Research on Micromorphology and Performance of TiAlN Coating and TiAlSiN Coating on Zirconium Alloy Surface AITranslate
Abstract AITranslate
TiAlSiN coating and TiAlN coating were deposited on Zr-4 alloy surface by multi-arc ion plating,respectively.Surface micromorphology of the coatings were observed by scanning electron microscope.Statistics and analysis of the large particle distribution of the coatings were carried out by ImageJ.The phase composition of the coatings was analyzed by X-ray diffractometer.The mechanical properties of the coatings were tested by an automatic scratch tester.And the samples were subjected to 800℃ high temperature oxidation resistance test in a high temperature heat treatment furnace.The results show that the amount of large particles on the surface of TiAlSiN coating is less than that of TiAlN coating.Both TiAlSiN coating and TiAlN coating have Ti2N phase and Ti3AlN phase.In addition,TiAlSiN coating also has AlN phase and Si3N4 amorphous phase.Because the addition of Si elements leads to residual stress,TiAlSiN coating has lower coating/substrate adhesion strength than TiAlN coating.Oxidation weight gain of TiAlSiN coating sample is far lower than that of TiAlN coating sample.
KeyWords AITranslate
1张聪惠,刘大利,兰新哲,赵西成.锆合金氧化膜对腐蚀性能影响研究现状[J].热加工工艺,2011,40(16):117-120. 被引量:10
2范清松,杨忠波,赵文金,陈善华.Sn和Nb对Zr-Sn-Nb-Fe锆合金中第二相粒子的影响[J].热加工工艺,2014,43(22):1-4. 被引量:6
3吴华,范洪远,应诗浩,黄新泉.表面处理对锆合金性能的影响[J].金属热处理,2006,31(1):17-19. 被引量:23
4罗扬,林庆选.锆合金R60705的表面渗氮处理[J].金属热处理,2014,39(12):64-66. 被引量:10
5张立杰,范洪远,应诗浩,李聪.锆合金氧化膜研究进展[J].材料导报,2006,20(F11):422-424. 被引量:8
6王浩然,邱长军.锆合金表面技术的研究进展[J].世界有色金属,2016,0(9):46-47. 被引量:8
7胡汝骞,樊湘芳,丰振东,龚仁政,夏炎.Zr4合金离子氮化和软氮化表面处理的研究[J].热加工工艺,2016,45(14):130-132. 被引量:5
8陈昌浩,金永中,陈建,龙国俊,余学金,蔡瑜.弧电流对多弧离子镀TiN涂层形貌及力学性能的影响[J].热加工工艺,2016,45(14):117-119. 被引量:7
9朱鹏志,朱颖,李刘合.TiAlSiN涂层刀具的发展与应用[J].新技术新工艺,2014(5):105-110. 被引量:15
10杨昌虎,马忠权,袁剑辉.基底温度对直流磁控溅射制备掺铝氧化锌薄膜性能的影响[J].光学学报,2011,31(5):254-260. 被引量:12
1周军,樊湘芳,李涛,邱长军,李怀林.弧电流对多弧离子镀TiAlN涂层表面形貌和性能的影响[J].材料保护,2018,51(6):74-78. 被引量:3
2李涛,樊湘芳,邱长军,杨振,刘艳红,王晓婧.锆管表面Cr/TiAlSiN涂层的高温抗氧化性能[J].材料保护,2019,0(6):138-142. 被引量:2
3杨振,樊湘芳,邱长军,李涛,刘艳红,王晓婧,李怀林.锆合金表面涂层耐高温高压动水腐蚀性能的研究[J].表面技术,2019,48(9):204-210. 被引量:3
4林云根,魏宇惠,王谦之.硬质合金表面TiAlN涂层在不同切削液中的摩擦腐蚀性能[J].材料保护,2019,52(11):1-7.
5朱锦云,樊湘芳,杨振,李涛,杜成明.0Cr15Ni5Cu2Ti钢表面多弧离子镀TiAlSiN涂层的性能研究[J].真空科学与技术学报,2020,40(3):198-202. 被引量:2
6罗伟,潘东,王宇,曾波,覃炳朝,王均.磁控溅射TiAlN和TiAlSiN对Zr-Fe-Cr合金600℃腐蚀性能的影响[J].四川冶金,2020,42(5):10-14.
7赵磊,梁启超,刘传龙,王天国.不同负偏压下多弧离子镀TiAlN薄膜的微观结构与耐腐蚀性研究[J].材料保护,2022,55(10):118-122.
8杨振,樊湘芳,邱长军,李涛,刘艳红,王晓婧.锆合金表面镀Cr/TiAlN涂层的抗高温水蒸气氧化性能研究[J].真空科学与技术学报,2019,39(2):145-149. 被引量:4
1王梦超,王丽君,陈辉.U71Mn钢轨铣削用PVD-TiAlN涂层刀片失效分析[J].表面技术,2020,49(3):300-308. 被引量:1
2方波,张林,蔡飞,张世宏.冷作模具钢等离子渗镀CrVN复合涂层摩擦磨损性能研究[J].真空,2020,57(2):33-39. 被引量:2
3张而耕,黄彪,陈强,周琼,李朝明,潘文高,林荣川,陈刚.微纳米超硬TiAlSiN涂层的研究与应用进展[J].应用技术学报,2020,20(2):118-125. 被引量:2
4罗伟,潘东,王宇,曾波,覃炳朝,王均.磁控溅射TiAlN和TiAlSiN对Zr-Fe-Cr合金600℃腐蚀性能的影响[J].四川冶金,2020,42(5):10-14.
5吴浩龙,王天国.氮氩比对模具钢表面镀TiAlN薄膜形貌和性能的影响[J].材料保护,2020,53(8):43-47. 被引量:2
6彭二宝,马骁.电压对刀具用42CrMo钢离子镀TiAlSiN涂层组织及耐磨性能的影响[J].材料保护,2021,54(2):93-97. 被引量:1
7苗利静,江柯敏,段北晨,孟凡平,卢焕明.X射线光电子能谱和聚焦离子束法研究FeCrAl合金元素含量对涂层抗氧化行为的影响[J].分析测试技术与仪器,2021,27(3):174-181.
8朱锦云,樊湘芳,杜成明.0Cr15Ni5Cu2Ti钢表面2种气体氮化层的性能研究[J].材料保护,2021,54(11):35-38. 被引量:1
9黄贞普,陈勇,赵英泽.锆合金包壳表面抗氧化涂层研究进展[J].机械工程师,2022(4):38-40.
10刘张慧,胡海洋,王建刚,祝晓烨,马静,李建辉,于会超,冯志浩.锆合金表面改性工艺的研究进展[J].金属热处理,2022,47(12):258-268.
1董卫萍,柳琪,王进,马大衍.热作模具钢CrTiAlSiN多元复合涂层的工业制备及性能研究[J].模具制造,2018,18(1):86-89. 被引量:2
2张文,邱长军,曾小安,王浩然,王晓婧,刘艳红,李怀林.表面镀Cr膜锆合金的抗高温氧化性能研究[J].稀有金属与硬质合金,2017,45(6):71-75. 被引量:5
3周军,樊湘芳,丰振东,胡汝骞.渗氮处理对Zr4合金表面TiAlSiN涂层性能的影响[J].金属热处理,2018,43(1):142-146. 被引量:2
4翟云霄,古一,黄璜,赵培新,黄继武,夏长清.Ta-10W/Ti的高温界面反应研究[J].材料导报,2016,30(24):103-107. 被引量:3
5刘益民,张利祥,李俊.哈氏合金HR-120制造800℃高温风机的试验研究[J].宝钢技术,2017,10(6):49-52. 被引量:1
6赵林科,李小宁,岳强,徐滨,王晨阳.Zr-4合金板材微观组织异常条线现象的研究[J].钛工业进展,2018,35(1):42-46.
7刘金钏,袁尔东,严慧玲,任娇艳.改良的亚油酸-硫氰酸钾显色法在抗氧化实验教学中的应用[J].科教导刊,2017(12):129-130.
8孙伟,宫秀敏,叶卫平,张覃铁,朱小清.三种材料多弧离子镀TiN涂层性能比较[J].电加工与模具,2000(1):31-33. 被引量:3
9Anying WANG,Shuai YAN,Bin LIN,Xiaofeng ZHANG,Xiaoxue ZHOU.Aqueous lubrication and surface microstructures of engineering polymer materials (PEEK and PI) when sliding against Si3N4[J].摩擦:英文版,2017,5(4):414-428. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TG146.414[金属学及工艺—金属材料]
Citation Information:
TiAlSiN coating and TiAlN coating were deposited on Zr-4 alloy surface by multi-arc ion plating,respectively.Surface micromorphology of the coatings were observed by scanning electron microscope.Statistics and analysis of the large particle distribution of the coatings were carried out by ImageJ.The phase composition of the coatings was analyzed by X-ray diffractometer.The mechanical properties of the coatings were tested by an automatic scratch tester.And the samples were subjected to 800℃ high temperature oxidation resistance test in a high temperature heat treatment furnace.The results show that the amount of large particles on the surface of TiAlSiN coating is less than that of TiAlN coating.Both TiAlSiN coating and TiAlN coating have Ti2N phase and Ti3AlN phase.In addition,TiAlSiN coating also has AlN phase and Si3N4 amorphous phase.Because the addition of Si elements leads to residual stress,TiAlSiN coating has lower coating/substrate adhesion strength than TiAlN coating.Oxidation weight gain of TiAlSiN coating sample is far lower than that of TiAlN coating sample.
quote
| GB/T 7714-2015 | [1] ZHOU Jun, FAN Xiang-fang, FENG Zhen-dong, et al. Research on Micromorphology and Performance of TiAlN Coating and TiAlSiN Coating on Zirconium Alloy Surface[J]. Rare Metals and Cemented Carbides, 2017(6): 66-70. |
| MLA | [1] ZHOU Jun, et al., "Research on Micromorphology and Performance of TiAlN Coating and TiAlSiN Coating on Zirconium Alloy Surface." Rare Metals and Cemented Carbides, no. 6, 2017, pp. 66-70. |
| APA | [1] ZHOU Jun, FAN Xiang-fang, FENG Zhen-dong, HU Ru-qian, & LI Huai-lin. (2017). Research on Micromorphology and Performance of TiAlN Coating and TiAlSiN Coating on Zirconium Alloy Surface. Rare Metals and Cemented Carbides(6), 66-70. |
| IEEE | [1] ZHOU Jun, FAN Xiang-fang, FENG Zhen-dong, HU Ru-qian, and LI Huai-lin, "Research on Micromorphology and Performance of TiAlN Coating and TiAlSiN Coating on Zirconium Alloy Surface," Rare Metals and Cemented Carbides, no. 6, pp. 66-70, 2017. keywords: {Zr-4 alloy;TiAlSiN coating;TiAlN coating;multi-arc ion plating;high temperature oxidation resistance;coating/substrate adhesion strength} |