤灰对染料的吸附特性[J].非金属矿,2018,41(1):76-79. 被引量:3

6李梦阳,张亚雷,沈峥,张勇.含钼废水处理技术及其机理研究进展[J].环境污染与防治,2019,41(1):106-109. 被引量:6

7王剑峰,张金利,杨庆.粉煤灰对Cr(Ⅵ)的吸附特性[J].环境工程学报,2014,8(11):4593-4599. 被引量:14

1于波,于洪翠,宋邦雄,齐瑞雪.粉煤灰对硝基苯的吸附:动力学和热力学研究[J].环境科学与技术,2020(S01):11-16. 被引量:2

2陈昆昆,吴贤,王治钧.D296树脂从含铼酸性溶液中吸附铼的研究[J].有色金属:冶炼部分,2015(7):43-46. 被引量:20

3贾艳萍,姜成,张羽汐,殷爱鸣,刘彬.粉煤灰的特性及其去除水中重金属的研究进展[J].硅酸盐通报,2015,34(7):1896-1902. 被引量:8

4吴永谦,吴贤,陈昆昆,张卜升,郭瑞,马光.高温合金酸浸渣氧化焙烧—碱浸工艺研究[J].有色金属:冶炼部分,2015(8):43-45.

5张龙强,申颖颖,张平,赵秋菊,安立超.钢渣固定床对水中Pb(Ⅱ)和Cd(Ⅱ)的吸附研究[J].环境工程,2016,34(1):25-30. 被引量:2

6钱冬旭,张亚雷,周雪飞,代朝猛,钱雅洁,苏益明.钼污染水体处理技术研究进展[J].化工进展,2016,35(2):617-623. 被引量:5

7李银,刘瑜,李昌乐.含水层介质对Cr(VI)的吸附特征[J].环境工程学报,2016,10(4):2071-2076. 被引量:1

8常云龙,刘洋,邓丽,宋增意,刘丹.NH_4SCN解吸剂对负载Re的D296树脂的解吸影响[J].沈阳工业大学学报,2016,38(3):263-267. 被引量:1

9高玉红,魏蕊娣,任立伟.改性粉煤灰吸附处理含铜废水的试验研究[J].粉煤灰综合利用,2016,30(2):18-20. 被引量:4

10邬欣慧,陈春强,马东,陈钇汀,孙玉颖.水热改性竹叶对水中Cr(Ⅵ)的吸附性能[J].环境工程学报,2016,10(6):2915-2920. 被引量:1

1朱慧,吴双桃.凤眼莲干粉对水中Sb^(3+)的吸附特性初探[J].工业安全与环保,2013,39(7):1-3.

2车荣睿.离子交换法在治理含钼废水中的应用[J].离子交换与吸附,1994,10(2):180-184. 被引量:8

3刘迪,于常武,刘刚,赵靖雨,魏明,杨帅.脱水污泥吸附去除废水中钼污染物的研究[J].辽宁化工,2014,43(8):977-979. 被引量:2

4张凤,王慢慢,杨文娟,马晓艳,周娅芬.壳聚糖交联天然沸石用于水溶液中亚甲基蓝的吸附研究[J].四川师范大学学报:自然科学版,2014,37(6):893-898. 被引量:2

5于常武,高超.丝藻对含钼废水中MoO_4^(2-)的吸附特性及机制研究[J].环境污染与防治,2015,37(7):55-60. 被引量:7

6王强,王银叶,荆立坤,张晓艳.天然沸石处理电镀废水中镍吸附特性的研究[J].天津城市建设学院学报,2008,14(3):201-203. 被引量:2

7金瑜,张红健.化丝废水中钼的回收利用[J].环境科技,2010,23(4):51-53.

8赵彩荣,范文元.乳化液膜法提取钼的研究[J].水处理技术,2002,28(6):320-322. 被引量:6

9于常武,高超,王琳.腐殖质吸附重金属钼(MoO_4^(2-))的性能研究[J].环境工程,2015,33(6):10-14. 被引量:2

10廖秋玲,高竹青.离子交换法从烟道灰中提取铼的工艺研究[J].中国资源综合利用,2011,29(12):18-21. 被引量:6

Basic Information:

DOI:

Chinese Library Classification Number:X703.5[环境科学与工程—环境工程]

Citation Information:

Molybdenum removal experiments of simulated molybdenum-containing wastewater were carried out with fly ash as the absorbent. Influences of absorption pH and absorbent dosage on adsorption results were studied, and the adsorption isotherm equation and kinetics were discussed. The results show that the adsorption effect of fly ash for molybdenum is best with a molybdenum removal rate of 74.3 %, under the conditions of molybdenum initial concentration 10 mg/L and pH=8.1. The addtion of 2.5 g absorbent into 50 mL molybdenum-containing solution resultes in optium molybdenum removal up to 85.4%. Molybdenum adsorption on fly ash conforms with Langmuir adsorption isotherm equation, dominated by surface single-molecule layer adsorption. The adsorption kinetic data are fitted with second-order kinetic model, representing the characteristics of both physical adsorption and chemisorption.

quote

GB/T 7714-2015 [1] JIA Han-shuai, LIU Han-hu, YU Chang-wu, et al. Molybdenum-containing Wastewater Treatment Effect of Fly Ash and its Adsorption Mechanism[J]. Rare Metals and Cemented Carbides, 2012(4): 73-76.
MLA [1] JIA Han-shuai, et al., "Molybdenum-containing Wastewater Treatment Effect of Fly Ash and its Adsorption Mechanism." Rare Metals and Cemented Carbides, no. 4, 2012, pp. 73-76.
APA [1] JIA Han-shuai, LIU Han-hu, YU Chang-wu, HU Shu, & ZHOU Jiang. (2012). Molybdenum-containing Wastewater Treatment Effect of Fly Ash and its Adsorption Mechanism. Rare Metals and Cemented Carbides(4), 73-76.
IEEE [1] JIA Han-shuai, LIU Han-hu, YU Chang-wu, HU Shu, and ZHOU Jiang, "Molybdenum-containing Wastewater Treatment Effect of Fly Ash and its Adsorption Mechanism," Rare Metals and Cemented Carbides, no. 4, pp. 73-76, 2012. keywords: {fly ash;molybdenum removal;adsorption;adsorption isotherm equation;secondorder kinetic model}