School of Metallurgical and Chemical Engineering,Jiangxi University of Science and Technology;School of Metallurgical and Chemical Engineering,Jiangxi University of Science and Technology;School of Metallurgical and Chemical Engineering,Jiangxi University of Science and Technology;School of Metallurgical and Chemical Engineering,Jiangxi University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using sodium bicarbonate solution as the precipitant of yttrium carbonate,the influence of reaction temperature,feeding speed,seed crystal amount and aging time on the crystallinity of yttrium carbo-nate was studied by response surface method,and the optimal technical conditions for crystallization of yttrium carbonate were obtained.The results show that the four factors have effect on the crystallinity of yttrium carbonate crystal in order:seed crystal amount>reaction temperature>aging time>feeding speed.The optimal technical conditions are reaction temperature of 72.22℃,feeding speed of 1.91 mL/min,seed crystal amount of 7.19 mL and aging time of 2.29 h.Under the optimal conditions,the average intensity of the three major XRD peaks of yttrium carbonate is 515,the particle size distribution is concentrated and large particles are dominative,the crystal grain size significantly increases,the specific surface area of the crystal decreases,and the flocculent structure on the particle surface decreases.

KeyWords AITranslate

yttrium carbonate crystallinity sodium bicarbonate precipitation response surface method

1胡悦,潘伟.Er,Yb共掺氧化钇透明陶瓷的Judd-Ofelt参数计算(英文)[J].稀有金属材料与工程,2018,47(S1):366-369. 被引量:1

2康菊芸,陈光耀,兰豹豹,李宝同,鲁雄刚,李重河.Y掺杂BaZrO_3的稳定性及抗钛熔体的侵蚀性[J].中国有色金属学报,2019,29(4):749-755. 被引量:3

3窦彩虹,魏世忠,周玉成,徐流杰.水热合成不同形态氧化钇的制备工艺及生长机制[J].稀有金属,2018,42(8):856-863. 被引量:3

4黄昕,李琴,杨明,罗洋,叶信宇,杨幼明.大颗粒草酸钕热分解特性及动力学研究[J].中国稀土学报,2016,34(1):83-92. 被引量:11

5孟祥龙,冯宗玉,黄小卫,董金诗,王良士,赵龙胜.氧化钙沉淀硫酸稀土过程中杂质的分布与去除[J].稀有金属,2018,42(10):1114-1120. 被引量:16

6朱伟,邱东兴,裴浩宇,周雪珍,祝文才,李静,刘艳珠,李东平,周新木,李永绣.Y_2(CO_3)_3的沉淀结晶过程与晶粒大小控制[J].中国稀土学报,2016,34(2):180-188. 被引量:11

7胡艳宏,李梅,柳召刚,阮莹,王觅堂,王丽.碳酸氢铵沉淀法制备大颗粒CeO_2的研究[J].稀土,2008,29(4):12-17. 被引量:7

8高国华,赖安邦,廖春发,刘钧云,任卫,肖燕飞.Na2CO3沉淀制备超细Y2O3粉体的研究[J].中国稀土学报,2020,38(5):622-632. 被引量:5

9王东杰,易红宏,唐晓龙,郭文亮,侯少春,王素梅.REx(CO3)y沉淀废水处理的资源化研究[J].稀有金属,2018,42(5):537-545. 被引量:3

10Zonghe Yu,Meng Wang,Liangshi Wang,Longsheng Zhao,Zongyu Feng,Xu Sun,Xiaowei Huang.Preparation of crystalline mixed rare earth carbonates by Mg(HCO3)2 precipitation method[J].稀土学报:英文版,2020,0(3):292-298. 被引量:6

1陈冀渝.废玻璃在铺地烧结砖中的应用[J].砖瓦,2021(8):36-37.

2曾盛熊,王成伟.肝脏未分化胚胎性肉瘤误诊为肝包虫一例[J].临床放射学杂志,2021,40(5):898-899. 被引量:1

3李大塘,刘秋华,汤璐.钴(Ⅱ)盐鉴别可溶性碳酸盐溶液实验的设计与研究[J].化学教育(中英文),2021,42(16):49-54.

4沈铭晖,史红玲,郭庆超,陆琴.黑龙江卡伦山以上河段水沙特性及造床流量研究[J].泥沙研究,2021,46(4):21-27. 被引量:6

Basic Information:

DOI:

Chinese Library Classification Number:TQ133.23[化学工程—无机化工]

Citation Information:

Using sodium bicarbonate solution as the precipitant of yttrium carbonate,the influence of reaction temperature,feeding speed,seed crystal amount and aging time on the crystallinity of yttrium carbo-nate was studied by response surface method,and the optimal technical conditions for crystallization of yttrium carbonate were obtained.The results show that the four factors have effect on the crystallinity of yttrium carbonate crystal in order:seed crystal amount>reaction temperature>aging time>feeding speed.The optimal technical conditions are reaction temperature of 72.22℃,feeding speed of 1.91 mL/min,seed crystal amount of 7.19 mL and aging time of 2.29 h.Under the optimal conditions,the average intensity of the three major XRD peaks of yttrium carbonate is 515,the particle size distribution is concentrated and large particles are dominative,the crystal grain size significantly increases,the specific surface area of the crystal decreases,and the flocculent structure on the particle surface decreases.

quote

GB/T 7714-2015 [1] LIU Qing-sheng, CHENG Hua-jin, WANG Xue-zhong, et al. Optimization of Crystallinity of Yttrium Carbonate Precipitation by Response Surface Method[J]. Rare Metals and Cemented Carbides, 2021(4): 35-42.
MLA [1] LIU Qing-sheng, et al., "Optimization of Crystallinity of Yttrium Carbonate Precipitation by Response Surface Method." Rare Metals and Cemented Carbides, no. 4, 2021, pp. 35-42.
APA [1] LIU Qing-sheng, CHENG Hua-jin, WANG Xue-zhong, & LI Hua-jie. (2021). Optimization of Crystallinity of Yttrium Carbonate Precipitation by Response Surface Method. Rare Metals and Cemented Carbides(4), 35-42.
IEEE [1] LIU Qing-sheng, CHENG Hua-jin, WANG Xue-zhong, and LI Hua-jie, "Optimization of Crystallinity of Yttrium Carbonate Precipitation by Response Surface Method," Rare Metals and Cemented Carbides, no. 4, pp. 35-42, 2021. keywords: {yttrium carbonate;crystallinity;sodium bicarbonate;precipitation;response surface method}