Experimental Study on Strength of Cold-bound Pellets of Carbon-dosing Nb-Fe Associated Ore AITranslate
Abstract AITranslate
The strength of cold-bound pellets of carbon-dosing Nb-Fe associated ore was studied using polyvinyl alcohol as the binder.The influences of carbon to oxygen ratio in pellets,compacting pressure,binder concentration and drying temperature on the strength of green and roasted pellets were investigated.The results show that the strength of both dry and wet pellets is maximum at carbon to oxygen ratio 1.0,compacting pressure 15 MPa,binder concentration 3%,roasting temperature 100 ℃.
KeyWords AITranslate
1张波;刘承军;姜茂发.白云鄂博稀土铌铁复合矿提铌工艺的研究[A]北京:冶金工业出版社,20099-13.
2张志霞,解建军,韩涛,胡长庆,王丽丽.含铁粉尘再资源化利用与碳酸化球团工艺[J].烧结球团,2011,36(2):44-49. 被引量:8
3郭玉华,徐洪军,周继程,齐渊洪.新西兰海沙矿含碳球团成型、还原实验研究[J].矿冶工程,2010,30(6):78-80. 被引量:1
4郭玉华,高岗,韩勇,齐渊洪.转炉炼钢污泥冷固结成型实验研究[J].烧结球团,2010(1):30-33. 被引量:5
5沈宗斌,沙永志.钢铁粉尘冷固结球团工艺研究[J].钢铁,2003,38(12):1-5. 被引量:15
6尹海生,吕庆,蒋武峰.有机物粘结的高配煤球团的强度试验[J].河北理工学院学报,1996,18(3):38-43. 被引量:2
7张一敏.球团矿生产技术[M]北京:冶金工业出版社,200525-67.
8陈津,刘浏,曾加庆.竖炉型含碳球团有机粘结剂的选择与应用[J].烧结球团,2000,25(6):29-31. 被引量:5
1李强,陈铁军,马浩,黄献宝.用球团返粉压团焙烧制备氧化球团的研究[J].烧结球团,2013,38(3):22-26. 被引量:1
2唐敬坤,郭磊,郭占成.球团矿高温还原过程中抗压强度变化及机理[J].钢铁,2014,49(7):66-71. 被引量:14
3马兰,杨绍利,曾扬州.钒钛铁精矿内配碳球团低温焙烧特性研究[J].钢铁钒钛,2014,35(6):60-65. 被引量:1
4杨慧芬,蒋蓓萍,袁运波,王亚运,苑修星.焙烧制度对煤泥-浸锌渣冷固结球团还原行为的影响[J].金属矿山,2015,44(1):161-165. 被引量:1
5杨慧芬,王亚运,江波,张伟豪,宋荣龙.浸锌渣-煤泥-CaO冷固结球团的制备及还原性能研究[J].烧结球团,2017,42(1):28-32. 被引量:2
1邢宏伟,魏福申,田铁磊,霍国杰,李雅茹.PMC精粉配比对氧化球团质量的影响规律[J].烧结球团,2018,43(6):70-73. 被引量:5
2刘朝卿,刘然,吕庆,刘小杰,张欣媛.冀东磁铁精粉球团矿的矿相结构研究[J].钢铁钒钛,2014,35(6):124-129. 被引量:4
3郭春梅.焙烧温度对纳米钒催化剂性能的影响研究[J].钢铁钒钛,2015,36(5):25-29.
4陈小龙,李家新,杨佳龙,春铁军,郭其飞.优化球团原料的配矿[J].中国冶金,2016,26(9):18-22. 被引量:9
5罗果萍,刘安康,王永斌,朱建国.MgO对含钾钠氟球团还原膨胀性能的影响[J].钢铁,2016,51(11):14-18. 被引量:5
6王治帅,公旭中,王志,刘文礼.电石渣制备高强度氧化钙及其含碳球团循环生产电石[J].中国氯碱,2017(1):42-46. 被引量:8
7杨慧芬,王亚运,江波,张伟豪,宋荣龙.浸锌渣-煤泥-CaO冷固结球团的制备及还原性能研究[J].烧结球团,2017,42(1):28-32. 被引量:2
8田筠清,青格勒,刘长江,李永欣.使用石灰石生产低硅碱性球团矿试验[J].中国冶金,2018,28(4):13-16. 被引量:20
9周明顺,王义栋,赵东明,王俊山,李建军,金增武.高硫铁精矿配比对球团工艺参数及性能的影响[J].钢铁,2018,53(5):11-17. 被引量:12
10张军强,钟梅,于星,王志,钱国余,公旭中.电石渣基CaO球团热强度的调控[J].聚氯乙烯,2018,46(7):9-14.
1谭富彬,赵玲,刘林,李茜.纳米银粉的液固相化学制备方法及特性[J].贵金属,1999,20(3):9-12. 被引量:31
2王建军,王桦.氢氧化铝b值的研究[J].有色金属分析通讯,2000(6):22-23.
3王玲珑,熊曼辰,王禾,常红清.压球烘干车间智能模糊控制器的设计[J].科学技术与工程,2011,11(23):5656-5659. 被引量:2
4奚红杰,于淼,曹宏.氢氧化铟粉末的研制[J].世界有色金属,2003(9):20-20. 被引量:3
5田宝喜.红土镍矿制含碳球团实验研究[J].黑河学院学报,2011,2(6):125-128.
6张梅,罗永光.锌浸出渣的微波干燥与常规干燥对比实验研究[J].企业技术开发,2010,29(A7):91-92. 被引量:3
7刘诚.电池级氧化钴的研制[J].有色金属,2002,54(4):25-29. 被引量:20
8石西昌,孙锡良.液相共沉淀法制备超细In_2O_3·SnO_2复合粉末[J].有色金属,2005,57(3):24-27. 被引量:6
9刘松利,白晨光,胡途.钒钛铁精矿内配碳球团压团工艺研究[J].稀有金属,2011,35(1):83-88. 被引量:4
10刘晓东,吕宪俊.提高活性白土活性度的工艺条件研究[J].非金属矿,2006,29(2):44-46. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TF046[冶金工程—冶金物理化学]
Citation Information:
The strength of cold-bound pellets of carbon-dosing Nb-Fe associated ore was studied using polyvinyl alcohol as the binder.The influences of carbon to oxygen ratio in pellets,compacting pressure,binder concentration and drying temperature on the strength of green and roasted pellets were investigated.The results show that the strength of both dry and wet pellets is maximum at carbon to oxygen ratio 1.0,compacting pressure 15 MPa,binder concentration 3%,roasting temperature 100 ℃.
quote
| GB/T 7714-2015 | [1] ZHANG Fu-shun, ZHAO Zeng-wu, FENG Nai-xiang, et al. Experimental Study on Strength of Cold-bound Pellets of Carbon-dosing Nb-Fe Associated Ore[J]. Rare Metals and Cemented Carbides, 2012(2): 60-63. |
| MLA | [1] ZHANG Fu-shun, et al., "Experimental Study on Strength of Cold-bound Pellets of Carbon-dosing Nb-Fe Associated Ore." Rare Metals and Cemented Carbides, no. 2, 2012, pp. 60-63. |
| APA | [1] ZHANG Fu-shun, ZHAO Zeng-wu, FENG Nai-xiang, CHANG Hong-tao, & LI Xiao-gang. (2012). Experimental Study on Strength of Cold-bound Pellets of Carbon-dosing Nb-Fe Associated Ore. Rare Metals and Cemented Carbides(2), 60-63. |
| IEEE | [1] ZHANG Fu-shun, ZHAO Zeng-wu, FENG Nai-xiang, CHANG Hong-tao, and LI Xiao-gang, "Experimental Study on Strength of Cold-bound Pellets of Carbon-dosing Nb-Fe Associated Ore," Rare Metals and Cemented Carbides, no. 2, pp. 60-63, 2012. keywords: {Nb-Fe associated ore;cold-bound pellet;carbon-dosing;strength} |