Optimization of Cu and Sc Content in Al-Cu-Sc Aluminum Alloy Conductor Materials by Response Surface Method AITranslate
Abstract AITranslate
In order to improve the electrical conductivity and mechanical properties of Al-Cu-Sc aluminum alloy conductor materials,the response surface method(RSM)of central composite design was applied to design experiments with Design-Expert 8.0.6 software.The contents of Cu and Sc elements in Al-Cu-Sc aluminum alloy conductor materials were optimized,and a second-order response model was established regarding the effects of Cu and Sc element contents on the electrical conductivity and tensile strength of the alloy.The results show that the optimized conditions are Cu Content of 0.35%and Sc Content of 0.24%.The results of validation experiments under these conditions show that the response surface model has high reliability.The electrical conductivity of Al-0.35%Cu-0.24%Sc alloy material reaches 56.4%IACS and the tensile strength reaches 83.25 MPa,which meets the requirements for the electrical conductivity and mechanical properties of the alloy.
KeyWords AITranslate
1张强,许超,李海龙,杨长龙,李禄洋,郎大志,陈友慧,祝志祥.耐热铝合金导体材料的研究进展[J].热加工工艺,2020,49(19):7-10. 被引量:4
2钟夏平,高英俊,刘慧.Al-Cu合金时效初期的价电子结构[J].中国有色金属学报,2004,14(1):55-59. 被引量:16
3徐国富,金头男,邹景霞,尹志民,聂祚仁.微量Sc元素对Al-Cu合金组织与性能的影响[J].材料热处理学报,2004,25(2):15-18. 被引量:11
4岳嵩,邓显波,张嘉艺,王斌,王海生.低温下Sc微合金化对8xxx系铝合金导线蠕变性能的影响[J].材料热处理学报,2017,38(9):36-42. 被引量:5
5方三明,杨成刚,余爱武,万亿平,李貌,李其胜.Sc、Ti、Zr复合微合金化对纯铝组织和力学性能的影响[J].热加工工艺,2015,44(10):87-89. 被引量:3
6张茁,陈康华.固溶处理对Al-Zn-Mg-Cu铝合金电导率的影响[J].粉末冶金材料科学与工程,2004,9(1):79-83. 被引量:17
1谢金财,程伟,余灿梅,刘崇宇,江鸿杰,黄宏锋.搅拌摩擦加工优化Al-Si-Mg-Sc合金的力学性能[J].特种铸造及有色合金,2022,42(5):569-573.
1丁伟.基于数据分析的立式击弦机轴架性能自动化测试研究[J].自动化与仪器仪表,2021(8):27-30.
2高孝书,吕云.基于RSM和MPSO的镁合金薄板冲压工艺参数优化[J].热加工工艺,2021,50(15):79-83. 被引量:3
3刘士雨,俞缙,刘文强,蔡燕燕,涂兵雄.基于MICP的珊瑚砂砂浆裂缝自修复新型细菌载体[J].建筑材料学报,2021,24(4):687-693. 被引量:3
4龙建辉,张玲玲,邢鲜丽,郭晓娟.基于温度路径的冻融作用下黄土强度及微观结构研究[J].煤田地质与勘探,2021,49(4):242-249. 被引量:1
5王志勇,李德鹏,李惠玲,王繁业.微乳液中豆荚过氧化物酶催化制备(S)-奥美拉唑[J].华中师范大学学报:自然科学版,2021,55(4):597-602.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.2[金属学及工艺—金属材料]
Citation Information:
In order to improve the electrical conductivity and mechanical properties of Al-Cu-Sc aluminum alloy conductor materials,the response surface method(RSM)of central composite design was applied to design experiments with Design-Expert 8.0.6 software.The contents of Cu and Sc elements in Al-Cu-Sc aluminum alloy conductor materials were optimized,and a second-order response model was established regarding the effects of Cu and Sc element contents on the electrical conductivity and tensile strength of the alloy.The results show that the optimized conditions are Cu Content of 0.35%and Sc Content of 0.24%.The results of validation experiments under these conditions show that the response surface model has high reliability.The electrical conductivity of Al-0.35%Cu-0.24%Sc alloy material reaches 56.4%IACS and the tensile strength reaches 83.25 MPa,which meets the requirements for the electrical conductivity and mechanical properties of the alloy.
quote
| GB/T 7714-2015 | [1] QU Chen-chi, LIU Kui-ren, HAN Qing, et al. Optimization of Cu and Sc Content in Al-Cu-Sc Aluminum Alloy Conductor Materials by Response Surface Method[J]. Rare Metals and Cemented Carbides, 2021(4): 43-49. |
| MLA | [1] QU Chen-chi, et al., "Optimization of Cu and Sc Content in Al-Cu-Sc Aluminum Alloy Conductor Materials by Response Surface Method." Rare Metals and Cemented Carbides, no. 4, 2021, pp. 43-49. |
| APA | [1] QU Chen-chi, LIU Kui-ren, HAN Qing, LI Bin-chuan, WANG Chun-xin, GAO Xiang, & CHEN Jian-she. (2021). Optimization of Cu and Sc Content in Al-Cu-Sc Aluminum Alloy Conductor Materials by Response Surface Method. Rare Metals and Cemented Carbides(4), 43-49. |
| IEEE | [1] QU Chen-chi, LIU Kui-ren, HAN Qing, LI Bin-chuan, WANG Chun-xin, GAO Xiang, and CHEN Jian-she, "Optimization of Cu and Sc Content in Al-Cu-Sc Aluminum Alloy Conductor Materials by Response Surface Method," Rare Metals and Cemented Carbides, no. 4, pp. 43-49, 2021. keywords: {Al-Cu-Sc alloy;response surface method;central composite design;second-order response model;composition optimization} |