Research on Preparation and Interfacial Reaction of Ti_3SiC_2/Al-Mg Composites AITranslate
Abstract AITranslate
Using Ti3SiC2 as the external strengthening phase and Al-Mg alloy as the matrix,Ti3SiC2/Al-Mg composites were prepared by spark plasma sintering(SPS).The effect of subsequent heat treatment on interfacial reaction was researched.The results show that Ti3SiC2/Al-Mg composites can be prepared successfully by SPS,and insulation temperature is a key factor affecting interfacial reaction during heat treatment.When the temperature is lower than 550℃,no interfacial reaction occurs.When the temperature reaches 600 ℃,a slight interfacial reaction occurs,and the main products are Al4 C3 and Mg2 Si.Interfacial reaction leads to an increase of material hardness,but a decrease of the density and conductivity.In addition,with the increase of Mg content in the matrix,the grain size of Ti3SiC2/Al-Mg composites gradually decreases and the hardness gradually increases.
KeyWords AITranslate
1兖利鹏,王爱琴,谢敬佩,倪增磊.铝基复合材料在汽车领域的应用研究进展[J].稀有金属与硬质合金,2013,41(2):44-48. 被引量:22
2白朴存,代雄杰,赵春旺,邢永明.Al_2O_3/Al复合材料的界面结构特征[J].复合材料学报,2008,25(1):88-93. 被引量:27
3吴玉锋,杜文博,聂祚仁,曹林锋,左铁镛.颗粒增强镁基复合材料研究进展[J].稀有金属材料与工程,2007,36(1):184-188. 被引量:19
4刘耀,张建波,李勇,肖翔鹏,陈辉明.MAX/金属基自润滑复合材料的研究现状及进展[J].材料导报:纳米与新材料专辑,2015,29(2):517-523. 被引量:15
1SPS 049 1/35 Sd.Kfz.171“黑豹”A后期型履带及活动悬挂组建[J].模型世界,2017,0(12):25-25.
2刘文扬,张建波,邬善江,胡美俊,陈婷婷,郭丽丽.Si对Ti_3SiC_2/Al复合材料的摩擦性能影响[J].有色金属科学与工程,2017,8(5):89-94. 被引量:2
3安勇良,尹冬松,谭志强.Gd对Al-Mg合金微观组织和力学性能的影响[J].黑龙江科技大学学报,2017,27(6):670-673. 被引量:4
4张婧昕,李柱.上市公司高管减持的市场反应研究[J].经贸实践,2017(13):1-3. 被引量:1
5靳廷甲,章祥林,徐建.铁酸锰/腐植酸复合材料制备及其对亚甲基蓝吸附性能[J].腐植酸,2017,0(6):51-51.
6王登峰.钢铁材料抗拉强度与硬度关系分析[J].名城绘,2017(12):84-84.
7施苗,朱丹,张宇,邓晖.伴有黑质超声改变的僵人综合征一例[J].中华神经科杂志,2018,51(2):133-135.
8杨素媛,郭丹,沈娟,贺静怡.SPS制备TiNi增强镁合金复合材料的微观结构及力学性能[J].复合材料学报,2018,35(2):371-376. 被引量:3
9姚时,张鸣帅,李林璇,廖云开,周娜,范世锁,唐俊.茶渣负载纳米四氧化三铁复合材料制备及其对亚甲基蓝的吸附机理[J].环境化学,2018,37(1):96-107. 被引量:20
10韩臻臻,贾慧敏,杨树华,曹丙强,姜亚南.ZnFe_2O_4纳米粒子-石墨烯复合材料制备和超级电容器性能[J].中国粉体技术,2018,24(1):86-89. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TB331[一般工业技术—材料科学与工程]
Citation Information:
Using Ti3SiC2 as the external strengthening phase and Al-Mg alloy as the matrix,Ti3SiC2/Al-Mg composites were prepared by spark plasma sintering(SPS).The effect of subsequent heat treatment on interfacial reaction was researched.The results show that Ti3SiC2/Al-Mg composites can be prepared successfully by SPS,and insulation temperature is a key factor affecting interfacial reaction during heat treatment.When the temperature is lower than 550℃,no interfacial reaction occurs.When the temperature reaches 600 ℃,a slight interfacial reaction occurs,and the main products are Al4 C3 and Mg2 Si.Interfacial reaction leads to an increase of material hardness,but a decrease of the density and conductivity.In addition,with the increase of Mg content in the matrix,the grain size of Ti3SiC2/Al-Mg composites gradually decreases and the hardness gradually increases.
quote
| GB/T 7714-2015 | [1] LIU Wen-yang, JIN Yi-ming, HU Tao-tao, et al. Research on Preparation and Interfacial Reaction of Ti_3SiC_2/Al-Mg Composites[J]. Rare Metals and Cemented Carbides, 2017(6): 59-65. |
| MLA | [1] LIU Wen-yang, et al., "Research on Preparation and Interfacial Reaction of Ti_3SiC_2/Al-Mg Composites." Rare Metals and Cemented Carbides, no. 6, 2017, pp. 59-65. |
| APA | [1] LIU Wen-yang, JIN Yi-ming, HU Tao-tao, WU Shan-jiang, ZHANG Jian-bo, LI Yong, & XIAO Xiang-peng. (2017). Research on Preparation and Interfacial Reaction of Ti_3SiC_2/Al-Mg Composites. Rare Metals and Cemented Carbides(6), 59-65. |
| IEEE | [1] LIU Wen-yang, JIN Yi-ming, HU Tao-tao, WU Shan-jiang, ZHANG Jian-bo, LI Yong, and XIAO Xiang-peng, "Research on Preparation and Interfacial Reaction of Ti_3SiC_2/Al-Mg Composites," Rare Metals and Cemented Carbides, no. 6, pp. 59-65, 2017. keywords: {Ti3SiC2/Al-Mg composite;spark plasma sintering(SPS);interfacial reaction;heat treatment} |