Analysis of the Impact Factors on the Hardness and Strength of Coarse-grained Cemented Carbide AITranslate
Abstract AITranslate
Influences of technological factors and their interaction on the hardness and transverse rupture strength of coarse-grained cemented carbide were investigated by variable search method, and the factors includes alloy carbon content,sintering process, cobalt content, binder phase composition, ball to powder ratio and milling time. The results show that cobalt content and milling time are the main impact factors of hardness, while sintering process,ball milling process and binder phase composition mainly influence alloy strength. The coarse-grained cemented carbide with fewer defects, more uniform binder phase distribution and higher strength can be obtained by appropriately increasing sintering temperature.
KeyWords AITranslate
1张忠健,汪晓,李仁琼,胡茂中.中国硬质合金产业的技术进步[J].硬质合金,2007,24(1):33-38. 被引量:22
2周建华,卢伟民.国内外硬质合金生产现状及近期发展动向分析[J].稀有金属与硬质合金,2006,34(1):36-41. 被引量:25
3林晨光.中国超细和纳米晶WC-Co硬质合金的研究开发概况[J].中国钨业,2005,20(2):19-23. 被引量:27
4李勇,谢淑华.WC粗晶硬质合金的研究进展[J].材料研究与应用,2009,3(2):77-80. 被引量:12
5姚珍芝.质量认证讲座 第六部分 美国道林·夏宁(D.Shainin)实验设计方法(D.O.E)介绍[J].低压电器,1998(6):56-60. 被引量:4
6姚珍芝.美国道林·夏宁(D.Shainin)实验设计方法(D.O.E)介绍(续)[J].低压电器,1999(1):52-56. 被引量:1
7何宪峰,石建华.优质粗晶WC碳化工艺研究[J].稀有金属快报,2005,24(10):28-35. 被引量:23
8Anil Kumar,Sugarland. High-strength tungsten carbide material for use in earth-boring bits [P]. US Pat: 5281260,1994-01-25.
9周新华,王力民,赵声志,肖可俊.碳含量对粗晶硬质合金性能的影响[J].硬质合金,2009,26(2):82-86. 被引量:13
10郭圣达,羊建高,陈颢.粗晶粒WC-Co类硬质合金研究现状[J].粉末冶金工业,2011,21(4):58-63. 被引量:17
1邓四文.相同硬度的高钴和低钴含量硬质合金性能比较[J].理化检验:物理分册,2022,58(6):21-25.
2王进军.超细晶WC-Co硬质合金制备技术的研究[J].稀有金属与硬质合金,2015,43(2):50-53. 被引量:3
3杨胜,顾金宝,廖军,陈洪霞.烧结压力对WC-12%Co粗晶硬质合金组织及性能的影响[J].稀有金属与硬质合金,2015,43(2):54-58.
4罗桂甫,吴建国.粗晶硬质合金的研究进展[J].硬质合金,2013,30(1):46-52. 被引量:13
5谭征.粗晶WC-Co类硬质合金的工艺研究进展[J].中国锰业,2013,31(3):47-49. 被引量:2
6毛善文.硬质合金抗弯强度影响因素的统计研究[J].硬质合金,2013,30(4):197-203. 被引量:10
7郭圣达,吕健,陈颢,羊建高,钟明龙,朱二涛.非均匀结构硬质合金的研究现状及发展趋势[J].稀有金属与硬质合金,2013,41(6):67-69. 被引量:14
8江丙武,蔡海燕,宋耀强,赵东,阳进,黄蕊,杜秋容.国内外路面铣刨刀具用硬质合金的现状与发展趋势[J].硬质合金,2014,31(3):194-200. 被引量:1
9严维,王水龙,郭圣达,郭建锋,黄星,陈颢,李律达,曹赛鹏.Mo添加对WC-6Co硬质合金组织性能的影响[J].稀有金属与硬质合金,2020,48(4):73-78. 被引量:3
10秦琴,王楠,颜子镒,田金欣,唐诗佳,杨昊栋,黄泰博.WC粗晶硬质合金摩擦性能影响因素分析[J].稀有金属与硬质合金,2021,49(5):82-86. 被引量:2
1郑清宏,刘江,时凯华,黄伟.粗细WC晶粒配比对双晶结构硬质合金力学性能与组织结构的影响[J].稀有金属与硬质合金,2020(1):75-79. 被引量:4
2杨胜,顾金宝,廖军,陈洪霞.烧结压力对WC-12%Co粗晶硬质合金组织及性能的影响[J].稀有金属与硬质合金,2015,43(2):54-58.
3江丙武,蔡海燕,宋耀强,赵东,阳进,黄蕊,杜秋容.国内外路面铣刨刀具用硬质合金的现状与发展趋势[J].硬质合金,2014,31(3):194-200. 被引量:1
4张卫兵,刘向中,陈振华,陈鼎,彭程.WC-Co硬质合金最新进展[J].稀有金属,2015,39(2):178-186. 被引量:63
5朱国丽,何清勇,唐琛,王权,张平,乔娇.WC-10%Co非均匀结构细晶合金的研究[J].硬质合金,2015,32(2):88-94. 被引量:5
6龙坚战,陆必志,易茂中,陈飞.新型粘结相硬质合金的研究进展[J].硬质合金,2015,32(3):204-212. 被引量:26
7金鹏,彭文.硬质合金导热系数的研究[J].硬质合金,2015,32(5):300-305. 被引量:8
8张颢,孔德方,朱婷,钟耿,张卫兵.网状基体和核心的特征对网状结构硬质合金抗弯强度的影响[J].硬质合金,2015,32(5):306-310. 被引量:5
9郭娟,李军民.新型硬质合金刀具材料的组织与性能分析[J].工具技术,2016,50(2):63-66.
10张岩,王洪福,何泠,王海鹏,罗伟,王俊元.WC-Co截齿的材料成分及硬度分析[J].热加工工艺,2017,46(2):109-112. 被引量:2
1张正富,彭金辉,郭圣达,李芳,袁明健,张华明.粗晶WC-Co硬质合金强度和密度影响因素的变量搜索试验研究[J].粉末冶金技术,2011,29(4):243-249. 被引量:5
2占志泽.浅谈提高我厂硬质合金强度之途径[J].江西冶金,1997,17(3):19-21.
3杨胜,顾金宝,廖军,陈洪霞.烧结压力对WC-12%Co粗晶硬质合金组织及性能的影响[J].稀有金属与硬质合金,2015,43(2):54-58.
4吴迪,熊志翔,白英龙,果世驹,杨霞,徐红霞.铸造碳化钨反应烧结制备粗晶硬质合金[J].粉末冶金材料科学与工程,2011,16(4):471-477. 被引量:3
5聂洪波.超粗晶WC-Co硬质合金的制备方法与机理及性能研究[J].中国钨业,2016,31(4):51-57. 被引量:10
6陈洪霞,薛林,顾金宝,杨胜,袁明健.烧结工艺对粗晶硬质合金微观组织及性能的影响[J].稀有金属与硬质合金,2015,43(5):64-67 71. 被引量:2
7李勇,谢淑华.WC粗晶硬质合金的研究进展[J].材料研究与应用,2009,3(2):77-80. 被引量:12
8程鑫,张立.热处理对粗晶WC-Co硬质合金力学性能的影响[J].稀有金属与硬质合金,2012,40(2):45-47. 被引量:8
9陈芃,李海坤.硬质合金高温处理回收工艺研究[J].硬质合金,2001,18(4):201-203. 被引量:13
10马鋆,张立,南晴,解明伟,冯于平,雷霆.Cr、V、Ta添加剂对超粗晶和特粗晶硬质合金电化学腐蚀行为的影响[J].粉末冶金材料科学与工程,2012,17(6):825-832. 被引量:16
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]
Citation Information:
Influences of technological factors and their interaction on the hardness and transverse rupture strength of coarse-grained cemented carbide were investigated by variable search method, and the factors includes alloy carbon content,sintering process, cobalt content, binder phase composition, ball to powder ratio and milling time. The results show that cobalt content and milling time are the main impact factors of hardness, while sintering process,ball milling process and binder phase composition mainly influence alloy strength. The coarse-grained cemented carbide with fewer defects, more uniform binder phase distribution and higher strength can be obtained by appropriately increasing sintering temperature.
quote
| GB/T 7714-2015 | [1] GUO Sheng-da, YANG Jian-gao, HUANG Hai-ping, et al. Analysis of the Impact Factors on the Hardness and Strength of Coarse-grained Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2012(4): 56-58. |
| MLA | [1] GUO Sheng-da, et al., "Analysis of the Impact Factors on the Hardness and Strength of Coarse-grained Cemented Carbide." Rare Metals and Cemented Carbides, no. 4, 2012, pp. 56-58. |
| APA | [1] GUO Sheng-da, YANG Jian-gao, HUANG Hai-ping, XU Fang, HU Yong-mei, & ZHENG Biao-hua. (2012). Analysis of the Impact Factors on the Hardness and Strength of Coarse-grained Cemented Carbide. Rare Metals and Cemented Carbides(4), 56-58. |
| IEEE | [1] GUO Sheng-da, YANG Jian-gao, HUANG Hai-ping, XU Fang, HU Yong-mei, and ZHENG Biao-hua, "Analysis of the Impact Factors on the Hardness and Strength of Coarse-grained Cemented Carbide," Rare Metals and Cemented Carbides, no. 4, pp. 56-58, 2012. keywords: {coarse-grained cemented carbide;hardness;transverse rupture strength;impact factor;variable search} |